Abstract
Abstract Cubic silicon carbide (3C-SiC) ceramics are one of the most promising candidates for structural materials in future fusion reactors. In a fusion environment, irradiation of high-energy neutrons induces a large number of point defects and many transmutants (H, He, Li, Be, B, Mg, Al and P). The interaction of irradiation-induced point defects with the transmutants affects the evolution of micro structure in 3C-SiC, however, the micro processes are still mysterious. In this work, we carry out systematical ab initio calculations concerning the interaction of irradiation-induced point defects with the transmutants in 3C-SiC. It is found that Li and Be atoms prefer to occupy the tetrahedral interstitial site surrounding by four carbon atoms. B atom is favorable to occupy the substitutional site of carbon, while Mg, Al, and P atoms prefer to occupy the substitutional site of silicon. Moreover, only B, Mg and Al pairs have positive binding energies, which suggests that B, Mg, and Al pairs tend to segregate and form clusters at substitutional sites. Vacancy and self-interstitial atom can act as trapping centers for transmutants, especially for Mg. The electron density and the volume difference are analyzed to understand the underlying reasons controlling the interaction of point defects with transmutants.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silicon Carbide Semiconductor Technologies · Semiconductor materials and devices · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. Handbook of SiC properties for fuel performance modeling10.1016/j.jnucmat.2007.05.016 ↗
2. Diffusion of fission products and radiation damage in SiC10.1088/0022-3727/46/47/473001 ↗
3. Continuous SiC fiber, CVI SiC matrix composites for nuclear applications: Properties and irradiation effects10.1016/j.jnucmat.2013.06.040 ↗
4. Designing radiation resistance in materials for fusion energy10.1146/annurev-matsci-070813-113627 ↗
5. Radiation effects in SiC for nuclear structural applications10.1016/j.cossms.2012.03.005 ↗
6. Current status and recent research achievements in SiC/SiC composites10.1016/j.jnucmat.2014.06.003 ↗
7. Silicon carbide composite for light water reactor fuel assembly applications10.1016/j.jnucmat.2013.12.004 ↗
8. Promise and challenges of SiCf/SiC composites for fusion energy applications10.1016/S0022-3115(02)00976-5 ↗
9. Displacement damage in silicon carbide irradiated in fission reactors10.1016/j.jnucmat.2004.02.012 ↗
10. Damage production and accumulation in SiC structures in inertial and magnetic fusion systems10.1016/j.jnucmat.2010.12.077 ↗
11. Transmutation of silicon carbide in fusion nuclear environment10.1016/j.jnucmat.2012.11.018 ↗
12. Effect of H and He irradiation on cavity formation and blistering in ceramics10.1016/j.nimb.2012.03.030 ↗
13. A comparison of defects in helium implanted in α- and β-SiC10.1016/S0022-3115(00)00211-7 ↗
14. Swelling of SiC under helium implantation10.1063/1.2137441 ↗
15. Experimental simulation of the effect of transmuted helium on the mechanical properties of silicon carbide10.1016/S0022-3115(02)01052-8 ↗
16. Surface blistering of ion irradiated SiC studied by grazing incidence electron microscopy10.1016/S0022-3115(02)01271-0 ↗
17. Helium-bubble formation behavior of SiCf/SiC composites after helium implation10.1016/S0022-3115(98)00619-9 ↗
18. Effect of helium on radiattion damage in a SiC/C composites10.1016/S0272-8842(99)00087-5 ↗
19. The influences of irradiation temperatures and helium production on the dimensional stability of silicon carbide10.1016/S0022-3115(02)01062-0 ↗
20. Synergistic Effects of Heavy Ion and Helium Irradiation on Microstructural and Dimensional Change in β-SiC10.2320/matertrans.46.1388 ↗
21. Irradiation-induced microstructural change in helium-implanted single crystal and nano-engineered SiC10.1016/j.jnucmat.2014.07.020 ↗
22. In-situ evolution of helium bubbles in SiC under irradiation10.1063/1.4936562 ↗
23. Evolution of Helium Platelets and Associated Dislocation Loops in α-SiC10.1103/PhysRevLett.82.2709 ↗
24. Microstructural evolution of helium-implante α-SiC10.1103/PhysRevB.61.12923 ↗
25. Dose dependence of formation of nanoscale cavities in helium-implanted 4H-SiC10.1063/1.1611630 ↗
26. Evolution of defects in silicon carbide implanted with helium ions10.1016/j.nimb.2013.10.064 ↗
27. Dose dependence of helium bubble formation in nano-engineered SiC at 700 °C10.1016/j.jnucmat.2016.01.029 ↗
28. Magnesium behavior and structural defects in Mg+ ion implanted silicon carbide10.1016/j.jnucmat.2014.12.071 ↗
29. Precipitates and voids in cubic silicon carbide implanted with 25Mg+ ions10.1016/j.jnucmat.2017.10.046 ↗
30. The effect of irradiation-induced point defects on energetics and kinetics of hydrogen in 3C-SiC in a fusion environment10.1088/1741-4326/aa6b82 ↗
31. The stability of vacancy clusters and their effect on helium behaviors in 3C-SiC10.1016/j.jnucmat.2018.03.010 ↗
32. Mechanism for hydrogen-promoted information of helium polymer in silicon carbide material: A diffusion study10.1016/j.jallcom.2015.06.107 ↗
33. The energetics of helium and hydrogen atoms in β-SiC: an ab initio approach10.1007/s10853-008-3180-2 ↗
34. First principles calculation of noble gas atoms properties in 3C-SiC10.1016/j.jnucmat.2012.06.022 ↗
35. Theoretical study of helium insertion and diffusion in 3C-SiC10.1016/j.jnucmat.2005.09.006 ↗
36. He-vacancy interaction and multiple He trapping in small void of silicon carbide10.1016/j.jnucmat.2014.10.062 ↗
37. Interaction between helium and intrinsic point defects in 3C-SiC single crystal10.1063/1.4985604 ↗
38. Thermodynamic and kinetic properties of intrinsic defects and Mg transmutants in 3C-SiC determined by density functional theory10.1016/j.jnucmat.2014.01.035 ↗
39. Impurity-controlled dopant activation: Hydrogen-determined site selection of boron in silicon carbide10.1063/1.1410337 ↗
40. Different roles of carbon and silicon interstitials in the interstitial-mediated boron diffusion in SiC10.1103/PhysRevB.70.115203 ↗
41. First-principles studies of the diffusion of B impurities and vacancies in SiC10.1103/PhysRevB.69.125203 ↗
42. Ab initio molecular dynamics for liquid metals10.1103/PhysRevB.47.558 ↗
43. Efficient iterative schemes for Ab initio total-energy calculations using a plane-wave basis set10.1103/PhysRevB.54.11169 ↗
44. Self-consistent equations including exchange and correlation effects10.1103/PhysRev.140.A1133 ↗
45. Special points for Brillouin-zone integrations10.1103/PhysRevB.13.5188 ↗
46. Ab initio pseudopotential study of structural and high-pressure properties of SiC10.1103/PhysRevB.35.8196 ↗
47. Hydrogen as a Cause of Doping in Zinc Oxide10.1103/PhysRevLett.85.1012 ↗
48. First-principle calculations for defects and impurities: Applications to III-nitrides10.1063/1.1682673 ↗
49. Interplay of solute-mixed self-interstitial atoms and substitutional solutes with interstitial and substitutional helium atoms in tungsten-transition metal alloys10.1088/1741-4326/aaf297 ↗
50. Experimental location of helium atoms in 6H-SiC crystal lattice after implantation and after annealing at 400°C10.1016/j.jnucmat.2014.12.118 ↗
51. Ag diffusion in cubic silicon carbide10.1016/j.jnucmat.2010.10.088 ↗
52. Studies of hydrogen in semiconductors using the positive muon as a proton analogue10.1098/rsta.1995.0006 ↗
53. The first 25 years of semiconductor muonics at ISIS, modelling the electrical activity of hydrogen in inorganic semiconductors and high-dielectrics10.1088/0031-8949/88/06/068503 ↗
54. Similarities, differences, and trends in the properties of interstitial H in cubic C, Si, BN, BP, AlP, and SiC10.1103/PhysRevB.42.9486 ↗
55. Dynamic hydrogen isotope behavior and its chemical states in SiC by XPS and TDS technique10.1016/j.jnucmat.2004.07.057 ↗
56. Temperature dependence of hydrogen isotope behaviors in non-He+ pre-implanted SiC and He+ pre-implanted SiC10.1016/j.fusengdes.2007.06.033 ↗
57. Helium interaction with vacancy-type defects created in silicon carbide single crystal10.1016/j.jnucmat.2013.01.288 ↗
58. Helium implantation defects in SiC: A thermal helium desorption spectrometry investigation10.1063/1.1527974 ↗
59. Clustering of transmutation elements tantalum, rhenium and osmium in tungsten in a fusion environment10.1088/1741-4326/aa70b2 ↗