Abstract The wetting of SiC plate by Y 2 O 3 /AlN additive was analysed using the sessile drop method. The wetting behaviour was observed by image capture system using a CCD camera during the heating, in argon atmosphere. The contact angle was measured as a function of temperature and time. After the wetting test the SiC plus additive samples were cut in order to observe the thickness plate cross section. The additive area and the interface between SiC and additive were analysed using scanning electron microscopy (SEM) and energy dispersive spectrometry (EDS). The wetting of SiC by Y 2 O 3 /AlN is influenced by the presence of a solid phase in some of the additive drops that depends mainly on the additive composition and consequently on the temperature. The measured contact angles were below 7°, reaching 0° for Y 2 O 3 /AlN additive tested at the eutectic composition, indicating a very good wettability of Y 2 O 3 /AlN on the SiC.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Surface Modification and Superhydrophobicity · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Review article: silicon carbide. Structure, properties and processing10.1590/S0366-69132000000100002 ↗
2. Thermochemical analysis of the silicon carbide-alumina reaction with reference to liquid-phase sintering of silicon carbide10.1111/j.1151-2916.1991.tb06885.x ↗
3. Liquid phase sintered SiC. Processing and transformation controlled microstructure tailoring10.1590/S1516-14392000000400007 ↗
4. Interfacial forces in Si3N4-and SiC-based systems and their influence on the joining process10.1111/j.1151-2916.1999.tb02284.x ↗
5. Effect of additive content on liquid-phase sintering on silicon carbide ceramics10.1016/S0025-5408(99)00172-5 ↗
6. Solution mechanisms for dopant oxides in yttria10.1111/j.1151-2916.1999.tb01954.x ↗
7. Slag-graphite wettabilitity and reaction kinetics Part 2 Wettability influenced by reduction kinetics10.1179/030192300677750 ↗
8. Thermodynamic modelling of wetting silicon nitride/Ni-Cr-Si alloy interfaces10.1016/0921-5093(94)90417-0 ↗
9. A thermodynamic criterion to predict wettability at metal-alumina interfaces10.1007/BF02651856 ↗
10. Wettability and interfacial energies in SiC-liquid metal systems10.1007/BF02403656 ↗
11. Active coating for SiC particles to reduce the degradation by liquid aluminium during processing of aluminium matrix composites: study of interfacial reactions10.1046/j.1365-2818.2001.00765.x ↗
12. The wettability of YAlSiON oxide glasses and its application in silicon nitride joining10.1016/S0955-2219(00)00115-1 ↗
13. Wetting behaviour of SiC ceramics: Part I – E2O3/Al2O3 additive system10.1016/j.matlet.2004.05.005 ↗
14. Wetting behaviour of SiC ceramics: Part II – Y2O3/Al2O3 and Sm2O3/Al2O310.1016/j.matlet.2004.05.004 ↗
15. Joining of silicon carbide using MgOAl2O3SiO2 filler10.1023/A:1004411108502 ↗
16. Slag-graphite wettability and reaction kinetics. Part 1: Kinetics and mechanism of molten FeO reaction10.1179/030192300677679 ↗
17. Measurement of contact angle and work of adhesion at high temperature10.1007/s10853-005-1945-4 ↗
18. Reactive spreading: adsorption, ridgind and compound formation10.1016/S1359-6454(00)00231-7 ↗
19. Mass transport phenomena at the liquid metal/substrate (metal, carbide) interface10.1016/S0921-5093(97)00097-X ↗