Thermal properties and Calcium-Magnesium-Alumina-Silicate (CMAS) resistance of LuPO4 as environmental barrier coatings
Source abstract
Abstract
Abstract LuPO4 ceramics have been synthesized by chemical precipitation and calcination approaches. The phase stability and the thermal properties of the ceramics as well as the thermochemical reactions between LuPO4 pellet and calcium–magnesium–alumina–silicate at 1300℃ have been investigated. The results indicated that LuPO4 has a relatively lower thermal conductivity (1.86 W m-1 K-1 at 1200 ℃) and a well-matched coefficient of thermal expansion (5.92 × 10-6 K-1) with SiC based ceramic matrix composites. No phase transformation occurs in single phase LuPO4 during the heating from room temperature to 1300 ℃. Corrosion tests showed that CMAS can dissolve LuPO4 and cause precipitation of crystalline phases such as Lu2Si2O7, CaAl2Si2O8, CaMgSi2O6, Ca2Lu8 (SiO4)6O2 and Ca8MgLu (PO4)7. Extending the corrosion duration results in the formation of Ca2Lu8 (SiO4)6O2 apatite and other crystalline phases with a dendritic-like structure in the CMAS layer. CMAS corrosion resistance of LuPO4 is significantly greater than Lu2Si2O7 since less LuPO4 need to be dissolved to form a protective apatite barrier layer. Ca8MgLu (PO4)7 tends to form a continuous reaction layer at the CMAS/LuPO4 interface. This dense and continuous layer can effectively inhibit molten CMAS penetration into LuPO4.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear materials and radiation effects · Advanced ceramic materials synthesis · Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
2. Observations of accelerated SiC recession by oxidation at high water-vapor pressures10.1111/j.1151-2916.2000.tb01172.x ↗
3. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
4. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
5. Rare earth silicate environmental barrier coatings: present status and prospective10.1016/j.ceramint.2017.01.153 ↗
6. Current status of environmental barrier coatings for Si-based ceramics
7. Thermal properties of rare-earth monosilicates for EBC on Si-based ceramicscomposites10.1111/jace.13982 ↗
8. Thermal expansion of rare‐earth pyrosilicates10.1111/jace.12388 ↗
9. The crystal chemistry of the rare-earth silicates10.1007/3-540-06125-8_3 ↗
10. Recession behavior of Yb2Si2O7 phase under high speed steam jet at high temperatures10.1016/j.corsci.2007.06.014 ↗
11. Water vapor corrosion behavior of lutetium silicates at high temperature10.1016/j.ceramint.2005.03.022 ↗
12. Recession mechanism of Lu-Si-O phase in high speed steam jet environment at high temperatures10.1016/j.ceramint.2005.05.014 ↗
13. Mechanisms of ytterbium monosilicate/mullite/silicon coating failure during thermal cycling in water vapor10.1111/jace.13792 ↗
14. Water vapor corrosion behavior and failure mechanism of plasma sprayed mullite/Lu2Si2O7-Lu2SiO5 coatings10.1016/j.ceramint.2018.05.020 ↗
15. Influence of phase composition on thermal aging behavior of plasma sprayed ytterbium silicate coatings10.1016/j.ceramint.2018.06.200 ↗
16. High temperature viscosity of calcium-magnesium-aluminosilicate glass from synthetic sand10.1016/j.scriptamat.2016.07.020 ↗
17. The influence of calcium–magnesium–aluminosilicate deposits on internal stresses in Yb2Si2O7 multilayer environmental barrier coatings10.1016/j.actamat.2015.12.016 ↗
18. Interaction of yttrium disilicate environmental barrier coatings with calcium-magnesium-iron alumino-silicate melts10.1016/j.actamat.2017.12.004 ↗
19. High-temperature interactions of desert sand CMAS glass with yttrium disilicate environmental barrier coating material10.1016/j.ceramint.2018.09.058 ↗
20. Hot corrosion of RE2SiO5with different cation substitution under calcium–magnesium–aluminosilicate attack10.1016/j.ceramint.2017.04.045 ↗
21. Exploration of YPO4 as a potential environmental barrier coating10.1016/j.ceramint.2009.10.014 ↗
22. Estimation of heat capacities of solid mixed oxides10.1016/S0040-6031(02)00177-6 ↗
23. Thermal conductivity of dense and porous yttria-stabilized zirconia10.1023/A:1017970924312 ↗
24. Environmental degradation of thermal-barrier coatings by molten deposits-Related Articles10.1557/mrs.2012.230 ↗
25. Infiltration-inhibiting reaction of gadolinium zirconate thermal barrier coatings with CMAS melts10.1111/j.1551-2916.2007.02175.x ↗
26. Calcium–magnesium–aluminosilicate corrosion behaviors of rare-earth disilicates at 1400°C10.1016/j.jeurceramsoc.2013.05.030 ↗
27. Theoretical exploration of the abnormal trend in lattice thermal conductivity for monosilicates RE2SiO5 (RE = Dy, Ho, Er, Tm, Yb and Lu)10.1016/j.jeurceramsoc.2018.04.014 ↗
28. Phase equilibrium in the fluorapatite–anorthite–diopside system10.1111/j.1151-2916.2000.tb01695.x ↗
29. CMAS-resistant plasma sprayed thermal barrier coatings based on Y2O3-stabilized ZrO2 with Al3+ and Ti4+ solute additions10.1007/s11666-014-0077-2 ↗
30. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗