journal article·2023-04

Effects of molten Na2SO4 on wet oxidation behavior of SiCf/SiC composites above 1200 ℃

Feiyu Guo, Xiaowu Chen, Jinshan Yang, Xiangyu Zhang, Chunjing Liao, Jianbao Hu, Haijun Zhou, Shaoming Dong

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Ceramic-matrix composites take the heat10.1557/mrs.2015.283 ↗
2. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
3. Accelerated oxidation of SiC CMC's by water vapor and protection via environmental barrier coating approach10.1016/S0955-2219(02)00141-3 ↗
4. Influences of coexisting O-2 in H2O-annealing ambient on thermal oxidation kinetics and MOS interface properties on 4H-SiC (1-100)10.1016/j.mssp.2020.105147 ↗
5. Degradation of a SiC-SiC composite in water vapor environments10.1111/jace.16838 ↗
6. Hot-corrosion of silicon carbide in combustion gases at temperatures above the dew point of salts10.1016/S0955-2219(98)00239-8 ↗
7. Molten salt corrosion of SiC and Si3N4 ceramics10.1111/j.1151-2916.1976.tb10962.x ↗
8. Oxidation behaviour of SiC fibre reinforced SiC10.1016/0022-3115(95)00133-6 ↗
9. Oxidation behavior of silicon carbide10.1111/j.1151-2916.1958.tb12932.x ↗
10. Oxidation and volatilization of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
11. Thermodynamic properties of Si(OH)4(g) based on combined experimental and quantum chemistry data10.1111/jace.15922 ↗
12. High-temperature Na2SO4 deposit-assisted corrosion of silicon carbide - I: temperature and time dependence10.1111/jace.13409 ↗
13. SiC recession caused by SiO2Scale volatility under combustion conditions: I, experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
14. Optimizing microstructure and properties of SiCf/SiC composites prepared by reactive melt infiltration
15. Na2SO4 deposit‐induced hot corrosion of BN‐coated α‐SiC10.1111/jace.17576 ↗
16. Polymorphism of silica10.1023/A:1018636920023 ↗
17. Thermal change in unit-cell dimensions, and a hexagonal structure of tridymite10.1524/zkri.1978.148.3-4.237 ↗
18. Crystal structures of quartz and magnesium germanate by profile analysis of synchrotron-radiation high-resolution powder data10.1107/S0021889887011567 ↗
19. Effects of impurities and manufacturing methods on the devitrification of silica fibers10.1111/j.1151-2916.1991.tb04352.x ↗
20. Molecular diffusion of oxygen and water in crystalline and amorphous silica10.1080/13642819208207643 ↗
21. Oxidation kinetics of silicon carbide crystals and ceramics: I, in dry oxygen10.1111/j.1151-2916.1986.tb07470.x ↗
22. High‐temperature Na2SO4 deposit‐assisted corrosion of silicon carbide– II: Effects of B, C, and Si10.1111/jace.14596 ↗
23. Interactions of water vapor with oxides at elevated temperatures10.1016/j.jpcs.2004.06.044 ↗
24. The system sodium oxide-silica10.1021/j150313a018 ↗
25. Na2SO4 deposit‐induced hot corrosion of SiC fibers relevant for SiC CMCs10.1111/jace.17982 ↗