journal article·2022-04

Vickers crack extension and residual fracture strength of annealed and thermally tempered glass in water

Hong-Seok Kim, Sang-Hu Park

Publisher page

Abstract

Abstract The effect of water contact on the propagation of microscale surface cracks is investigated in two types of glass: annealed and tempered glass. Initial flaw is artificially created on the glass surface using a Vickers indenter, and is covered with a water droplet for 20 min. Micrographs of the flaw taken before and after water contact confirms the increase in crack length from around 61 to 103 µm for thermally tempered glass. After water dipping, the maximum length to which the crack growth is approximately 57% smaller in the thermally tempered glass than in the annealed glass. Despite the severe effect of water contact on crack propagation, it is found that the fracture strength is not substantially altered by water dipping; even though the crack length is enlarged, the fracture strength of glass is similar, and in the case of tempered glass, its fracture strength is slightly changed within 7% due to the blunting of the crack tip by water or others.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced Surface Polishing Techniques · Laser Material Processing Techniques · Surface Roughness and Optical Measurements

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Artificial ageing of glass with sand abrasion10.1016/j.conbuildmat.2017.03.094 ↗
2. Investigation the effect of weathering on chemically strengthened flat glasses
3. Impact of dust and other environmental factors on glass transmittance in warm and humid climatic zone10.1007/s10098-016-1302-0 ↗
4. T.A. Michalske, S.W. Freiman, A molecular interpretation of stress corrosion in silica, Nature 295 (5849) 511–512.10.1038/295511a0 ↗
5. Influence of water vapor on crack propagation in soda-lime glass10.1111/j.1151-2916.1967.tb15145.x ↗
6. Stress corrosion and static fatigue of glass10.1111/j.1151-2916.1970.tb15962.x ↗
7. Crack growth in borate and silicate glasses: stress-corrosion susceptibility and hydrolytic resistance
8. Crack growth in hydrous soda-lime silicate glass
9. Sub-critical crack growth in silicate glasses: role of network topology10.1063/1.4932377 ↗
10. Subcritical crack growth parameters in glass as a function of environmental conditions10.1007/s40940-020-00134-6 ↗
11. Kinetics of indentation cracking in glass10.1111/j.1151-2916.1993.tb03726.x ↗
12. Effect of water corrosion on cracks and vickers imprints in glass10.1007/s10704-012-9712-4 ↗
13. Further damage induced by water in micro-indentations in phosphate laser glass10.1016/j.apsusc.2013.11.129 ↗
14. Effect of water on the transmittance of glass plates with eroded surfaces10.1016/j.jeurceramsoc.2005.03.249 ↗
15. Varshneya · 2013
16. 2016
17. Difference of cracking behavior due to Vickers indentation between physically and chemically tempered glasses10.1016/j.jnoncrysol.2012.02.020 ↗
18. Driving force for indentation cracking in glass: composition, pressure and temperature dependence10.1098/rsta.2014.0140 ↗
19. Correlation between multistage crack-growth and time-dependent strength in commercial silicate-glasses. 1. Influence of ambient media and types of initial cracks
20. Indentation residual stresses in soda-lime and borosilicate glasses10.1016/j.jnoncrysol.2018.09.051 ↗
21. Lawn · 1993
22. J.D. Poloniecki, T.R. Wilshaw, Determination of surface crack size densities in glass, Nat. Phys. Sci. 229 (8) 226–227.10.1038/physci229226a0 ↗
23. On the inhomogeneity of residual stresses in tempered glass panels10.3176/eng.2012.1.01 ↗
24. Fractographic analysis of surface flaws in glass10.4028/www.scientific.net/KEM.290.300 ↗
25. Microfracture beneath point indentations in brittle solids10.1007/BF00541038 ↗
26. Elastic stress fields caused by indenting brittle materials10.1080/01418618208236917 ↗
27. Crack blunting of high-silica glass10.1111/j.1151-2916.1982.tb10486.x ↗
28. Direct observation of crack tip geometry of SiO2 glass by high-resolution electron microscopy10.1111/j.1151-2916.1984.tb19748.x ↗