Ti3Si(Al)C2-based ceramics fabricated by reactive melt infiltration with Al70Si30 alloy
Source abstract
Abstract
Abstract Dense Ti3Si(Al)C2-based ceramics were synthesized using reactive melt infiltration (RMI) of Al70Si30 alloy into the porous TiC preforms. The effects of the infiltration temperature on the microstructure and mechanical properties of the synthesized composites were investigated. All the composites infiltrated at different temperatures were composed of Ti3Si(Al)C2, TiC, SiC, Ti(Al, Si)3 and Al. With the increase of infiltration temperature from 1050 °C to 1500 °C, the Ti3Si(Al)C2 content increased to 52 vol.% and the TiC content decreased to 15 vol.%, and the Vickers hardness, flexural strength and fracture toughness of Ti3Si(Al)C2-based composite reached to 9.95 GPa, 328 MPa and 4.8 MPa m1/2, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. The MAX phases: unique new carbide and nitride materials10.1511/2001.28.736 ↗
2. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
3. Layered machinable ceramics for high temperature applications10.1016/S1359-6462(96)00418-6 ↗
4. Microstructural evolution and mechanical properties of Ti3SiC2-TiC composites10.1016/j.jallcom.2010.04.116 ↗
5. Synthesis of Ti3SiC2/TiC composites from TiH2/SiC/TiC powders10.1016/j.matlet.2005.02.077 ↗
6. Synthesis and characterization of 0.3Vf TiC-Ti3SiC2 and 0.3Vf SiC-Ti3SiC2 composites10.1016/S0925-8388(02)00985-4 ↗
7. Strengthening of Ti3AlC2 by incorporation of Si to form Ti3Al1−xSixC2 solid solutions10.1016/j.actamat.2005.10.057 ↗
8. A dense and fine-grained SiC/Ti3SiAlC2 composite and its high-temperature oxidation behavior10.1016/j.jeurceramsoc.2012.04.029 ↗
9. In situ processing and high-temperature properties of Ti3SiAlC2/SiC composites10.1111/j.1744-7402.2006.02057.x ↗
10. Mechanical behaviour of Al3Ti intermetallic and L12 phases on its basis10.1016/S0966-9795(01)00073-5 ↗
11. Microstructure and mechanical behavior of a multiphase Al3Ti-based intermetallic alloy10.1016/S0966-9795(00)00050-9 ↗
12. Reactive hot pressing and mechanical properties of TiAl3/Ti3AlC2/Al2O3 in situ composite10.1016/j.matdes.2013.02.053 ↗
13. Formation of NbAl3/Al2O3 composites by pressureless reactive infiltration10.1111/j.1551-2916.2008.02583.x ↗
14. Near net shape manufacturing of ceramics10.1016/S0254-0584(99)00115-7 ↗
15. Synthesis of Ti3SiC2 bulks by infiltration method10.1016/j.jallcom.2010.12.092 ↗
16. Synthesis of Ti3SiC2 by infiltration of molten Si10.1016/j.jallcom.2011.06.074 ↗
17. Three-dimensional printing of Ti3SiC2-based ceramics10.1111/j.1551-2916.2010.04257.x ↗
18. Three-dimensional printing of nanolaminated Ti3AlC2 toughened TiAl3-Al2O3 composites10.1111/j.1551-2916.2007.01668.x ↗
19. Near-net-shape fabrication of Ti3AlC2-based composites10.1111/j.1744-7402.2007.02123.x ↗
20. Ti3AlC2-Al2O3-TiAl3 composite fabricated by reactive melt infiltration10.1016/S1003-6326(08)60431-8 ↗
21. Reactive infiltration processing of Ti3AlC2 and Ti3SiC2-based composites
22. Effect of aluminum on the reaction synthesis of ternary carbide Ti3SiC210.1016/S1359-6462(03)00391-9 ↗
23. Effect of Al addition on the synthesis of Ti3SiC2 bulk material by pulse discharge sintering process10.1016/j.jeurceramsoc.2007.03.038 ↗
24. Effect of Al addition on phase purity of Ti3SiAlC2 synthesized by mechanical alloying10.1016/j.jmatprotec.2006.09.001 ↗
25. Effect of Al addition on pressureless reactive sintering of Ti3SiC210.1016/j.scriptamat.2006.08.019 ↗
26. Fracture toughness of ceramics using the SEVNB method: from a preliminary study to a standard test method
27. Effect of solid solution of Si on mechanical properties of TiAl3 based on the multi-laminated Ti-(SiCP/Al) composite system10.1016/j.msea.2013.05.007 ↗
28. The thermal stability of TiC particles in an Al7wt.% Si alloy10.1016/S0921-5093(03)00143-6 ↗
29. Si-induced twinning of TiC and formation of Ti3SiC2 platelets10.1016/S1359-6454(02)00248-3 ↗
30. Effects of Si and Al on twin boundary energy of TiC10.1016/S1359-6454(03)00032-6 ↗
31. Energetics of point defects in TiC10.1016/j.jeurceramsoc.2008.06.027 ↗
32. Effect of TiC content on the microstructure and properties of Ti3SiC2-TiC composites in situ fabricated by spark plasma sintering10.1016/j.msea.2007.12.004 ↗
33. Elastic and mechanical properties of the MAX phases10.1146/annurev-matsci-062910-100448 ↗
34. Micro-scale plastic deformation of polycrystalline Ti3SiC2 under room-temperature compression10.1016/S0955-2219(00)00310-1 ↗
35. Processing and mechanical properties of Ti3SiC2: II, effect of grain size and deformation temperature10.1111/j.1151-2916.1999.tb02167.x ↗
36. Machinability of Ti3SiC2 with layered structure synthesized by hot pressing mixture of TiCx and Si powder10.1016/j.jeurceramsoc.2012.04.021 ↗
37. Mechanical properties and oxidation resistance of Ti3SiC2/SiC composite synthesized by in situ displacement reaction of Si and TiC10.1016/S0167-577X(02)01429-5 ↗
38. In situ reaction synthesis and characterization of Ti3Si(Al)C2/SiC composites10.1016/j.ceramint.2005.07.004 ↗
39. The effects of several coatings on cyclic oxidation resistance of TiAl intermetallics10.1016/S0257-8972(98)00645-8 ↗
40. Fabrication and characterization of a carbon fibre reinforced carbon-silicon carbide-titanium silicon carbide hybrid matrix composite10.1016/j.msea.2009.08.069 ↗
41. Friction and wear behaviors of C/C-SiC composites containing Ti3SiC210.1016/j.wear.2011.08.029 ↗
42. Processing, microstructure and ablation behavior of C/SiC-Ti3SiC2 composites fabricated by liquid silicon infiltration10.1016/j.corsci.2013.04.029 ↗