Effect of SiC nanowires on the thermal shock resistance of joint between carbon/carbon composites and Li2O–Al2O3–SiO2 glass ceramics
Source abstract
Abstract
Abstract In order to improve the bonding property of joint between SiC modified carbon/carbon (C/C) composites and Li2O–Al2O3–SiO2 (LAS) glass ceramics, SiC nanowires were attempted as the reinforcement materials in the interface region of SiC transition layer and Li2O–MgO–Al2O3–SiO2 (LMAS) gradient joining interlayer. The C/C–LAS joint with SiC nanowire-reinforced interface layer was prepared by a three-step technique of pack cementation, in situ reaction and hot-pressing. The microstructure and thermal shock resistance of the as-prepared joints were examined. The average shear strength of the joined samples with SiC nanowires increased from 24.9 MPa to 31.6 MPa after 40 thermal cycles between 1000 °C and room temperature, while that of the joined samples without SiC nanowires dropped from 21.4 MPa to 8.3 MPa. The increase of thermal shock resistance of the C/C–LAS joints was mainly attributed to the toughening mechanism of SiC nanowires by pullout, bridging and crack deflection.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Diamond and Carbon-based Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. MAS-NMR investigations of the crystallization behaviour of lithium aluminum silicate (LAS) glasses containing P2O5 and TiO2 nucleants10.1016/j.jssc.2010.04.011 ↗
2. Negative thermal expansion of lithium aluminosilicate ceramics at cryogenic temperatures10.1016/j.scriptamat.2010.03.047 ↗
3. Synthesis powder precursor of LAS ceramics via pH controlled wet chemical process10.1016/j.powtec.2011.04.032 ↗
4. The complexity of the matrix micro structure in SiC-fiber-reinforced glass ceramic composites10.1016/0955-2219(95)00098-4 ↗
5. Conventional sintering of LAS–SiC nanocomposites with very low thermal expansion coefficient10.1016/j.jeurceramsoc.2010.07.003 ↗
6. Influences of SiCf content and length on the strength, toughness and dielectric properties of SiCf/LAS glass–ceramic composites10.1016/j.ceramint.2012.09.094 ↗
7. Dielectric properties of SiC/LAS composite10.1016/j.matlet.2004.09.026 ↗
8. The effect of heat-treatment temperature upon the properties of matrix-inhibited carbon–carbon composites10.1016/0008-6223(92)90028-U ↗
9. Influence of interlayer's thickness on strength of joints between LAS glass-ceramic and carbon/carbon composites10.3724/SP.J.1077.2011.00847 ↗
10. The preparation and mechanical properties of carbon–carbon/lithium–aluminum–silicate composite joints10.1016/j.matdes.2012.07.060 ↗
11. Single-crystal SiC nanowires with a thin carbon coating for stronger and tougher ceramic composites10.1002/adma.200500104 ↗
12. Nanobeam mechanics: elasticity, strength, and toughness of nanorods and nanotubes10.1126/science.277.5334.1971 ↗
13. Fabrication and mechanical properties of silicon carbide nanowires/epoxy resin composites10.1016/j.cap.2007.10.074 ↗
14. The effect of SiC nanowires on the flexural properties of CVI-SiC/SiC composites10.1016/j.jnucmat.2007.03.092 ↗
15. Wear behavior of SiC nanowire-reinforced SiC coating for C/C composites at elevated temperatures10.1016/j.jeurceramsoc.2013.06.018 ↗
16. SiC nanowires reinforced MAS joint of SiC coated carbon/carbon composites to LAS glass ceramics10.1016/j.msea.2011.10.088 ↗
17. Oxidation protection and behavior of C/C composites with an in situ SiC nanowire–SiC–Si/SiC–Si coating10.1016/j.corsci.2012.11.039 ↗
18. A gradient LMAS interlayer joint of SiC coated C/C composites to LAS glass ceramics10.1016/j.ceramint.2013.08.021 ↗
19. Comparison of the short beam shear (SBS) and interlaminar shear device (ISD) tests10.1016/S1359-835X(97)00009-2 ↗
20. Nanocrystalline-matrix ceramic composites for improved fracture toughness10.1557/mrs2004.12 ↗
21. Strength behavior of polycrystalline alumina subjected to thermal shock10.1111/j.1151-2916.1970.tb15997.x ↗