Ti3SiC2 interphase coating in SiCf/SiC composites: Effect of the coating fabrication atmosphere and temperature
Source abstract
Abstract
Abstract The SiC fibers were coated with Ti3SiC2 interphase by dip-coating. The Ti3SiC2 coated fibers were heat-treated from 900 °C to 1100 °C in vacuum and argon atmospheres to comparatively analyze the effect of temperature and atmosphere on the microstructural evolution and mechanical strength of the fibers. The results show that the surface morphology of Ti3SiC2 coating is rough in vacuum and Ti3SiC2 is decomposed at 1100 °C. However, in argon atmosphere, the surface morphology is smooth and Ti3SiC2 is oxidized at 1000 °C and 1100 °C. At 1100 °C, Ti3SiC2 oxidized to form a thin layer of amorphous SiO2 embedded with TiO2 grains. Meanwhile, defects and pores appeared in the interphase scale. As a result, the fiber strength treated in the argon was lower than that treated in vacuum. The porous Ti3SiC2 interphase fabricated under vacuum was then employed to prepare the SiCf/SiC mini composite by chemical vapor infiltration (CVI) combined with precursor infiltration pyrolysis (PIP), and can effectively improve the toughness of SiCf/SiC mini composite. The propagating cracks can be deflected within the porous interphase layer, which promotes fiber pull-outs under the tensile strength.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Ceramic fibers for matrix composites in high-temperature engine applications10.1126/science.285.5428.699 ↗
2. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
3. Issues and advances in SiCf/SiC composites development for fusion reactors10.1016/j.jnucmat.2004.04.002 ↗
4. The role of the fiber-matrix interface in ceramic composites
5. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
6. Mechanical properties of 3D KD-I SiCf/SiC composites with engineered fibre–matrix interfaces10.1016/j.compscitech.2011.01.014 ↗
7. Effect of intermediate heat treatment on mechanical properties of SiCf/SiC composites with BN interphase prepared by ICVI10.1016/j.jeurceramsoc.2010.12.018 ↗
8. Mechanical properties of SiCf/SiC composites with PyC and the BN interface10.1016/j.ceramint.2015.02.041 ↗
9. Boron nitride interphase in ceramic-matrix composites10.1111/j.1151-2916.1991.tb06789.x ↗
10. Effect of boron nitride coating on fiber-matrix interactions
11. Carbon and oxide coatings on continuous ceramic fibers
12. Microstructural and microtextural investigations of boron nitride deposited from BCl3-NH3-H2 gas mixtures10.1016/S0955-2219(03)00126-2 ↗
13. The MN+ 1AXN phases: a new class of solids: thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
14. Synthesis and characterization of a remarkable ceramic: Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
15. The MAX phases: unique new carbide and nitride materials – ternary ceramics turn out to be surprisingly soft and machinable, yet also heat-tolerant, strong and lightweight10.1511/2001.28.334 ↗
16. Damage mechanisms around hardness indentations in Ti3SiC210.1111/j.1151-2916.1997.tb02861.x ↗
17. High temperature oxidation and hot corrosion behavior of Ti3SiC2-based materials
18. Kink formation around indents in laminated Ti3SiC2 thin films studied in the nanoscale10.1016/S1359-6462(03)00214-8 ↗
19. Growth of Ti 3 SiC 2 thin films by elemental target magnetron sputtering10.1063/1.1790571 ↗
20. Microstructure and mechanism of damage tolerance for Ti3SiC2 bulk ceramics10.1007/s100190050114 ↗
21. Formation of Ti3SiC2 interphase coating on SiCf/SiC composite by electrophoretic deposition10.1111/ijac.12804 ↗
22. On the chemical vapour deposition of Ti 3 SiC 2 from TiCl 4-SiCl 4-CH 4-H 2 gas mixtures10.1007/BF01151093 ↗
23. Pulsed reactive chemical vapor deposition in the C-Ti-Si system from H2/TiCl4/SiCl410.1016/j.tsf.2004.09.043 ↗
24. CVD of Ti3SiC210.1002/1521-3862(200011)6:6<289::AID-CVDE289>3.0.CO;2-4 ↗
25. The growth of Ti3SiC2 coatings onto SiC by reactive chemical vapor deposition using H-2 and TiCl410.1016/j.surfcoat.2006.09.040 ↗
26. Synthesis of boron nitride coatings on quartz fibers: thickness control and mechanism research
27. Formation of BN films on carbon fibers by dip-coating10.1016/S0257-8972(01)01539-0 ↗
28. A modified dip-coating method to prepare BN coating on SiC fiber by introducing the sol–gel process10.1016/j.surfcoat.2015.12.023 ↗
29. Microstructural characterization and fracture properties of SiC-based fibers annealed at elevated temperatures10.1007/s10853-006-0579-5 ↗
30. Microstructure and mechanical properties of SiC fibres after exposure at elevated temperature10.1080/17436753.2016.1186856 ↗
31. Microstructure and oxidative degradation behavior of silicon carbide fiber Hi-Nicalon type S10.1016/S0022-3115(98)00223-2 ↗
32. Thermal stability of the low-oxygen-content silicon carbide fiber, Hi-NicalonTM10.1016/S0266-3538(99)00012-3 ↗
33. Oxidation behavior of Hi-Nicalon SiC monofilament fibres in air and O2-H2O–Ar atmospheres10.1016/j.corsci.2011.12.019 ↗
34. Scheelite coatings on SiC fiber: Effect of coating temperature and atmosphere10.1016/j.ceramint.2020.08.286 ↗
35. Strength degradation of SiC fibers with a porous ZrB2-SiC coating: role of the coating porous structure10.1016/j.jeurceramsoc.2019.12.017 ↗
36. Zirconium and hafnium germanate-based thin films on SiC fibers10.1134/S0020168515100167 ↗
37. Characterization of dip-coated boron nitride on silicon carbide fibers10.1111/j.1151-2916.1994.tb07260.x ↗
38. Mechanical properties of the SiCf/SiC composites reinforced with KD-I and KD-II fibers fabricated assisted by a microwave heating method10.1016/j.ceramint.2019.03.223 ↗
39. Comparison of thermal stability in MAX211 and 312 phases
40. Phase stability of Ti3SiC2 at elevated temperatures10.1016/j.scriptamat.2005.08.039 ↗
41. Phase stability of Ti3SiC2 at high pressure and high temperature10.1016/j.ceramint.2013.04.111 ↗
42. Kwon · 2020
43. Synthesis of fine Ca-doped BaTiO 3 powders by solid-state reaction method—Part I: Mechanical activation of starting materials10.1007/s10832-007-9066-x ↗
44. Thermal stability of Ti3SiC2 thin films10.1016/j.actamat.2006.10.010 ↗
45. Oxidation behaviour of Ti3SiC2-based ceramic at 900–1300°C in air10.1016/S0010-938X(00)00142-6 ↗
46. High temperature oxidation resistance of Ti3SiC2 in air and low oxygen atmosphere10.1111/ijac.12746 ↗
47. Characterisation of phase relations and properties in air-oxidised Ti3SiC210.1016/j.msea.2007.02.034 ↗
48. Kink formation around indents in laminated Ti3SiC2 thin films studied in the nanoscale10.1016/S1359-6462(03)00214-8 ↗
49. Effects of temperature and atmosphere on microstructural evolution and mechanical properties of KD-II SiC fibers10.1016/j.ceramint.2020.06.225 ↗
50. Effects of SiO 2 and TiO 2 fillers on thermal and dielectric properties of eco-friendly bismuth glass microcomposites of plasma display panels10.1007/s12034-010-0005-0 ↗
51. The effect of heat treatment on the microstructure and mechanical properties of KD-II SiC fibers in air
52. Brittle interface layers and the tensile strength of metal matrix-fibre composites10.1007/BF00551024 ↗
53. Coating of carbon fibers—the strength of the fibers10.1111/j.1151-2916.1995.tb08372.x ↗
54. Gibson · 2016
55. Clyne · 2019
56. Chawla · 2012
57. Warren · 1991
58. Tensile testing of insulating thin films; humidity effect on tensile strength of SiO2 films10.1016/S0924-4247(99)00363-5 ↗
59. Determination of thermal expansion coefficient of thermal oxide
60. Effect of heat treatment on the microstructure and tensile strength of KD-II SiC fibers10.1016/j.msea.2016.07.066 ↗
61. Evaluation of a porous fiber coating in SiC–Si 3N 4 minicomposite10.1557/JMR.1997.0177 ↗
62. A porous, oxidation-resistant fiber coating for CMC interphase