Abstract

Abstract The arc erosion behavior of Ti3AlC2 in oxygen, air, nitrogen, carbon dioxide, argon, and sulfur hexafluoride atmospheres at 9 kV voltage was studied. The breakdown strength increased in the order of oxygen, air, carbon dioxide, nitrogen, argon, and sulfur hexafluoride, whereas the arc energy decreased. Cracks, pits, and bulges on the eroded surface were investigated using scanning electron microscopy and three-dimensional (3D) laser confocal scanning microscopy. Raman spectroscopy and X-ray photoelectron spectroscopy (XPS) were used to determine the composition of the eroded surface. The arc energy and electromagnetic force lead to the formation of erosion characteristics. The mechanism of erosion under the different atmospheres is discussed systematically, and is called the “decomposition-oxidation” process in oxygen, air, and carbon dioxide and the “decomposition-rereaction” process in nitrogen and sulfur hexafluoride. This study provides a reference for the application of MAX phase materials in high-voltage electrical appliances.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (43)

Show source-provided references
1. Discharge characteristics of an atmospheric pressure radio-frequency plasma jet10.1088/0022-3727/38/9/011 ↗
2. Twenty-five years of progress in vacuum arc research and utilization10.1109/27.650894 ↗
3. Influence of alloy components on arc erosion morphology of Ag/MeO electrical contact materials10.1016/S1003-6326(16)64105-5 ↗
4. Effect of preparing method of ZnO powders on electrical arc erosion behavior of Ag/ZnO electrical contact material10.1557/jmr.2016.20 ↗
5. Effect of WC particle size and Ag volume fraction on electrical contact resistance and thermal conductivity of Ag-WC contact materials10.1016/j.matdes.2015.07.006 ↗
6. Effect of TiB2 particle size on erosion behavior of ag-4wt% TiB2 composite10.1016/S1875-5372(16)60004-8 ↗
7. Enhanced arc erosion resistance of TiB2/Cu composites reinforced with the carbon nanotube network structure10.1016/j.matdes.2019.108136 ↗
8. Formation and effects of CuO nanoparticles on Ag/SnO2 electrical contact materials10.1016/j.jallcom.2016.12.092 ↗
9. Influence of rare earth on the wetting ability of AgSnO2 contact material10.1016/S1875-5372(14)60143-0 ↗
10. Effect of CuO additives on the formation of SnO2-rich layers in Ag-SnO2 materials10.1016/j.jallcom.2018.08.159 ↗
11. Microstructure and vacuum arc characteristics of CuO skeletal structure Ag-CuO contact materials10.1016/j.jallcom.2016.05.271 ↗
12. How Cu doping improves the interfacial wettability between Ag and SnO2 of Ag/SnO2 contact material10.1016/j.jallcom.2019.04.134 ↗
13. Investigation on arc erosion behaviors and mechanism of W70Cu30 electrical contact materials adding graphene10.1016/j.jallcom.2016.12.044 ↗
14. Erosion behavior of a Cu-Ti3AlC2 cathode by multi-electric arc10.3390/ma12182947 ↗
15. Arc ablation behavior and microstructure evolution of plastically deformed and micro-alloyed Cu–Cr–Zr alloys10.1016/j.jallcom.2019.153123 ↗
16. Impact of the gas environment on the electric arc
17. AC Breakdown characteristics of c-C4F8/N2 gas mixtures in an extremely non-uniform electric field10.3390/en11123533 ↗
18. Investigation of voltage and potential gradient of arc column in fluoro-carbon gas and its gas mixtures
19. Summary of Constitutional Data on the Al–Ti–C System10.1007/BF02647559 ↗
20. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
21. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
22. Nb doping in Ti3AlC2: effects on phase stability, high-temperature compressive properties, and oxidation resistance10.1016/j.jeurceramsoc.2017.04.026 ↗
23. Ti3AlC2, a candidate structural material for innovative nuclear energy system: The microstructure phase transformation and defect evolution induced by energetic heavy-ion irradiation10.1016/j.actamat.2020.03.008 ↗
24. High-temperature oxidation behavior of un-dense Ti3AlC2 material at 1000 °C in air10.1016/j.ceramint.2011.10.091 ↗
25. Microstructure and properties of Ti3AlC2 prepared by the solid–liquid reaction synthesis and simultaneous in-situ hot pressing process10.1016/S1359-6454(02)00117-9 ↗
26. Effect of textureon oxidation resistance of Ti3AlC210.1016/j.jeurceramsoc.2018.03.009 ↗
27. MAX phases: bridging the gap between metals and ceramics
28. Deformation mechanisms during high temperature tensile creep of Ti3AlC2 MAX phase10.1016/j.jallcom.2016.09.194 ↗
29. Layered machinable and electrically conductive Ti2AlC and Ti3AlC2 ceramics10.1016/S1005-0302(10)60064-3 ↗
30. Investigation of Ti3AlC2 formation mechanism through diffusional reaction between carbon and Mo-modified Ti6Al4V10.1016/j.jeurceramsoc.2019.11.062 ↗
31. A spectroscopic detecting system for measuring the temperature distribution of silver breaking arc using a CCD color camera10.1109/19.772195 ↗
32. Influence of breakdown voltages on arc erosion of a Ti3AlC2 cathode in an air atmosphere10.1016/j.ceramint.2017.05.018 ↗
33. Size-dependent modifications of the first-order Raman spectra of nanostructured rutile TiO210.1103/PhysRevB.77.195414 ↗
34. Raman effect of corundum10.1063/1.1711980 ↗
35. Crystal-chemistry of the Ti3AlC2 and Ti4AlN3 layered carbide/nitride phases-characterization by XPS10.1016/S0022-3697(00)00268-7 ↗
36. TiO2 by XPS10.1116/1.1247794 ↗
37. Characterization of water exposed plasma sprayed oxide coating materials using XPS10.1016/j.apsusc.2008.03.168 ↗
38. Corrundum (α-Al2O3) by XPS10.1116/1.1247851 ↗
39. First-order Raman scattering of the MAX phases: Ti2AlN, Ti2AlC0.5N0.5, Ti2AlC, (Ti0.5V0.5)2AlC, V2AlC, Ti3AlC2, and Ti3GeC210.1002/jrs.3036 ↗
40. Measurement of AlN/GaN (0001) heterojunction band offsets by x-ray photoemission spectroscopy10.1063/1.116355 ↗
41. ESCA, XRD, and IR Characterization of Aluminum Oxide, Hydroxyfluoride, and Fluoride Surfaces in Correlation with Their Catalytic Activity in Heterogeneous Halogen Exchange Reactions10.1006/jcat.1994.1208 ↗
42. Arc ablation properties of Ti3SiC2 material10.1016/j.ceramint.2019.06.305 ↗
43. Corrosion and degradation mechanism of Ag/Ti3AlC2 composites under dynamic electric arc discharge10.1016/j.corsci.2019.05.005 ↗