journal article·2012-12

Influence of C doping on the fracture mode and abrasive wear of Al2O3

Noor A. Yahya, Richard I. Todd

Publisher page

Abstract

Abstract Previous studies have shown that the addition of SiC nanoparticles to Al 2 O 3 changes the fracture mode from intergranular to transgranular and in doing so improves the wear resistance. The reason for this is not clear but a change to the grain boundary chemistry caused by impurities such as C added with the SiC may be involved. The aim of the current study was to investigate the influence of small amounts of C doping on the fracture mode and wear properties of Al 2 O 3 . The microstructure and properties of Al 2 O 3 doped with 0 and 0.012 wt% C were studied. Al 2 O 3 showed mainly intergranular fracture. The addition of 0.012 wt% C to Al 2 O 3 changed the fracture mode to mainly transgranular. The wear resistance improved and the percentage of surface grains pulled out was lower compared to pure Al 2 O 3 .
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. New design concept of structural ceramics–ceramic nanocomposites10.2109/jcersj.99.974 ↗
2. Mechanical behavior of alumina-silicon carbide nanocomposites10.1111/j.1151-2916.1993.tb03814.x ↗
3. Fabrication, characterization and properties of alumina matrix nanocomposites
4. Microstructural requirements for alumina-SiC nanocomposites10.1179/096797899680471 ↗
5. Polishing behaviour and surface quality of alumina and alumina/silicon carbide nanocomposites10.1111/j.1151-2916.2000.tb01357.x ↗
6. Relationship between wear rate, surface pullout and microstructure during abrasive wear of alumina and alumina/SiC nanocomposites10.1016/j.actamat.2005.03.031 ↗
7. The relationship between microstructure, fracture and abrasive wear in Al2O3/SiC nanocomposites and microcomposites containing 5 and 10% SiC10.1016/j.jeurceramsoc.2009.03.023 ↗
8. Microstructure–property relationships in wear resistant alumina/SiC nanocomposites10.4028/www.scientific.net/AST.45.555 ↗
9. Effect of silicon carbide nano-phase on the wet erosive wear of polycrystalline alumina10.1016/0955-2219(95)00198-0 ↗
10. The wear behaviour of Al2O3–SiC ceramic nanocomposites10.1016/S1359-6462(99)00403-0 ↗
11. Sliding wear of alumina/silicon carbide nanocomposites10.1111/j.1151-2916.1999.tb02071.x ↗
12. Particulate strengthened oxide ceramic nanocomposite
13. Electron microscopy of crack/particle interactions in Al2O3/SiC nanocomposites10.1046/j.1365-2818.1997.d01-610.x ↗
14. A Quantitative analysis of crack–interface interactions in Al2O3-based nanocomposites10.1080/01418619808241916 ↗
15. Microstructural requirements for alumina–SiC nanocomposites10.1179/096797899680471 ↗
16. Alumina-carbon composites with high hardness
17. Abrasive wear of Al2O3–SiC and Al2O3–(SiC)–C composites with micrometer- and submicrometer-sized alumina matrix grains10.1016/j.jeurceramsoc.2008.04.018 ↗
18. Compression creep of alumina containing interfacial silicon, carbon, and nitrogen, derived from a polysilazane precursor10.1111/j.1551-2916.2009.03515.x ↗
19. Linear intercept technique for measuring grain size in two-phase polycrystalline ceramics10.1111/j.1151-2916.1972.tb11224.x ↗
20. Theory and application of a micro-scale abrasive wear test10.1520/JTE11487J ↗
21. Probing the improbable: imaging carbon atoms in alumina10.1016/S1369-7021(10)70184-X ↗
22. Demystifying the role of sintering additives with “complexion”10.1016/j.jeurceramsoc.2007.12.018 ↗
23. Carbon nanotube toughened aluminium oxide nanocomposites10.1016/j.jeurceramsoc.2009.09.032 ↗
24. Multi-walled carbon nanotubes reinforced Al2O3 nanocomposites: mechanical properties and interfacial investigations10.1016/j.compscitech.2010.03.007 ↗
25. Bending strength and microstructure of Al2O3 ceramics densified by spark plasma sintering10.1016/S0955-2219(00)00086-8 ↗