Low temperature synthesis of dense MoAlB thin films
Source abstract
Abstract
While bulk synthesis of MoAlB requires temperatures larger than 1000 °C with up to 40 % of excess Al in the feedstock, here we report the temperature range for the formation of single phase, orthorhombic MoAlB synthesized by magnetron sputtering from a stoichiometric target is 450–650 °C. Lower synthesis temperatures yield the formation of amorphous films, while at 700 °C, impurity phases form in addition to orthorhombic MoAlB. Amorphous MoAlB films were observed by in-situ X-ray diffraction to crystallize between 545 and 575 °C. Hence, we infer that the formation of orthorhombic MoAlB thin films is surface diffusion mediated below 545 °C. As bulk diffusion is activated between 545 and 575 °C the synthesis of fully dense MoAlB films with a maximum hardness of 15 ± 2 GPa and a Young’s modulus of 379 ± 30 GPa at 600 °C is surface and bulk diffusion mediated.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: MXene and MAX Phase Materials · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Elastic properties, thermal stability, and thermodynamic parameters of MoAlB10.1103/PhysRevB.95.144108 ↗
2. Synthesis of MoAlB particulates and their porous derivatives by selective deintercalation of Al from MoAlB
3. Theoretical investigation of structural, elastic, and electronic properties of ternary boride MoAlB10.1002/pssb.201700010 ↗
4. Synthesis and characterization of an alumina forming nanolaminated boride: MoAlB
5. Synthesis, microstructure and properties of MoAlB ceramics prepared by in situ reactive spark plasma sintering10.1016/j.ceramint.2020.03.059 ↗
6. Synthesis, microstructure and properties of MoAlB ceramics10.1016/j.ceramint.2018.04.177 ↗
7. Synthesis and oxidation resistance of MoAlB single crystals10.1016/j.ceramint.2018.10.170 ↗
8. Crack healing behavior of a MAB phase: MoAlB10.1016/j.jeurceramsoc.2019.05.059 ↗
9. Ultra-high temperature ablation behavior of MoAlB ceramics under an oxyacetylene flame10.1016/j.jeurceramsoc.2019.01.016 ↗
10. Cyclic oxidation behavior of MoAlB in the temperature range 450–850 °C10.1016/j.jallcom.2020.154802 ↗
11. Low temperature synthesis of phase pure MoAlB powder in molten NaCl
12. High-temperature tribological behaviors of MoAlB ceramics sliding against Al2O3 and Inconel 718 alloy10.1016/j.ceramint.2020.02.275 ↗
13. Thermal shock behavior of a nanolaminated ternary boride: MoAlB10.1016/j.ceramint.2018.08.071 ↗
14. Anisotropic thermal expansions of select layered ternary transition metal borides: MoAlB, Cr 2 AlB 2 Mn 2 AlB 2 and Fe 2 AlB 210.1063/1.5054379 ↗
15. Isothermal and cyclic oxidation of MoAlB in air from 1100°C to 1400°C10.1149/2.1891713jes ↗
16. X-ray photoelectron spectroscopy of the MAB phases, MoAlB, M2AlB2 (M = Cr, Fe), Cr3AlB4 and their binary monoborides10.1016/j.jeurceramsoc.2019.09.040 ↗
17. Friction and wear properties of MoAlB against Al2O3 and 100Cr6 steel counterparts10.1016/j.jeurceramsoc.2018.10.026 ↗
18. Atomic structure and lattice defects in nanolaminated ternary transition metal borides10.1080/21663831.2016.1245682 ↗
19. Preparation of fine-grained MoAlB with preferable mechanical properties and oxidation resistance10.1016/j.ijrmhm.2020.105345 ↗
20. Synthesis and properties of orthorhombic MoAlB coatings10.3390/coatings9080510 ↗
21. ImageJ2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
22. Autonomously self‐reporting hard coatings: tracking the temporal oxidation behavior of TiN by in situ sheet resistance measurements10.1002/adfm.202000146 ↗
23. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
24. Scherrer after sixty years: a survey and some new results in the determination of crystallite size10.1107/S0021889878012844 ↗
25. Influence of apparatus geometry and deposition conditions on the structure and topography of thick sputtered coatings10.1116/1.1312732 ↗
26. Structure-zone models of thin films
27. Correlation of electrical resistivity and grain size in sputtered titanium films10.1016/0040-6090(94)06259-N ↗
28. Stress-dependent elasticity of TiAlN coatings10.3390/coatings9010024 ↗