journal article·2020-06

Revealing the formation mechanism of the skin-core structure in nearly stoichiometric polycrystalline SiC fibers

Pengren Wang, Yanzi Gou, Hao Wang, Yingde Wang

Publisher page

Abstract

Abstract The polymer-derived SiC fibers have broad application prospects in the fields of aerospace, nuclear industry and high-tech weapon. Oxygen plays an essential role in adjusting the composition, structure and tensile strength of SiC fibers. Our studies have found that introducing too much oxygen during air curing process will form the skin-core structure in nearly stoichiometric polycrystalline SiC fibers. In order to reveal the formation mechanism of the skin-core structure, gradient oxygen was introduced into the fibers. The morphologies, phase distributions and defects of the fibers were well characterized. By strictly controlling the introduction of oxygen, the polycrystalline product fiber exhibits intragranular fracture behavior and excellent high-temperature resistance. The retention rate of its tensile strength can reach up to 91% and 61% after exposure at 1800 °C for 1 h and 10 h, respectively. The present results give valuable insights into the structural optimization of the nearly stoichiometric polycrystalline SiC fibers.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Silicon Carbide Semiconductor Technologies · Diamond and Carbon-based Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Simple synthesis of the continuous SiC fiber with high tensile strength10.1246/cl.1976.551 ↗
2. Ceramic fibers based on SiC and SiCN systems: current research, development, and commercial status10.1002/adem.201400069 ↗
3. Polymer-derived ceramics: 40 years of research and innovation in advanced ceramics10.1111/j.1551-2916.2010.03876.x ↗
4. Defect control of SiC polycrystalline fiber synthesized from poly-aluminocarbosilane10.1016/j.jeurceramsoc.2016.02.022 ↗
5. A review of the development of three generations of small diameter silicon carbide fibres10.1007/s10853-006-6566-z ↗
6. Formation of carbon-rich layer on the surface of SiC fiber by sintering under vacuum for superior mechanical and thermal properties10.1016/j.jeurceramsoc.2016.10.013 ↗
7. Polyaluminocarbosilane as precursor for aluminium-containing SiC fiber from oxygen-free sources10.1016/j.ceramint.2016.03.191 ↗
8. High-strength alkali-resistant sintered SiC fibre stable to 2,200 °C10.1038/35820 ↗
9. Microstructure and oxidative degradation behavior of silicon carbide Fiber hi–Nicalon type S
10. Fabrication of nearly stoichiometric polycrystalline SiC fibers with excellent high-temperature stability up to 1900 °C10.1111/jace.15366 ↗
11. Advances in inorganic fibers10.1007/b104208 ↗
12. Current status and prospects of SiCf/SiC for fusion structural applications10.1016/j.jeurceramsoc.2013.02.013 ↗
13. Preparation of SiC/SiC composites by hot pressing, using Tyranno-SA Fiber as reinforcement10.1111/j.1151-2916.2003.tb03272.x ↗
14. Progress in SiC-Based ceramic composites for fusion applications10.13182/FST03-A326 ↗
15. Preparation and characterization of SiC fibers with diverse electrical resistivity through pyrolysis under reactive atmospheres10.1016/j.jeurceramsoc.2016.09.023 ↗
16. Facile synthesis of melt-spinnable polyaluminocarbosilane using low-softening-point polycarbosilane for Si-C-Al-O fibers10.1007/s10853-016-0101-7 ↗
17. The high-temperature corrosion behavior of SiBCN fibers for aerospace applications10.1021/acsami.8b04497 ↗
18. Thermodynamic study of the thermal degradation of SiC-based fibres: influence of SiC grain size10.1007/BF00455414 ↗
19. Non-oxide (silicon carbide) fibers
20. Active-to-passive oxidation transition for polycarbosilane-derived silicon carbide fibers heated in Ar-O2, gas mixtures10.1023/A:1014945823031 ↗
21. Ceramic filament Fibers-A review10.1002/mame.201100364 ↗
22. Cao · 2017
23. Microstructure and mechanical properties of SiC-polycrystalline fiber and new defect-controlling process10.1111/ijac.12719 ↗
24. Effect of reduced pressure on oxidation and thermal stability of polycarbosilane-derived SiC fibers10.1023/B:JMSC.0000004421.67094.2e ↗
25. Conversion of polyaluminocarbosilane (PACS) to Si-Al-C10.1016/S1003-6326(06)60043-5 ↗
26. Effect of oxygen on the mechanical properties of polymer-derived Si-Al-C-O fibers10.4028/www.scientific.net/KEM.336-338.1287 ↗
27. Study on thermal-curing of polycarbosilane fibers
28. Effects of Al and O content on transformation from SiAlCO to Si(Al)C fibers after high temperature treatment10.15541/jim20150402 ↗
29. Mesoporous silicon carbide nanofibers with in situ, embedded carbon for co-catalyst free photocatalytic hydrogen production10.1007/s12274-015-0971-z ↗