Interfacial reaction between different MgO-based refractories and the CaO-FeOx-SiO2 slag system at 1400°C

Junmo Jeon, Daniel Lindberg

Abstract

Interfacial reactions between MgO-Al 2 O 3 , MgO-Cr 2 O 3 , and MgO-C refractories and the CaO-FeO x -SiO 2 slag system were investigated at 1400 °C under Ar atmosphere. Sessile drop tests were carried out to observe the behaviors of the liquid CaO-FeO x -SiO 2 slag with different basicities (CaO/SiO 2 : 0.25, 1.0, and 1.5) on the MgO-Al 2 O 3 , MgO-Cr 2 O 3 , and MgO-C refractories. Furthermore, the corrosion behaviors of MgO-Al 2 O 3 , MgO-Cr 2 O 3 , and MgO-C in contact with the liquid CaO-FeO x -SiO 2 slag (S2, CaO/SiO 2 =1.0) were studied using immersion tests for 30 min. As a result, the MgO-Cr 2 O 3 refractory showed higher resistance against the slags than the MgO-Al 2 O 3 and MgO-C refractories, with less dissolution and no gas reactions. The chemical reaction between MgO-Al 2 O 3 / MgO-Cr 2 O 3 and slag was studied with thermodynamic modeling using the thermochemical software, FactSage 8.3. The calculation results were in good agreement with the results of the sessile drop test and immersion test.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Iron and Steelmaking Processes · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Refractories for copper production10.1080/08827509608914131 ↗
2. 2004
3. Thermal shock behaviour of magnesia–spinel composites10.1016/j.jeurceramsoc.2003.07.017 ↗
4. Thermal expansion of Al2O3, BeO, MgO, B4C, SiC, and TiC Above 1000°C10.1111/j.1151-2916.1959.tb12958.x ↗
5. Fracture mechanics behavior of coarse-grained MgO–C at room and high temperature10.1016/j.ceramint.2023.08.081 ↗
6. Spinel-containing alumina-based refractory castables10.1016/j.ceramint.2011.03.049 ↗
7. Thermal expansion of spinels MgCr2O4, MgAl2O4 and MgFe2O4
8. Slag resistance of Al2O3–MgO refractory castables in different environmental conditions10.1111/jace.12433 ↗
9. Corrosion of spinel clinker by CaO–Al2O3–SiO2 ladle slag10.1016/S0955-2219(01)00509-X ↗
10. Corrosion of high alumina spinel castables by steel ladle slag10.1179/174328106X80109 ↗
11. Thermodynamic stability of spinel phase at the interface between alumina refractory and CaO–CaF2–SiO2–Al2O3–MgO–MnO Slags10.1111/jace.13570 ↗
12. Corrosion of magnesia-chromite refractory by PbO-rich copper slags10.1016/j.corsci.2021.109949 ↗
13. Degradation mechanisms and use of refractory linings in copper production processes: a critical review10.1016/j.jeurceramsoc.2013.10.005 ↗
14. Degradation mechanisms of magnesia-chromite refractories by high-alumina stainless steel slags under vacuum conditions10.1016/j.jeurceramsoc.2005.12.025 ↗
15. Reactive wetting phenomena of MgO–C refractories in contact with CaO–SiO2 slag10.1016/S1003-6326(12)61818-4 ↗
16. Wetting, spreading and corrosion behavior of molten slag on dense MgO and MgO-C refractory10.1016/j.ceramint.2018.09.234 ↗
17. Melt corrosion of oxide and oxide–carbon refractories10.1179/095066099101528234 ↗
18. Corrosion-erosion behavior of MgAl2O4 spinel refractory in contact with high MnO slag10.1016/j.ceramint.2017.08.034 ↗
19. Post-mortem analysis of alumina-magnesia-carbon refractory bricks used in steelmaking ladles10.1016/j.ceramint.2018.09.150 ↗
20. Chemical degradation mechanisms of magnesia–chromite refractories in the copper smelting furnace10.1007/s11837-018-3083-x ↗
21. Post-mortem study of magnesia–chromite refractory used in a submerged arc furnace in the copper-making process10.1007/s11837-018-3090-y ↗
22. Corrosion behavior of MgO–C refractory in ferromanganese Slags10.2355/isijinternational.52.62 ↗
23. N. Eustathopoulos, M.G. Nicholas, and B. Drevet, Wettability at High Temperatures, R.W. Cahn (Series Editor), Pergamon Materials Series Volume 3, Oxford (1999).
24. W.S. Rasband, Image J., U.S. National Institutes of Health, Bethesda, Maryland, USA, 1997–2018. 〈https://imagej.net/ij/〉.
25. version 8.3, 〈www.factsage.com〉.
26. Characteristics and utilisation of copper slag—a review10.1016/S0921-3449(02)00171-4 ↗
27. Slag use in cement manufacture and cementitious applications
28. Thermodynamic activities of FeO in CaO-FeO-SiO2 slags10.1002/srin.199401187 ↗