The high-temperature CMAS corrosion behavior of high-entropy (La0.2Nd0.2Sm0.2Eu0.2Gd0.2)2Hf2O7 hafnate thermal barrier coating material with fluorite structure
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Thermal barrier coatings for gas-turbine engine applications10.1126/science.1068609 ↗
2. Overview on advanced thermal barrier coatings10.1016/j.surfcoat.2010.08.151 ↗
3. The hotter the engine, the better10.1126/science.1179327 ↗
4. Thermochemical interaction of thermal barrier coatings with molten CaO-MgO-Al2O3-SiO2 (CMAS) deposits10.1111/j.1551-2916.2006.01209.x ↗
5. Mechanism of crack nucleation and growth in YSZ thermal barrier coatings corroded by CMAS at high temperatures: first-principles calculation10.1016/j.corsci.2018.07.033 ↗
6. Graceful behavior during CMAS corrosion of a high-entropy rare-earth zirconate for thermal barrier coating material10.1016/j.jeurceramsoc.2021.10.022 ↗
7. Hot corrosion behavior and wettability of calcium–magnesium–alumina–silicate (CMAS) on LaTi2Al9O19 ceramic10.1016/j.corsci.2019.108199 ↗
8. TBC experience in landbased gas turbines10.1007/s11666-997-0009-5 ↗
9. Methods to reduce the thermal conductivity of EB-PVD TBCs10.1016/S0257-8972(01)01651-6 ↗
10. High-temperature interaction of yttria stabilized zirconia coatings with CaO–MgO–Al2O3–SiO2 (CMAS) deposits10.1016/j.surfcoat.2009.07.034 ↗
11. Step-by-step investigation of degradation mechanisms induced by CMAS attack on YSZ materials for TBC applications10.1016/j.surfcoat.2013.08.055 ↗
12. CMAS resistance characteristics of LaPO4/YSZ thermal barrier coatings at 1250°C–1350°C10.1016/j.corsci.2019.04.014 ↗
13. Entropy-stabilized oxides, J.P. Maria10.1038/ncomms9485 ↗
14. High-entropy ceramics: Present status, challenges, and a look forward10.1007/s40145-021-0477-y ↗
15. (La0.2Ce0.2Nd0.2Sm0.2Eu0.2)2Zr2O7: A novel high-entropy ceramic with low thermal conductivity and sluggish grain growth rate10.1016/j.jmst.2019.05.054 ↗
16. Dual-phase rare-earth-zirconate high-entropy ceramics with glass-like thermal conductivity10.1016/j.jeurceramsoc.2020.11.047 ↗
17. Ultrafast high-temperature sintering of (Y0.2Dy0.2Er0.2Tm0.2Yb0.2)4Hf3O12 high-entropy ceramics with defective fluorite structure10.1016/j.jeurceramsoc.2022.04.023 ↗
18. High temperature corrosion of (Er0.25Tm0.25Yb0.25Lu0.25)2Si2O7 environmental barrier coating material subjected to water vapor and molten calcium–magnesium–aluminosilicate (CMAS)10.1016/j.corsci.2020.108881 ↗
19. Investigation on improving corrosion resistance of rare earth pyrosilicates by high-entropy design with RE-doping10.1016/j.corsci.2022.110217 ↗
20. Calcium-magnesium-alumina-silicate (CMAS) resistant high entropy ceramic (Y0.2Gd0.2Er0.2Yb0.2Lu0.2)2Zr2O7 for thermal barrier coatings10.1016/j.jmst.2021.07.053 ↗
21. Ultrafast high-temperature sintering (UHS) of fine grained α-Al2O310.1016/j.jeurceramsoc.2021.05.056 ↗
22. Ultrafast high-temperature sintering of silicon nitride: A comparison with the state-of-the-art techniques10.1016/j.jeurceramsoc.2021.06.021 ↗
23. Ultrafast high-temperature sintering (UHS) of Li1.3Al0.3Ti1.7(PO4)310.1016/j.ceramint.2021.04.216 ↗
24. Li7La3Zr2O12 solid electrolyte sintered by the ultrafast high-temperature method10.1016/j.jeurceramsoc.2021.05.041 ↗
25. Ultrafast high-temperature sintering of high-entropy (La0.2Nd0.2Sm0.2Eu0.2Gd0.2)2Hf2O7 ceramics with fluorite structure10.1016/j.ceramint.2022.09.041 ↗
26. Pyrochlore Rare-Earth Hafnate RE2Hf2O7 (RE = La and Pr) Nanoparticles Stabilized by Molten-Salt Synthesis at Low Temperature10.1021/acs.inorgchem.8b02728 ↗
27. CMAS corrosion behavior of Sc doped Gd2Zr2O7 /YSZ thermal barrier coatings and their corrosion resistance mechanisms10.1016/j.corsci.2021.109899 ↗
28. Review of non-reactive and reactive wetting of liquids on surfaces10.1016/j.cis.2007.04.009 ↗