Laser-supported joining of SiC-fiber/SiCN ceramic matrix composites fabricated by precursor infiltration
Source abstract
Abstract
Abstract SiC-fiber/SiCN ceramic matrix composites were manufactured by means of polymer infiltration and pyrolysis. The fiber preform was made by slurry infiltration and winding using a computer-controlled winding module. Multiple infiltration steps using a Si–C–N precursor were included to increase the density. The influence of the sintering conditions on the microstructure of the CMC was demonstrated. Pipe sections made of the CMC materials were joined using a laser-supported heating technology with an Y–Al–Si–O glass–ceramic filler. The thermal response of the CMC components was controlled by the anisotropic thermal conductivity. Fast heating by laser beam was achieved for elements rotating in the direction of the fiber winding. SEM micrographs of the joints showed the good wettability of the CMC by the glass–ceramic filler. Nearly defect-free joints were obtained using a nitrogen process atmosphere. The laser-supported technology was shown to be promising for the joining of CMC components.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Committee on Advanced Fibres for High-Temperature Ceramic Composites, C.o.E.a.T.S. · 1998
2. Oxidation resistant non-oxide ceramic matrix composites
3. Krenkel · 2008
4. Composite materials for high temperature reactors: technology development roadmap
5. Silicon carbide composites as fusion power reactor structural materials10.1016/j.jnucmat.2011.03.005 ↗
6. Coatings and joining for SiC and SiC-composites for nuclear energy systems10.1016/j.jnucmat.2007.03.189 ↗
7. Design requirements for SiC/SiC composites structural material in fusion power reactor blankets10.1016/S0920-3796(97)00200-7 ↗
8. Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications10.1016/S0022-3115(99)00268-8 ↗
9. Silicon carbide-based materials for joining silicon carbide composites for fusion energy applications10.1016/S0022-3115(02)01063-2 ↗
10. Microstructure and mechanical properties of low-activation glass–ceramic joining and coating for SiC/SiC composites10.1016/S0022-3115(00)00096-9 ↗
11. Joining of machined SiC/SiC composites for thermonuclear reactors10.1016/j.jnucmat.2008.02.020 ↗
12. Effects of neutron irradiation on glass–ceramics as pressure-less joining materials for SiC based components for nuclear applications10.1016/j.jnucmat.2012.05.035 ↗
13. Cordierite-mullite coating for SiC/SiC composites10.1016/S0955-2219(01)00535-0 ↗
14. Glass–ceramic joining and coating of SiC/SiC for fusion applications10.1016/S0022-3115(98)00176-7 ↗
15. Wetting and joining of silicon carbide with a molten glass under air
16. Crystallization of yttria–alumina–silica–glasses10.1111/j.1151-2916.1992.tb04427.x ↗
17. Thermodynamic evaluation of the Si–C–Al–Y–O system for LPS-SiC application10.1007/s11669-010-9695-7 ↗
18. Oxynitride glasses, their properties and crystallization – a review10.1016/S0022-3093(02)01938-5 ↗
19. Recent advances and issues in development of silicon carbide composites for fusion applications10.1016/j.jnucmat.2008.12.305 ↗
20. R&D of joining technology for SiC components with channel10.1016/j.jnucmat.2008.12.263 ↗
21. Laser joining of silicon carbide – a new technology for ultra-high temperature resistant joint10.1016/j.nucengdes.2004.03.002 ↗
22. Electrically conductive ceramics and new joining technologies for applications in HTR engineering10.1016/j.nucengdes.2011.09.065 ↗
23. High-temperature stability of laser-joined silicon carbide components10.1016/j.jnucmat.2013.07.067 ↗
24. Chemical interaction of yttrium alumosilicate glass with CeO2, UO2 and PuO2 at high temperatures10.1016/j.nucengdes.2011.05.012 ↗
25. Mechanical and microstructural characterisation of SiC- and SiBNC-fibre reinforced CMCs manufactured via PIP method before and after exposure to air10.1016/j.jeurceramsoc.2012.05.028 ↗
26. Processing and performance of SiC/Blackglas™ CFCCs using filament winding10.1002/9780470314876.ch48 ↗
27. Processing and performance of continuous fiber ceramic composites by preceramic polymer pyrolysis: I – Filament winding10.1177/002199801772662028 ↗
28. Processing and performance of Nicalon/Blackglas and Nextel/Blackglas using cure-on-the-fly filament winding and preceramic polymer pyrolysis with inactive fillers10.1016/S0266-3538(01)00066-5 ↗
29. KiON® Corporation. TB2: KiON® Ceraset® Polyureasilazane and KiON® Ceraset® Polysilazane 20. Pensylvania: KiON® Corporation.
30. Petzow · 2002
31. Silicon nitride for high-temperature applications
32. Munz · 1999
33. SiC continuous fiber-reinforced Si3N4 by infiltration and reaction bonding
34. Informationszentrum technische Keramik · 2012
35. Thermo-mechanical properties and microstructure of silicon carbide composites fabricated by nano-infiltrated transient eutectoid process10.1016/S0920-3796(02)00180-1 ↗
36. CeramTec: material table. www.ceramtec.com [19.04.13].
37. Property tailorability for advanced CVI silicon carbide for fusion10.1016/j.fusengdes.2005.08.045 ↗
38. Temperature-dependent absorptances of ceramics for Nd:YAG and CO2 laser processing applications10.1115/1.2824250 ↗
39. SiC particle reinforced oxynitride glass: processing and mechanical properties10.1016/S0955-2219(96)00165-3 ↗
40. Effect of SiC particles on the laser sintering of Al–7Si–0.3Mg alloy10.1016/j.scriptamat.2008.03.007 ↗
41. Gaskorrosion nichtoxidischer Werkstoffe
42. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗