journal article·2015-01Open access

The influence of slag compositional changes on the chemical degradation of magnesia-chromite refractories exposed to PbO-based non-ferrous slag saturated in spinel

L. Scheunis, M. Campforts, P.T. Jones, B. Blanpain, A. Malfliet

Abstract

Abstract In non-ferrous metallurgy the refractory life is application dependent, typically going from several months up to 2 years or more. Slag engineering is widely used to reduce the dissolution rate of a refractory lining by forming a solid protection layer at the slag-lining interface, thereby increasing the lining's lifetime. The non-ferrous slag in this paper is engineered to form a protective spinel layer. This phase, however, only forms near and at the slag-lining interface, while deeper inside the sample forsterite grains are detected, resulting in direct contact between the still unsaturated slag and the magnesia-chromite refractory phases. At this position the MgO dissolution increases with a factor 3–4 compared with the slag-refractory interface, attacking the bonding between grains and decreasing the brick's mechanical strength. As this happens deeper inside the sample, the spalling risk increases. Strategies to simultaneously reduce refractory dissolution and spalling are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Advanced ceramic materials synthesis · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Wear of chrome magnesite bricks in copper smelting furnaces
2. Refractories for the copper and lead industry
3. Refractory materials for the copper and lead industry
4. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
5. Chemical corrosion mechanisms of magnesia-chromite and chrome-free refractory bricks by copper metal and anode slag10.1016/j.jeurceramsoc.2006.08.020 ↗
6. Degradation mechanisms of magnesia-chromite refractories in vacuum-oxygen decarburisation ladles during production of stainless steel10.1179/030192300677525 ↗
7. Using confocal scanning laser microscopy for the in situ study of high-temperature behaviour of complex ceramic materials10.1016/j.jeurceramsoc.2007.01.022 ↗
8. A study of slag-infiltrated magnesia-chromite refractories using hybrid microwave heating10.1016/S0955-2219(00)00343-5 ↗
9. Degradation mechanisms of magnesia-chromite refractories by high-alumina stainless steel slags under vacuum conditions10.1016/j.jeurceramsoc.2005.12.025 ↗
10. Melt corrosion of oxide and oxide-carbon refractories10.1179/095066099101528234 ↗
11. Degradation of MgO–C refractories by MnO-rich stainless steel slags10.1016/j.ceramint.2008.12.007 ↗
12. In situ observation of the direct and indirect dissolution of MgO particles in CaO–Al2O3–SiO2-based slags10.1016/j.jeurceramsoc.2006.05.107 ↗
13. The effect of phase formation during use on the chemical corrosion of magnesia–chromite refractories in contact with a non-ferrous PbO–SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
14. Reactions of dense MgO with calcium ferrite-based slags at 1573K10.1007/s11663-005-0055-7 ↗
15. The effect of the CaO/SiO2 ratio on the phase equilibria in the ZnO–“Fe2O3”–(PbO+CaO+SiO2) system in air: CaO/SiO2=0.1, PbO/(CaO+SiO2)=6.2, and CaO/SiO2=0.6, PbO/(CaO+SiO2)=4.310.1007/s11663-003-0064-3 ↗
16. Experimental study of phase equilibria in the PbO–ZnO–“Fe2O3”–CaO–SiO2 system in air for high lead smelting slags (CaO/SiO2=0.35 and PbO/(CaO+SiO2)=5.0 by weight)10.1007/s11663-002-0065-7 ↗
17. Experimental liquidus in the PbO–ZnO–“Fe2O3”–(CaO+SiO2) system in air, with CaO/SiO2=0.35 and PbO/(CaO+SiO2)=3.210.1007/s11663-002-0068-4 ↗
18. Experimental study of phase equilibria in the PbO–MgO–SiO2 system10.1007/s11663-001-0002-1 ↗
19. The effect of phase formation during use on the chemical corrosion of magnesia–chromite refractories in contact with a non-ferrous PbO–SiO2 based slag10.1016/j.jeurceramsoc.2013.12.026 ↗
20. Coupled experimental and thermodynamic modelling study of the system PbO–ZnO–FeO–Fe2O3–CaO–SiO2–Al2O3 for lead and zinc smelting
21. FactSage thermochemical software and databases10.1016/S0364-5916(02)00035-4 ↗
22. FactSage thermochemical software and databases—recent developments10.1016/j.calphad.2008.09.009 ↗
23. Mechanism of solid-state reaction between magnesium oxide and aluminum oxide and between magnesium oxide and ferric oxide10.1111/j.1151-2916.1961.tb13724.x ↗
24. Fundamentals and applications on in situ spinel formation mechanisms in Al2O3–MgO refractory castables10.1016/j.ceramint.2011.10.074 ↗
25. Kinetic mechanisms of the formations of MgCr2O4 and FeCr2O4 spinels from their metal-oxides10.1016/0167-2738(91)90081-L ↗
26. Kinetics of spinel formation and growth during dissolution of MgO in CaO–Al2O3–SiO2 slag10.1007/s11663-008-9186-y ↗
27. Cr and Al diffusion in chromite spinel: experimental determination and its implication for diffusion creep10.1007/s00269-008-0238-2 ↗
28. Interdiffusion in the MgO–Al2O3 spinel with or without some dopants10.1007/BF02651865 ↗
29. Interdiffusion studies in system MgO-Al2O310.1016/0022-3697(71)90015-1 ↗
30. Defects and cation diffusion in magnetite 110.1002/bbpc.19770810320 ↗
31. Neutron scattering and polarization by ferromagnetic materials10.1103/PhysRev.84.912 ↗
32. Physical properties and cation arrangement of oxides with spinel structures II. Electronic conductivity10.1063/1.1746466 ↗
33. Defects and cation diffusion in magnetite(II)10.1002/bbpc.19770810412 ↗
34. Forsterite bursting in magnesia chromite bricks—two case studies from lead and copper smelting furnaces
35. Complex phase equilibria in refractories design and use10.1111/j.1151-2916.2002.tb00555.x ↗