Tetragonal phase stabilization and densification in AC flash-sintered 1.5 mol% yttria-stabilized zirconia polycrystals with high toughness
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (53)
Show source-provided references
1. Ceramic steel?10.1038/258703a0 ↗
2. Martensitic transformation in zirconia containing ceramics and its applications10.1016/j.cossms.2006.02.012 ↗
3. Transformation toughening10.1007/BF00809059 ↗
4. Ultrahigh toughness zirconia ceramics10.1073/pnas.2304498120 ↗
5. Higher fracture toughness of tetragonal zirconia ceramics through nanocrystalline structure10.1016/j.scriptamat.2009.03.019 ↗
6. Fracture toughness of nanocrystalline tetragonal zirconia with low yttria content10.1016/S1359-6454(02)00283-5 ↗
7. Transparent high-strength nanosized yttria stabilized zirconia obtained by pressure-less sintering10.1016/j.jeurceramsoc.2022.07.027 ↗
8. Low-temperature processing and mechanical properties of zirconia and zirconia-alumina nanoceramics10.1111/j.1151-2916.2003.tb00015.x ↗
9. Improvement of mechanical strength of 8 mol% yttria-stabilized zirconia ceramics by spark-plasma sintering10.1149/1.1456915 ↗
10. Warm pressing of zirconia nanoparticles by the spark plasma sintering technique10.1016/j.scriptamat.2008.02.015 ↗
11. Influence of the field and the current limit on flash sintering at isothermal furnace temperatures10.1111/jace.12472 ↗
12. Flash sintering of nanograin zirconia in <5 s at 850°C10.1111/j.1551-2916.2010.04089.x ↗
13. Near complete densification of flash sintered 8YSZ: controlled shrinkage rate effects10.1016/j.jeurceramsoc.2021.03.005 ↗
14. Low temperature degradation resistant nanostructured yttria-stabilized zirconia for dental applications10.1016/j.ceramint.2016.02.026 ↗
15. Flash sintering of a three‐phase alumina, spinel, and yttria‐stabilized zirconia composite10.1111/jace.14818 ↗
16. Joule heating during flash-sintering10.1016/j.jeurceramsoc.2012.02.030 ↗
17. Effect of the current density on the densification of 3 mol% yttria-stabilized zirconia in flash sintering10.1016/j.jallcom.2020.154061 ↗
18. Accessing the role of Joule heating on densification during flash sintering of YSZ10.1016/j.scriptamat.2022.114508 ↗
19. From conventional ac flash-sintering of YSZ to hyper-flash and double flash10.1016/j.jeurceramsoc.2013.03.019 ↗
20. Abnormal grain growth in DC flash sintered 3–mol% yttria‐stabilized zirconia ceramics10.1111/jace.18542 ↗
21. Effect of boundary conditions on reduction during early stage flash sintering of YSZ10.1016/j.actamat.2019.05.001 ↗
22. Investigation of electrochemical, optical and thermal effects during flash sintering of 8YSZ10.3390/ma11071214 ↗
23. Grain-size effect on cracking accumulation in yttria-doped zirconia ceramics during cyclic martensitic transformations10.1016/j.actamat.2021.116789 ↗
24. Crystallite and grain-size-dependent phase transformations in yttria-doped zirconia10.1111/j.1151-2916.2003.tb00025.x ↗
25. Densification of Y2O3 by flash sintering under an AC electric field10.1016/j.jeurceramsoc.2021.10.029 ↗
26. Chemical bonding and crystal structure in flash sintered Y2O3 under DC or AC field10.1016/j.jeurceramsoc.2023.01.062 ↗
27. Athermal effect of flash event on high-temperature plastic deformation in Y2O3-stabilized tetragonal ZrO2 polycrystal10.1016/j.jeurceramsoc.2022.04.055 ↗
28. Low-temperature degradation in yttria-stabilized tetragonal zirconia polycrystal: effect of Y3+ distribution in grain interiors10.1016/j.actamat.2022.117659 ↗
29. Vickers indentation fracture toughness of Y-TZP dental ceramics10.1016/j.ijrmhm.2016.12.016 ↗
30. Comparison between different fracture toughness techniques in zirconia dental ceramics10.1002/jbm.b.35137 ↗
31. Evaluation of KIc of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗
32. Effect of grain size on elastic modulus and hardness of nanocrystalline ZrO2–3 wt% Y2O3 ceramic10.1023/B:JMSC.0000025832.93840.b0 ↗
33. Flash sintering scaling-up challenges: influence of the sample size on the microstructure and onset temperature of the flash event10.1016/j.scriptamat.2020.04.022 ↗
34. Influence of forming methods on the microstructure of 3YSZ flash-sintered ceramics10.1016/j.mtla.2022.101419 ↗
35. Elastic-plastic indentation: hardness and fracture10.1016/0043-1648(77)90021-7 ↗
36. Shrinkage rate control during a flash state by current‐ramping for 3 mol% Y2O3–doped ZrO2 polycrystals10.1111/jace.17912 ↗
37. Phase relationships in the zirconia-yttria system10.1007/BF01031853 ↗
38. The tetragonal-monoclinic transformation in zirconia: lessons learned and future trends10.1111/j.1551-2916.2009.03278.x ↗
39. Neck formation and self-adjusting mechanism of neck growth of conducting powders in spark plasma sintering10.1111/j.1551-2916.2005.00777.x ↗
40. Local field strengths during early stage field assisted sintering (FAST) of dielectric materials10.1016/j.jeurceramsoc.2012.03.012 ↗
41. Microstructural temperature gradient-driven diffusion: Possible densification mechanism for flash sintering of zirconia?10.1016/j.ceramint.2018.09.311 ↗
42. Transformation behaviour of tetragonal zirconia: role of dopant content and distribution10.1016/j.msea.2003.08.063 ↗
43. Microstructure and surface segregation of 3 mol% Y2O3-doped ZrO2 particles10.1111/j.1551-2916.2006.01132.x ↗
44. Synthesis of yttria-stabilized zirconia nanoparticles by heating of alcohol-aqueous salt solutions10.1016/S0965-9773(98)00128-7 ↗
45. Effect of the introduction procedure and concentration of yttrium cations on the crystal structure of (1–x)ZrO2·xY2O3 powders10.1134/S0036023616110164 ↗
46. Current-ramp assisted sintering of 3YSZ: Electrochemical and microstructural comparison to flash and thermal sintering10.1016/j.jeurceramsoc.2019.09.036 ↗
47. Temperature gradient and microstructure evolution in AC flash sintering of 3 mol% yttria-stabilized zirconia10.1080/10426914.2016.1232814 ↗
48. Grain growth kinetics of 3 mol. % yttria-stabilized zirconia during flash sintering10.1016/j.jeurceramsoc.2018.11.032 ↗
49. Influence of the forming method on flash sintering of ZnO ceramics10.1016/j.ceramint.2020.08.210 ↗
50. Field assisted and flash sintering of alumina and its relationship to conductivity and MgO-doping10.1016/j.jeurceramsoc.2011.07.004 ↗
51. Flash sintering of dense alumina ceramic discs with high hardness10.1016/j.jeurceramsoc.2021.09.061 ↗
52. Effect of agglomeration on mechanical properties of porous zirconia fabricated by partial sintering10.1111/j.1151-2916.2002.tb00388.x ↗
53. Indentation microfracture in the Palmqvist crack regime: implications for fracture toughness evaluation by the indentation method10.1007/BF00721938 ↗