journal article·2025-03

Corrosion behaviors and failure mechanism of plasma sprayed Yb2Si2O7/Si environmental barrier coatings exposed to CMAS+ NaVO3

Xunxun Hu, Yongguo Chen, Hongbo Guo, Huibin Xu

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. SiC-matrix composite materials for advanced jet engines[J]10.1557/mrs2003.193 ↗
2. Advances in SiC/SiC composites for aero-propulsion[J]10.1002/9781118832998.ch7 ↗
3. Advanced structural ceramics in aerospace propulsion[J]10.1038/nmat4687 ↗
4. Creep Resistance and water vapor degradation of SiC/SiC ceramic matrix composite gas turbine hot section components[C]
5. Silicon carbide oxidation in steam up to 2 MPa[J]10.1111/jace.13094 ↗
6. Lorrette C., Sauder C., Billaud P., et al. SiC/SiC composite behavior in LWR conditions and under high temperature steam environment[C]//Top Fuel 2015.
7. Na2SO4 deposit-induced hot corrosion of SiC fibers relevant for SiC CMCs[J]10.1111/jace.17982 ↗
8. Effects of molten Na2SO4 on wet oxidation behavior of SiCf/SiC composites above 1200℃[J]10.1016/j.jeurceramsoc.2022.11.038 ↗
9. Strength degradation of oxide/oxide and SiC/SiC ceramic matrix composites in CMAS and CMAS/salt exposures[C]
10. Stress-corrosion behavior of SiCf/SiC under CMAS-wet-oxygen environments[J]10.1016/j.corsci.2024.111844 ↗
11. Rare earth silicate environmental barrier coatings for SiC/SiC composites and Si3N4 ceramics[J]10.1016/j.jeurceramsoc.2004.12.013 ↗
12. Rare earth silicate environmental barrier coatings: present status and prospective[J]10.1016/j.ceramint.2017.01.153 ↗
13. Progress on high-temperature protective coatings for aero-engines[J]10.1007/s44251-023-00005-6 ↗
14. Thermal properties of rare-earth monosilicates for EBC on Si-based ceramic composites[J]10.1111/jace.13982 ↗
15. Thermal expansion of rare-earth pyrosilicates [J]10.1111/jace.12388 ↗
16. Exploration of the low thermal conductivities of γ-Y2Si2O7, β-Y2Si2O7, β-Yb2Si2O7, and β-Lu2Si2O7 as novel environmental barrier coating candidates[J]10.1016/j.jeurceramsoc.2016.04.022 ↗
17. Response of ytterbium disilicate–silicon environmental barrier coatings to thermal cycling in water vapor[J]10.1016/j.actamat.2015.12.053 ↗
18. Molten calcium-magnesium-aluminosilicate interactions with ytterbium disilicate environmental barrier coating [J]10.1557/jmr.2020.211 ↗
19. High-temperature Na2SO4 interaction with air plasma sprayed Yb2Si2O7+Si EBC system: Topcoat behavior [J]10.1111/jace.17999 ↗
20. Interaction of CMAS on thermal sprayed ytterbium disilicate environmental barrier coatings: A story of porosity[J]10.1016/j.ceramint.2021.12.033 ↗
21. Hot corrosion behavior of Yb2Si2O7 environmental barrier coatings in molten NaVO3 salt [J]10.1016/j.ceramint.2021.07.237 ↗
22. Comprehensive microstructural characterization and CMAS infiltration resistance of ytterbium disilicate coatings with lamellar and quasi-columnar structures[J]10.1016/j.corsci.2023.111316 ↗
23. CMAS effects on ship gas-turbine components/materials[C]
24. The increasing complexity of hot corrosion10.1115/1.4038037 ↗
25. Corrosiveness of CMAS and CMAS+ salt (NaVO3, Na2SO4 and NaCl) to YSZ thermal barrier coating materials[J]10.1016/j.corsci.2022.110738 ↗
26. Comparison of NaVO3+ CMAS mixture and CMAS corrosion to thermal barrier coatings [J]10.1016/j.corsci.2020.108968 ↗
27. Crystallization behavior of CMAS and NaVO3+ CMAS mixture and its potential effect to thermal barrier coatings corrosion[J]10.1016/j.ceramint.2021.08.072 ↗
28. Corrosion resistance of GdPO4 thermal barrier coating candidate in the presence of CMAS+ NaVO3 and CMAS[J]10.1016/j.corsci.2022.110628 ↗
29. Sc-doped Gd2Zr2O7 coating on YSZ thermal barrier coatings to resist CMAS+ molten salt attack[J]10.1016/j.ceramint.2022.01.024 ↗
30. Thermal properties and calcium-magnesium-alumina-silicate (CMAS) resistance of LuPO4 as environmental barrier coatings[J]10.1016/j.jeurceramsoc.2019.11.018 ↗
31. Structure, composition, and defect control during plasma spray deposition of ytterbium silicate coatings[J]10.1007/s10853-015-9358-5 ↗
32. Garnet stability in the Al–Ca–Mg–Si–Y–O system with implications for reactions between TBCs, EBCs, and silicate deposits[J]10.1111/jace.17176 ↗
33. Apatite and garnet stability in the Al–Ca–Mg–Si–(Gd/Y/Yb)–O systems and implications for T/EBC: CMAS reactions[J]10.1111/jace.18179 ↗
34. Interaction of ytterbium monociliate environmental barrier coating material with molten calcium-magnesium-aluminosilicate (CMAS)[J10.1016/j.corsci.2022.110864 ↗
35. Corrosion mechanisms of high-entropy rare earth zirconate (Gd0.2Y0.2Er0.2Tm0.2Yb0.2)2Zr2O7 exposed to CMAS and multi-medium (NaVO3+CMAS) [J]10.1016/j.jeurceramsoc.2023.12.039 ↗
36. Silicate deposit degradation of engineered coatings in gas turbines: progress toward models and materials solutions10.1146/annurev-matsci-010917-105000 ↗
37. Corrosion behavior and mechanism of ytterbium monosilicate by molten calcium-magnesium-alumino-silicate melts at 1400℃ and 1500 ℃ [J]10.1016/j.ceramint.2023.04.213 ↗
38. Thermochemical interactions between CMAS and Ca2Y8 (SiO4) 6O2 apatite environmental barrier coating material[J]10.1016/j.jeurceramsoc.2019.08.040 ↗
39. Interactions between Ca2Gd8 (SiO4) 6O2 apatite and calcium-magnesium-aluminosilicate (CMAS) at elevated temperatures[J]10.1016/j.ceramint.2023.06.252 ↗
40. Thermochemical interactions between Ca2Sm8 (SiO4) 6O2 apatite and molten calcium–magnesium-aluminosilicate (CMAS)[J]10.1016/j.ceramint.2024.02.258 ↗
41. An interpretation of glass chemistry in terms of the optical basicity concept[J]10.1016/0022-3093(76)90027-2 ↗
42. 2ZrO2· Y2O3 thermal barrier coatings resistant to degradation by molten CMAS: part I, optical basicity considerations and processing[J]10.1111/jace.13210 ↗
43. Corrosion behavior of CMAS coupling NaVO3 salt for plasma-sprayed Al2O3/YSZ thermal barrier coatings[J]10.1016/j.corsci.2023.111369 ↗
44. Reaction behaviors and mechanisms of tri-layer Yb2SiO5/Yb2Si2O7/Si environmental barrier coatings with molten calcium-magnesium-alumino-silicate[J]10.1016/j.corsci.2021.110069 ↗
45. NdYbZr2O7 thermal barrier coating resistant to degradation by volcanic ash and CMAS[J]10.1016/j.corsci.2022.110795 ↗
46. Stokes J.L. Thermal expansion coefficients of Ca2Y8 (SiO4) 6O2 and Ca2Yb8 (SiO4) 6O2 apatite-type silicates [R]. 2021.
47. Synthesis and thermal expansion of ZrO2/ZrW2O8 composites[J]10.1016/j.jeurceramsoc.2004.09.015 ↗