journal article·2024-07

Investigation of pore structure and high-temperature fracture behavior of lamellar hydrates bonded alumina-spinel castables

Yawei Li, Wenjing Liu, Ning Liao, Mithun Nath, Shengnian Tie, Xin Liu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Magnesium Oxide Properties and Applications · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. Thermomechanical finite element modeling of steel ladle containing alumina spinel refractory lining10.1016/j.finel.2022.103762 ↗
2. Erosion and corrosion of alumina refractory by ingot casting steels10.1016/j.jeurceramsoc.2015.11.038 ↗
3. In-depth microstructural evolution analyses of cement-bonded spinel refractory castables: novel insights regarding spinel and ca6 formation10.1111/j.1551-2916.2012.05161.x ↗
4. Mechanical property and phase evolution of the hydrates of CAC-bonded alumina castables during drying at 110 °C10.1016/j.conbuildmat.2020.120962 ↗
5. In-depth investigation of pore structure and fracture behavior of CAC bonded alumina-spinel castables treated at 110–1600 °C
6. Calcium aluminate cement in castable alumina: From hydrate bonding to the in situ formation of calcium hexaluminate10.1016/j.ceramint.2021.02.066 ↗
7. The effect of temperature on the formation of the hydrated calcium aluminate cement structure10.1016/j.proeng.2013.04.015 ↗
8. Effect of curing temperature and water-to-cement ratio on corrosion of steel in calcium aluminate cement concrete10.1016/j.conbuildmat.2022.128875 ↗
9. Effects of accelerating and retarding agents on nucleation and crystal growth of calcium aluminate cement
10. Stability in the system CaO-Al2O3-H2O10.1016/j.cemconres.2012.09.002 ↗
11. In-situ XRD study of the temperature-dependent early hydration of calcium aluminate cement in a mix with calcite10.1016/j.cemconres.2020.106160 ↗
12. Effects of characteristic hydrates on the pore structure and fracture behavior of CAC bonded alumina-spinel castables10.1016/j.conbuildmat.2023.131736 ↗
13. Conversion of calcium aluminate cement hydrates at 60 °C with and without water10.1111/jace.15505 ↗
14. Effect of CaSO4 on hydration and phase conversion of calcium aluminate cement10.1016/j.conbuildmat.2019.07.004 ↗
15. CaCO3 addition effect on the hydration and mechanical strength evolution of calcium aluminate cement for endodontic applications10.1016/j.ceramint.2011.09.021 ↗
16. Assessment of fracture behavior of mono-carbonate (C4AcH11) bonded alumina-spinel castables by wedge splitting test
17. Thermodynamic evaluation and properties of refractory materials for steel ladle purging plugs in the system Al2O3-MgO-CaO10.1016/j.ceramint.2016.04.118 ↗
18. Effect of magnesium aluminum hydrotalcite on the properties of CAC-bonded castables10.1016/j.ceramint.2022.10.061 ↗
19. Infra-red spectra of inorganic aluminates and characteristic vibrational frequencies of AlO4 tetrahedra and AlO6 octahedra10.1016/0584-8539(67)80100-4 ↗
20. In situ spinel formation in a smart nano-structured matrix for no-cement refractory castables10.3390/ma13061403 ↗
21. Synthesis and evaluation of Mg-Al hydrotalcite formation and its influence on the microstructural evolution of spinel-forming refractory castables under intermediate temperatures10.1016/j.jeurceramsoc.2022.01.009 ↗
22. Observation and quantification of the fracture process zone for two magnesia refractories with different brittleness10.1016/j.jeurceramsoc.2017.02.005 ↗
23. Investigation of microstructure-property relantionships of magnesiahercynite refractory composites by a refined digital image correlation technique10.1016/j.jeurceramsoc.2019.05.010 ↗
24. Fracture process analysis in magnesia-hercynite refractory materials by combining an enhanced digital image correlation method with wedge splitting test10.1016/j.tafmec.2021.103134 ↗
25. A comprehensive evaluation of fracture toughness, fracture energy, flexural strength and microstructure of calcium aluminate cement concrete exposed to high temperatures10.1016/j.engfracmech.2021.108221 ↗
26. The influence of microstructure on the maximum load and fracture energy of refractory castables10.1016/j.ceramint.2009.07.033 ↗
27. Setting time and compressive strength prediction model of concrete by nondestructive ultrasonic pulse velocity testing at early age10.1016/j.conbuildmat.2020.119027 ↗
28. Non-destructive assessment of both mean strength and variability of concrete: A new bi-objective approach10.1016/j.conbuildmat.2016.03.120 ↗
29. Conventional and microwave-assisted sintering of ZnO-containing CAC-bonded alumina-based refractory castables10.1016/j.jeurceramsoc.2023.06.063 ↗
30. Effect of spinel content on hot strength of alumina-spinel castables in the temperature range 1000-1500 °C10.1016/S0955-2219(99)00042-4 ↗
31. Investigation of fracture behavior of typical refractory materials up to service temperatures10.1002/ces2.10123 ↗
32. Matrix microstructure optimization of alumina-spinel castables and its effect on high temperature properties10.1016/j.ceramint.2017.10.010 ↗
33. Investigation of refractory brittleness by fracture mechanical and fractographic methods
34. Investigation of fracture behavior of cement-bonded corundum castables using wedge splitting test and digital image correlation method10.1016/j.jeurceramsoc.2019.11.081 ↗
35. Effect of particle size of hydromagnesite on properties of calcium aluminate cement bonded corundum based castables10.1016/j.ceramint.2020.07.189 ↗