Undoped Y2O3 polycrystals were densified by flash sintering under DC or AC electric field with varying holding times up to 60 min, and their chemical bonding state and crystal structure were investigated by X-ray photoelectron spectroscopy (XPS) and X-ray diffraction (XRD), respectively. Only DC flash sintering with longer holding times (≥ 30 min) resulted in blackening in cathodic regions, indicating the electrode-dependent introduction of neutral oxygen vacancies. The Y 3d3/2 and Y 3d5/2 binding energies decreased with increasing holding time in both DC- and AC-flash-sintered Y2O3 specimens, regardless of polarity, indicating that positively charged oxygen vacancies were introduced by the flash sintering in an electrode-independent manner, even under DC electric field. In addition, the XRD analysis revealed that flash-sintered specimens with longer holding times exhibited short-range structural fluctuations. These electrode-dependent and independent point defect generations under electric fields may be related to the enhanced atomic diffusion during flash sintering.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Semiconductor materials and devices · Luminescence Properties of Advanced Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (51)
Show source-provided references
1. Flash sintering of nanograin zirconia in <5 s at 850°C10.1111/j.1551-2916.2010.04089.x ↗
2. Densification behaviour and microstructural development in undoped yttria prepared by flash-sintering10.1016/j.jeurceramsoc.2013.10.031 ↗
3. Low temperature and high strain rate superplastic flow in structural ceramics induced by strong electric-field10.1016/j.scriptamat.2017.11.042 ↗
4. Athermal effect of flash event on high-temperature plastic deformation in Y2O3-stabilized tetragonal ZrO2 polycrystal10.1016/j.jeurceramsoc.2022.04.055 ↗
5. Unusual electrode-dependent deformation of 3Y-TZP induced by weak electric current in oxygen-lean atmosphere10.1016/j.scriptamat.2021.114220 ↗
6. Properties of yttrium oxide ceramics10.1111/j.1151-2916.1957.tb12619.x ↗
7. M. Foex, Investigation on the melting point of yttrium oxide (possible secondary temperature standard), High Temp. - High Press. 9, 1977, pp. 269–282. 〈https://inis.iaea.org/search/search.aspx?orig_q=RN:9370084〉 (Accessed May 16, 2022).
8. T. Yamada, M. Yoshimura, S. Somiya, Redetermination of the solidification points of Al2O3, Y2O3, and HfO2 by digital pyrometry with an arc-imaging furnace, High Temp. - High Press. 18 (1986) 377–388. 〈https://inis.iaea.org/search/search.aspx?orig_q=RN:18079046〉 (Accessed 16 May 2022).
9. Y. Tsukuda, Application for refractory and corrosion resistant materials, Jpn. Ceram. Soc. Bull. 23 (1988) 456. 〈https://cir.nii.ac.jp/crid/1372820655052290948〉 (Accessed 16 May 2022).10.1179/000705988798271108 ↗
10. Densification of Y2O3 by flash sintering under an AC electric field10.1016/j.jeurceramsoc.2021.10.029 ↗
11. Electrical characteristics of flash sintering: Thermal runaway of Joule heating10.1016/j.jeurceramsoc.2014.12.022 ↗
12. Joule heating during flash-sintering10.1016/j.jeurceramsoc.2012.02.030 ↗
13. Particle size effects in flash sintering10.1016/j.jeurceramsoc.2012.04.028 ↗
14. Reduction in sintering temperature for flash-sintering of yttria by nickel cation-doping10.1016/j.actamat.2016.01.037 ↗
15. Electric current-controlled synthesis of BaTiO310.1111/jace.14938 ↗
16. Generation of electric-field stabilized zirconium monoxide secondary phase within cubic zirconia10.1016/j.scriptamat.2020.08.026 ↗
17. Blue photoluminescence at room temperature from Y2O3-doped ZrO2 polycrystals sintered by flash sintering10.35848/1882-0786/ab7710 ↗
18. Photoluminescence properties of undoped and Si4+-doped polycrystalline Y2O3 phosphors prepared by flash-sintering10.7567/1882-0786/ab2b6e ↗
19. Variation of photoluminescence intensity depending on the timing of electric field application during isothermal flash sintering for 3 mol %Y2O3–ZrO2 polycrystal10.1016/j.ceramint.2022.06.185 ↗
20. Anelasticity induced by AC flash processing of cubic zirconia10.1016/j.actamat.2022.117704 ↗
21. Inhomogeneous reduction and its relation to grain growth of titania during flash sintering10.1016/j.scriptamat.2018.06.017 ↗
22. The densification behavior of flash sintered BaTiO310.1016/j.scriptamat.2020.05.005 ↗
23. Effects of incubation on microstructure gradient in flash-sintered TiO210.1016/j.scriptamat.2021.114270 ↗
24. Effects of electric field on microstructure evolution and defect formation in flash-sintered TiO210.1016/j.jeurceramsoc.2022.06.009 ↗
25. Microstructure and defect gradients in DC and AC flash sintered ZnO10.1016/j.ceramint.2021.07.018 ↗
26. Electric-field-assisted processing of ceramics: Nonthermal effects and related mechanisms10.1557/s43577-020-00008-w ↗
27. Discovery of electrochemically induced grain boundary transitions10.1038/s41467-021-22669-0 ↗
28. Electrode effects on microstructure formation during FLASH sintering of yttrium-stabilized zirconia10.1111/jace.14234 ↗
29. Doping effect on sinterability of polycrystalline yttria: From the viewpoint of cation diffusivity10.1016/j.jeurceramsoc.2012.04.010 ↗
30. Rietveld refinement of Y2O3 using the Pearson VII profile shape function10.1002/crat.2170240609 ↗
31. Measurement of particle sizes in opaque bodies
32. A thermal perspective of flash sintering: the effect of AC current ramp rate on microstructure evolution10.1016/j.jeurceramsoc.2020.11.040 ↗
33. X-ray electron study of oxides of elements
34. Pressure-induced structural phase transitions in Y2O3 sesquioxide10.1088/1742-6596/215/1/012003 ↗
35. Properties of black Y2O3 sintered bodies10.1016/0025-5408(81)90013-1 ↗
36. Electrochemical blackening of yttria-stabilized zirconia – morphological instability of the moving reaction front10.1016/S0167-2738(98)00415-9 ↗
37. Current-induced abnormal and oriented grain growth in corundum upon flash sintering10.1016/j.scriptamat.2018.03.004 ↗
38. Electrical properties and defect structure of Y2O310.1111/j.1151-2916.1966.tb15404.x ↗
39. Electrical conductivity of Y2O3 as a function of oxygen partial pressure in wet and dry atmospheres10.1111/j.1151-2916.1986.tb07360.x ↗
40. Tutorial on interpreting x-ray photoelectron spectroscopy survey spectra: questions and answers on spectra from the atomic layer deposition of Al2O3 on silicon
41. Defect-rich dopant-free ZrO2 nanostructures with superior dilute ferromagnetic semiconductor properties10.1021/jacs.6b06949 ↗
42. Nitrogen diffusion in nitrogen-doped yttria stabilised zirconia10.1039/B315123A ↗
43. Low-temperature spark plasma sintering of yttria ceramics with ultrafine grain size10.1111/j.1551-2916.2011.04583.x ↗
44. Order-disorder phase transformation in ion-irradiated rare earth sesquioxides10.1063/1.2720716 ↗
45. Disorder-order phase transformation in a fluorite-related oxide thin film: in-situ X-ray diffraction and modelling of the residual stress effects10.1016/j.tsf.2015.08.030 ↗
46. Oxygen vacancy, oxygen vacancy-vacancy pairs, and Frenkel defects in cubic lutetium oxide10.1021/acs.jpcc.0c00974 ↗
47. Y. Dong, L. Qi, J. Li, I.-W. Chen, Electron localization enhances cation diffusion in zirconia and ceria: A first-principles study, 2018. 〈http://arxiv.org/abs/1808.05196〉.
48. Enhanced mobility of cations and anions in the redox state: The polaronium mechanism10.1016/j.actamat.2022.117941 ↗
49. Grain growth kinetics of 3 mol. % yttria-stabilized zirconia during flash sintering10.1016/j.jeurceramsoc.2018.11.032 ↗
50. Electric current dependence of plastic flow behavior with large tensile elongation in tetragonal zirconia polycrystal under a DC field10.1016/j.scriptamat.2020.113659 ↗
51. Effect of electric current on high temperature flow behavior of 8Y-CSZ ceramics10.1016/j.jeurceramsoc.2022.01.018 ↗