Microstructural development of SrAl12O19 in alumina–strontia composites
Source abstract
Abstract
Abstract Boehmite sol was prepared by hot water hydrolysis of aluminium iso-propoxide using nitric acid as catalyst. Strontium nitrate was added to the boehmite sol to yield 0-20 vol.% strontia. The boehmite with additives was dried at 120 °C. The powder samples were calcined at 1600 °C for 3 h and the formation of strontium hexa-aluminate is discussed using phase diagram, transmission electron microscope and energy dispersive spectra. The powder samples calcined at 500 °C were milled for 6 h, compacted into cylindrical pellets using uni-axial press at 180 MPa and sintered at 1600 °C for 6 h. A microstructural model was proposed for the formation of strontium hexa-aluminate. The sintered pellets were ground and phases determined using XRD. The formation of hexa-aluminate (plate-like) grains was confirmed using optical microscope and scanning electron micronscope.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Reduction and sintering of alumina/tungsten nano composites
2. Dispersion of alumina and Silicon carbide powders in alumina sol10.1111/j.1151-2916.1999.tb02019.x ↗
3. R-Curve behavior of in situ toughened Al2O3/CaAl12O19 ceramic composites
4. Exaggerated grain growth of Fe doped alumina10.1023/A:1006632629310 ↗
5. Mechanical properties and microstructure of TZP/TZP–Al2O3 composites10.1557/PROC-78-123 ↗
6. High toughness Ce-TZP/Al2O3 ceramics with improved hardness and strength10.1111/j.1151-2916.1991.tb07315.x ↗
7. In situ alumina/aluminate platelet composites10.1111/j.1151-2916.1992.tb05623.x ↗
8. AGG of faceted grains in Co liquid matrix10.1007/BF02652373 ↗
9. Growth of BaTiO3 grains by the twin-plate re-entrant edge mechanism10.1111/j.1151-2916.2000.tb01201.x ↗
10. Effect of initial particle size on microstructure of liquidphase sintered silicon carbide10.1016/S0955-2219(99)00239-3 ↗
11. Effect of heating rate on the exaggerated grain growth behaviour of Si3N410.1016/S0167-577X(97)00018-9 ↗
12. Effect of coalescence on the grain coarsening during liquid phase sintering of TaC–TiC–Ni cermets10.1016/S1359-6454(00)00117-8 ↗
13. AGG in diphasic Gel-derived Titania doped Mullite10.1111/j.1151-2916.1998.tb02478.x ↗
14. Impurity dependent morphology and grain growth in liquid phase sintered alumina10.1111/j.1151-2916.2001.tb00886.x ↗
15. High Toughness Ce-TZP/Al2O3 ceramics with improved hardness and strength10.1111/j.1151-2916.1991.tb07315.x ↗
16. Microstructure development and Mechanical properties of alumina-hex-aluminate composites as-sintered and after aging in aqueous physiological solution10.2109/jcersj.107.270 ↗
17. Control of Calcium hexaluminate grain morphology in in-situ toughened ceramic composites10.1007/BF00354672 ↗
18. Sintering of calcium aluminate mixes10.1179/096797899680426 ↗
19. Low temperature synthesis of calcium hexa-aluminate10.1111/j.1151-2916.2002.tb00170.x ↗
20. Effect of divalent cation additives on the γ–α alumina phase transition10.1111/j.1151-2916.2000.tb01296.x ↗
21. Microprobe Flourescence spectroscopy evaluation of stress fields developed along a propagating crack in an Al2O3/CaO·6Al2O3 ceramic composites10.1557/JMR.2001.0385 ↗
22. Effect of Strontia on the densification and mechanical properties of sol-gel alumina10.1016/j.ceramint.2005.06.014 ↗
23. Effect of calcia on the densification and mechanical properties of sol-gel alumina10.1080/0371750X.2006.11012220 ↗
24. sol–gel synthesis and characterisation of alumina–calcium hexaluminate composites10.1111/j.1551-2916.2005.00330.x ↗