Low-temperature reactive spark plasma sintering of dense SiC-Ti3SiC2 ceramics
Source abstract
Abstract
SiC-based ceramics are of great interest for various advanced applications. However, its fabrication requires high-temperature treatment at ∼2000 – 2100 °С. In this study, we developed an approach based on low-temperature reactive spark plasma sintering to produce dense SiC-based ceramics with superior mechanical properties. It was found that an SPS temperature of 1600 °C and introduction of 10 – 15 wt% of mechanically activated non-oxide Ti–Si–C additive is required to manufacture ceramics with a theoretical density of higher than 90%. Nonetheless, employing 5 – 15 wt% of the additive mixture and an SPS temperature of 1700 °C, the maximum density of ∼ 98% was achieved. The controlled formation and decomposition of the in-situ Ti3SiC2 MAX phase enables the fabrication of the engineering ceramics with enhanced compressive strength (550 MPa), elastic modulus (485 GPa), and microhardness (32 GPa), which are comparable to the best-reported SiC ceramics. The study has a significant potential for practical application in the production of advanced SiC-based ceramics for various purposes and could be used for further understanding and development of the high-temperature sintering methods.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Silicon carbide: synthesis and properties
2. Self-propagating high-temperature synthesis of silicon carbide nanopowders10.1134/S0012501613030032 ↗
3. Riedel · Handbook of Ceramic Hard Materials · 200010.1002/9783527618217 ↗
4. Silicon Carbide, III-Nitrides and Related Materials
5. Particle size effect of starting SiC on processing, microstructures and mechanical properties of liquid phase-sintered SiC10.1016/j.jeurceramsoc.2010.02.026 ↗
6. SiC/SiC composites through transient eutectic-phase route for fusion applications10.1016/j.jnucmat.2004.04.157 ↗
7. Large‐band‐gap SiC, III‐V nitride, and II‐VI ZnSe‐based semiconductor device technologies10.1063/1.358463 ↗
8. Design and material issues for high performance SiCf/SiC-based fusion power cores10.1016/S0920-3796(01)00181-8 ↗
9. Advanced materials for fusion technology10.1016/j.fusengdes.2005.08.008 ↗
10. Reactive spark plasma sintering of NiAl intermetallics: A comparative study10.1016/j.intermet.2022.107750 ↗
11. The effect of carbon on surface quality of solid-state-sintered silicon carbide as optical materials10.1016/j.matchar.2013.12.005 ↗
12. Effect of additive content on liquid-phase sintering on silicon carbide ceramics10.1016/S0025-5408(99)00172-5 ↗
13. Sintering of silicon carbide I. Effect of carbon10.1016/S0272-8842(02)00117-7 ↗
14. Sintering of silicon carbide II. Effect of boron10.1016/S0272-8842(02)00144-X ↗
15. Effect of microstructure on the mechanical properties of liquid-phase-sintered silicon carbide at pre-creep temperatures10.1016/j.jeurceramsoc.2011.01.003 ↗
16. Effects of additives on densification, microstructure and properties of liquid-phase sintered silicon carbide10.1023/A:1004881430804 ↗
17. Effect of particle dispersion on microstructure and strength of reaction-bonded silicon carbide10.1016/S0921-5093(01)01897-4 ↗
18. Reactive flash spark plasma sintering of alumina reinforced by silicon carbide nanocomposites: physicochemical study
19. Development of high-strength reaction-sintered silicon carbide10.1016/S0925-9635(03)00066-9 ↗
20. Large-scale fabrication of lightweight Si/SiC ceramic composite optical mirror10.1016/j.matlet.2003.09.010 ↗
21. Preparation of reaction bonded silicon carbide (RBSC) using boron carbide as an alternative source of carbon10.1016/j.jeurceramsoc.2010.11.032 ↗
22. Effect of TiSi2/Ti3SiC2 matrix phases in a reaction-bonded SiC on mechanical and high-temperature oxidation properties10.1016/j.jeurceramsoc.2016.01.015 ↗
23. Preparation of SiC/SiC composites by hot pressing, using Tyranno-SA fiber as reinforcement10.1111/j.1151-2916.2003.tb03272.x ↗
24. Additive-free hot-pressed silicon carbide ceramics—a material with exceptional mechanical properties10.1016/j.jeurceramsoc.2015.12.013 ↗
25. Processing of nano-SiC ceramics: densification by SPS and mechanical characterization10.1016/j.jeurceramsoc.2011.10.006 ↗
26. Role of boron on the Spark Plasma Sintering of an α-SiC powder10.1016/j.jeurceramsoc.2008.01.002 ↗
27. The spark plasma sintering of silicon carbide ceramics using alumina10.12693/APhysPolA.125.257 ↗
28. Z.A. Yasar, R.A. Haber, W. Rafaniello, SPS sintered silicon carbide-boron carbide composites, in: Advances in Ceramic Armor, Bioceramics, and Porous Materials, 2017, pp. 13–20–13–20.10.1002/9781119321682.ch2 ↗
29. Sintering behavior of spark plasma sintered SiC with Si-SiC composite nanoparticles prepared by thermal DC plasma process10.1186/s11671-017-2370-8 ↗
30. Spark plasma sintering of SiC ceramics based on natural renewable raw materials10.4028/www.scientific.net/MSF.992.759 ↗
31. Short SiC fiber/Ti3SiC2 MAX phase composites: fabrication and creep evaluation10.1111/jace.17337 ↗
32. Development of pore-free Ti-Si-C MAX/Al-Si composite materials manufactured by squeeze casting infiltration10.1007/s11665-019-04390-8 ↗
33. Joining of SiC ceramic-based materials with ternary carbide Ti3SiC210.1016/j.mseb.2010.09.002 ↗
34. Novel Cr2AlC MAX-phase/SiC fiber composites: synthesis, processing and tribological response10.1016/j.jeurceramsoc.2016.09.029 ↗
35. The Ti3SiC2 max phases as promising materials for high temperature applications: formation under various synthesis conditions10.1016/j.matchemphys.2021.124625 ↗
36. Study of the synthesis of MAX phase Ti3SiC2 powders by pressureless sintering10.1016/j.bsecv.2020.01.004 ↗
37. On the interactions of Ti2AlC, Ti3AlC2, Ti3SiC2 and Cr2AlC with silicon carbide and pyrolytic carbon at 1300 °C10.1016/j.jeurceramsoc.2015.07.029 ↗
38. I.M. Low, W.K. Pang, Decomposition kinetics of MAX phases in extreme environments, in: I.M. Low et al. (Eds.), MAX Phases and Ultra-High Temperature Ceramics for Extreme Environments, IGI Global, 2013, pp. 34–48.10.4018/978-1-4666-4066-5.ch002 ↗
39. Phase evolution of Ti3SiC2Annealing in vacuum at elevated temperatures
40. In situ synthesis of Ti3SiC2/SiC composite by displacement reaction of Si and TiC10.1016/j.msea.2004.03.046 ↗
41. R. Radhakrishnan, S.B.Bhaduri, J.C.H. Henager, Analysis on the sequence of formation of Ti3SiC2 and Ti3SiC2/SiC composites, in: International Conference and Exhibition on Powder Metallurgy and Partuculate Materials, Seattle, WA, 1995, pp. 129–137.
42. Solid-state synthesis and characterization of the ternary phase Ti3SiC210.1007/BF00352037 ↗
43. Microindentation and macroindentation of titanium silicon carbide Ti3SiC210.1007/s11106-005-0078-2 ↗
44. A progress report on Ti3SiC2, Ti3GeC2, and the H-phases, M2BX
45. CRC Materials Science and Engineering Handbook
46. Processing phenomena for recrystallized silicon carbide
47. P. Liang, J. Wu, J. Han, G. Wang, Q. Zhang, L. Li, Effects of SiC micro-powder content on properties of RSiC porous ceramics supports, IOP Conf. Ser. Mater. Sci. Eng. 678 (2019) 012096–012096.10.1088/1757-899X/678/1/012096 ↗
48. Progress and applications of recrystallized SiC and its composites10.1360/N972014-00446 ↗
49. High-temperature strength and toughness behaviors for reaction-bonded SiC ceramics below 1400 °C10.1016/j.matlet.2005.01.049 ↗
50. Effect of oxidation on the room-temperature flexural strength of reaction-bonded silicon carbides10.1111/j.1151-2916.1999.tb01967.x ↗
51. The influence of nanosize carbon concentration on mechanical properties of RBSIC
52. Reaction-bonded silicon carbide by reactive infiltration10.1021/ie001029e ↗
53. Mechanical behaviour of silicon-silicon carbide composites10.1016/0955-2219(95)00199-9 ↗
54. The fabrication of reaction-formed silicon carbide with controlled microstructure by infiltrating a pure carbon preform with molten Si10.1016/S0272-8842(03)00128-7 ↗
55. Solid state sintering of SiC-ceramics10.4028/www.scientific.net/MSF.624.71 ↗
56. Sintering and microstructure of silicon carbide ceramic with Y3Al5O12 added by sol-gel method10.1631/jzus.2005.B0213 ↗
57. High-temperature properties of liquid-phase-sintered α-SiC10.1016/S0921-5093(99)00769-8 ↗
58. Effect of additive content on the mechanical and thermal properties of pressureless liquid-phase sintered SiC10.1080/21870764.2020.1749376 ↗
59. Low temperature pressureless sintering of α-SiC with Al2O3 and CeO2 as additives10.1016/j.jeurceramsoc.2013.09.015 ↗
60. Microstructure and mechanical properties of silicon carbide processed by Spark Plasma Sintering (SPS)10.1016/j.ceramint.2012.05.003 ↗