Resistance to cyclic oxidation and evolution of oxide scale in 2.5D and 3D Cf/SiC composites with Si-B-C added matrix

Ramya Krishna, A. Udayakumar, Rahul Mitra

Abstract

The effect of fibre preform architecture (2.5D-woven and 3D-NOOBed) on the oxidation behaviour of CVI-processed C f /SiC composites with (PyC/SiC) n=4 interphase and SiC/SiBC matrix has been studied using non-isothermal and cyclic exposure tests. The mass loss of 3D C f /SiC composite by CO (g) formation exceeds that of 2.5D composite by ∼33 % during heating to 1200 °C in a thermogravimetric analyser and by ∼7–90 times on cyclic oxidation at 1250–1500 °C. FESEM-EDS and ToF-SIMS analyses confirm a stable borosilicate-rich oxide scale at 1400 °C, leading to > 80 % post-oxidation flexural strength retention. Sluggish SiO 2 growth kinetics and active oxidation of SiC are considered responsible for the oxide scale to be less protective at 1250 and 1500 °C, respectively. Poor strength retention (∼57 %) of the 3D C f /SiC composite exposed at 1250 °C is attributed to significant oxidation-induced damage caused by increased oxygen ingress through larger pore volume and higher interfacial area along the z-direction.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (69)

Show source-provided references
1. Design, preparation and properties of non-oxide CMCs for application in engines and nuclear reactors: an overview10.1016/S0266-3538(03)00230-6 ↗
2. SiC-matrix composite materials for advanced jet engines10.1557/mrs2003.193 ↗
3. C/C-SiC composites for space applications and advanced friction systems10.1016/j.msea.2005.08.204 ↗
4. Oxidation behaviour of SiC/SiC ceramic matrix composites in air10.1016/j.jeurceramsoc.2016.05.051 ↗
5. Carbon Fiber Reinforced Silicon Carbide Ceramic Matrix Composites
6. The design of the fibre-matrix interfacial zone in ceramic matrix composites10.1016/S1359-835X(97)00128-0 ↗
7. Selection, processing, properties and applications of ultra-high temperature ceramic matrix composites, UHTCMCs – a review10.1080/09506608.2019.1652006 ↗
8. Oxidation-resistant carbon-fiber-reinforced ceramic-matrix composites10.1016/S0266-3538(98)00146-8 ↗
9. Silicon and boron containing components by CVD and CVI for high temperature ceramic composites
10. Oxidation studies of SiC-coated 2.5D carbon fibre preforms
11. Boron-bearing species in ceramic matrix composites for long-term aerospace applications10.1016/j.jssc.2003.03.005 ↗
12. Synthesis and characterisation of Cf/SiC composites with modified silicon carbide matrix10.1016/j.cartre.2021.100082 ↗
13. Oxidation behavior of 2D C/SiC composites coated with multi-layer SiC/Si–B–C/SiC coatings under wet oxygen atmosphere10.1016/j.apsusc.2015.06.153 ↗
14. Evaluating the effect of oxygen content in BN interfacial coatings on the stability of SiC/BN/SiC composites10.1016/S1359-835X(98)00135-3 ↗
15. Oxidation behavior of 2D C/SiC composite modified by SiB4 particles in inter-bundle pores10.1016/j.compscitech.2007.10.016 ↗
16. Oxidation behavior of C/SiC-SiBCN composites at high temperature10.1016/j.jeurceramsoc.2019.04.025 ↗
17. Long-term oxidation behavior of C/SiC-SiBCN composites in wet oxygen environment10.1016/j.jeurceramsoc.2020.09.058 ↗
18. Oxidation behaviour of a multi-layered ceramic-matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
19. Preparation and oxidation protection of CVD SiC/a-BC/SiC coatings for 3D C/SiC composites10.1016/j.corsci.2009.01.026 ↗
20. Effect of CVD SiC seal coating on the mechanical properties of Cf/SiC composites generated through CVI10.1016/j.surfcoat.2013.01.007 ↗
21. Microstructural-property correlation of CVI processed Cf/SiC composites and property enhancement as a function of CVD SiC seal coating10.1016/j.ceramint.2015.08.020 ↗
22. Vapour phase synthesis and characterisation of Cf/SiC composites with self-healing Si-B-C monolayer coating10.1016/j.ceramint.2020.06.154 ↗
23. Mechanical behavior of SiCf/SiC composites with alternating PyC/SiC multilayer interphases10.1016/j.matdes.2012.07.073 ↗
24. Recent advances in the field of ceramic fibers and ceramic matrix composites
25. A comparative study of tensile strength of Cf/SiC composites having single layer and multilayer interphases10.1016/j.ceramint.2019.07.099 ↗
26. Single- and multilayered interphases in SiC/SiC composites exposed to severe environmental conditions: an overview10.1111/j.1744-7402.2009.02424.x ↗
27. Fibre-matrix interphases and interfaces in ceramic matrix composites processed by CVI10.1163/156855493X00112 ↗
28. Microstructure and mechanical properties of carbon fiber reinforced multilayered (PyC–SiC)n matrix composites10.1016/j.matdes.2015.07.018 ↗
29. Effect of CVI-induced porosity on elastic properties and mechanical behaviour of 2.5D and 3D Cf/SiC composites with multilayered interphase10.1016/j.jeurceramsoc.2024.02.039 ↗
30. Oxidation and defect control of CVD SiC coating on three-dimensional C/SiC composites10.1016/S0008-6223(02)00103-3 ↗
31. Oxidation of carbon fiber-reinforced silicon carbide matrix composites at reduced oxygen partial pressures10.1111/j.1551-2916.2010.04376.x ↗
32. Fracture toughness evolution and failure mechanisms of two-dimensional SiCf/SiC composites at temperatures up to 1500 °C in air10.1016/j.tafmec.2024.104458 ↗
33. Oxidation behavior of C/SiC-SiBCN composites at high temperature10.1016/j.jeurceramsoc.2019.04.025 ↗
34. Oxidation mechanisms and kinetics of SiC-matrix composites and their constituents10.1023/B:JMSC.0000048745.18938.d5 ↗
35. Oxidation protection of multilayer CVD SiC/B/SiC coatings for 3D C/SiC composite10.1016/j.msea.2007.02.059 ↗
36. Kinetics and mechanisms of oxidation of 2D Woven C/SiC composites: i, experimental approach10.1111/j.1151-2916.1994.tb07096.x ↗
37. Oxidation behavior of SiBC matrix modified C/SiC composites with different PyC interphase thicknesses10.1016/j.ceramint.2014.09.111 ↗
38. Evaluation of elastic constants and high temperature tensile behaviour with damage assessment of the SiC seal-coated 2.5D Cf/SiC composites having multilayered interphase and Si-B-C added matrix10.1016/j.jeurceramsoc.2022.12.066 ↗
39. Noobing: A nonwoven 3D fabric-forming process explained10.1080/00405000208630552 ↗
40. ASTM C1341-13, Standard Test Method for Flexural Properties of Continuous Fiber-Reinforced Advanced Ceramic Composites, ASTM Int. (2013). https://doi.org/10.1520/C1341-13.10.1520/C1341-13 ↗
41. On the structural role of boron in borosilicate glasses
42. Oxidation resistance and evolution of multi-layered oxide scale during isothermal and cyclic exposure of ZrB2–SiC–LaB6 composites at 1300 °C to 1500 °C10.1007/s11661-021-06501-4 ↗
43. Oxidation behavior and damage mechanism of SiC f /SiC minicomposites with multilayered (BN/SiC) n interfacial coatings at 1200 ℃10.1080/09276440.2022.2109795 ↗
44. Barin · 1995
45. Oxidation behaviour of silicon carbide - A review
46. Active oxidation of SiC10.1007/s11085-010-9216-4 ↗
47. The oxidation behaviour of carbon fibres10.1007/BF01154706 ↗
48. Oxidation kinetics and stress effects for the oxidation of continuous carbon fibers within a microcracked C/SiC ceramic matrix composite10.1111/j.1551-2916.2007.02170.x ↗
49. Oxidation Mechanisms and Kinetics of 1D-SiC/C/SiC Composite Materials: II, Modeling10.1111/j.1151-2916.1994.tb07016.x ↗
50. Surface oxidation chemistry of β-SiC10.1116/1.580466 ↗
51. Oxidation and Corrosion of Non-oxide Ceramics
52. Study on the oxygen diffusion in the oxide layers of SiBCN ceramics by SIMS10.1016/j.jeurceramsoc.2021.12.020 ↗
53. Oxidation effects on the mechanical properties of 2D woven C/SiC composites10.1016/0955-2219(94)90105-8 ↗
54. Effect of oxidation and residual stress on mechanical properties of SiC seal coated C/SiC composite10.1016/j.ceramint.2017.10.085 ↗
55. Oxidation behaviour of two-dimensional C/SiC modified with self-healing Si–B–C coating in static air10.1016/j.corsci.2012.08.003 ↗
56. Oxidation behavior of 3D C/SiC composites in two oxidizing environments10.1016/S0266-3538(00)00190-1 ↗
57. Oxidation behaviour of three-dimensional woven C/SiC composites10.1179/026708301101510456 ↗
58. The influence of high temperature exposure to air on the damage to 3D-C/SiC composites
59. Oxidation protective multilayer CVD SiC coatings modified by a graphitic B-C interlayer for 3D C/SiC composite10.1007/s10443-006-9025-8 ↗
60. Mechanical properties of 3D noninterlaced Cf/SiC composites prepared through hybrid process (CVI + PIP), Int. J. Mater
61. Debonding and pull-out processes in fibrous composites10.1007/BF01026323 ↗
62. Investigation on the structural origin of low thermal expansion coefficient of fused silica10.1016/j.mtla.2020.100752 ↗
63. Smithsonian physical tables
64. Thermal expansion of the cubic (3C) polytype of SiC10.1007/BF01106557 ↗
65. Transverse and longitudinal coefficient of thermal expansion of carbon fibers at high temperatures (300–2500K)10.1016/j.carbon.2008.07.035 ↗
66. Chawla · 2013
67. Increasing the strength and toughness of a carbon fiber/silicon carbide composite by heat treatment10.1016/j.carbon.2012.11.001 ↗
68. The structural performance of ceramic matrix composites
69. Characterization and modeling of tensile properties of continuous fiber reinforced C/C-SiC composite at high temperatures10.1016/j.jeurceramsoc.2020.09.043 ↗