journal article·2021-05

SiC/SiC mini-composites with yttrium disilicate fiber coatings: Oxidation in steam

Emmanuel E. Boakye, Thomas S. Key, Pavel Mogilevsky, Samuel J. Opeka, Randall Corns, Randall S. Hay, Michael K. Cinibulk

Publisher page

Abstract

Abstract Solutions of YPO4 were used to precipitate YPO4 on pre-oxidized Hi-Nicalon-S SiC fibers. Tows of the coated fibers were then infiltrated with a preceramic polymer loaded with SiC particles to form mini-composites. During pyrolysis of the matrix, SiO2 and YPO4 on the fibers reacted and formed a Y2Si2O7 fiber matrix interphase. Mini-composites were exposed to steam at 1000 °C for 10, 50, and 100 h, tensile tested, and the effect of oxidation in steam on the functionality of the Y2Si2O7 fiber coating was investigated. The minicomposites oxidized at 1000 °C for 10 h retained 100 % of their unoxidized strength, and those oxidized for 50 and 100 h retained 92 % and 90 % of unoxidized strength, respectively. Strength retention and fiber pullout in both unoxidized and oxidized minicomposites suggests that the Y2Si2O7 interphase was effective in maintaining a weak fiber-matrix interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (42)

Show source-provided references
1. Ceramic matrix composites taking flight at GE aviation
2. Oxidation-resistant Fiber coatings for non-oxide ceramic composites10.1111/j.1151-2916.1997.tb03263.x ↗
3. Modeling environmentally induced property degradation of SiC/BN/SiC ceramic matrix composites10.1111/jace.15325 ↗
4. Effect of a boron nitride interphase that debonds between the interphase and the matrix in SiC/SiC composites10.1111/j.1551-2916.2004.00104.x ↗
5. The concept of a strong interface applied to SiC/SiC composites with a BN interphase10.1016/S1359-6454(00)00247-0 ↗
6. Interfacial characterization of a slurry-cast melt-infiltrated SiC/SiC ceramic-matrix composite10.1016/S1359-6454(00)00248-2 ↗
7. Interface design for oxidation resistant ceramic composites10.1111/j.1151-2916.2002.tb00505.x ↗
8. Degradation of a SiC-SiC composite in water vapor environments10.1111/jace.16838 ↗
9. Intermediate temperature oxidative strength degradation of a SiC/SiNC composite with a polymer-derived matrix10.1111/jace.14741 ↗
10. Ceramics Matrix Composites enable revolutionary gains in turbine efficiency
11. Pest-resistance in SiC/BN/SiC composites10.1016/S0955-2219(02)00268-6 ↗
12. Degradation of SiC/BN/SiC composite in the burner rig10.1002/9780470294499.ch29 ↗
13. Oxidation-resistant interfacial coatings for continuous Fiber ceramic composites10.1002/9780470314715.ch43 ↗
14. Multilayered oxide interphase concept for ceramic-matrix composites10.1111/j.1151-2916.1998.tb02396.x ↗
15. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics10.1016/j.jeurceramsoc.2004.12.013 ↗
16. Silica activity measurements in the Y2O3-SiO2 system and applications to modeling of coating volatility10.1111/jace.12974 ↗
17. Evaluation of SiC/SiC minicomposites with yttrium disilicate fiber coatings10.1111/jace.15170 ↗
18. Processing and testing of RE2Si2O7 fiber–matrix interphases for SiC–SiC composites10.1111/jace.13935 ↗
19. Rare-earth disilicates as oxidation-resistant fiber coatings for silicon carbide ceramic matrix composites10.1111/j.1551-2916.2010.04306.x ↗
20. Mechanical properties and atomistic deformation mechanism of □-Y2Si2O7 from first-principles investigations10.1016/j.actamat.2007.07.010 ↗
21. Damage tolerance and extensive plastic deformation of β-Yb2Si2O7 from room to high temperatures10.1111/jace.13702 ↗
22. Interfacial bond strength in SiC/C/SiC composite materials, as studied by single-fiber push-out tests10.1111/j.1151-2916.1998.tb02434.x ↗
23. Hi-nicalon fiber-reinforced celsian matrix composites: influence of interface modification10.1557/JMR.1998.0213 ↗
24. Interface properties in high-strength Nicalon/C/SiC composites, as determined by rough surface analysis of fiber push-out tests10.1111/j.1151-2916.1998.tb02561.x ↗
25. 2016
26. In Situ-Y2Si2O7 coatings on Hi-Nicalon-S SiC fibers: phase formation and Fiber strength10.1111/jace.16428 ↗
27. Passive oxidation kinetics for glass and cristobalite formation on Hi-Nicalon-S SiC fibers in steam10.1111/jace.15763 ↗
28. Validity of using average diameter for determination of tensile strength and Weibull Modulus of ceramic filaments10.1111/j.1151-2916.1997.tb03188.x ↗
29. D4018-81, A. S. f. & Materials, T. a. (West Conshohocken, PA, 1981).
30. Materials, A. S. f. T. a. in C1557-14 (West Conshohocken, PA, 2014).
31. Oxidation kinetics strength of Hi-Nicalon-S SiC Fiber After oxidation in dry and wet air10.1111/jace.14833 ↗
32. Model for SiC Fiber strength after oxidation in dry and wet air10.1111/jace.15907 ↗
33. Model for SiC Fiber strength after oxidation in dry and wet air10.1111/jace.15907 ↗
34. Fiber strength of Hi-Nicalon-S after oxidation and scale crystallization in Si(OH)4 saturated steam10.1002/9781119320104.ch10 ↗
35. SiC Fiber strength after low pO2 oxidation10.1111/jace.15198 ↗
36. Zirconia-silica-Carbon coatings on ceramic fibers10.1111/j.1151-2916.2004.tb06348.x ↗
37. Kelly · 1986
38. On the strength of classical fibers and Fiber bundles10.1016/0022-5096(58)90039-5 ↗
39. Evaluation of monazite Fiber coatings in dense matrix composites10.1002/9780470294567.ch52 ↗
40. Evaluation of Porous ZrO2-SiO2 and Monazite coatings using Nextel™ 720 Fiber-Reinforced Blackglas Matrix Minicomposites10.1111/j.1151-2916.2001.tb00872.x ↗
41. Evaluation of SiC/SiC minicomposites with yttrium disilicate Fiber coatings
42. Effectiveness of monazite coatings in Oxide/Oxide composites after long term exposure at high temperature10.1111/j.1151-2916.2003.tb00018.x ↗