Development of electrical discharge machinable SiC-ZrN composites: Unveiling high temperature sliding wear resistance
Source abstract
Abstract
Dense SiC-(10-30 vol%) ZrN composites were developed using spark plasma sintering with AlN-Y2O3 additives at 1800 °C for 5 min in nitrogen atmosphere. The nascent oxide present on ZrN surface reduces liquid phase formation temperature, facilitating improved densification of SiC ceramics. Mechanical properties were retained, and electrical conductivity increased with ZrN addition. To demonstrate a rapid and low-cost machining alternative for SiC ceramics, SiC-ZrN composites were successfully cut using wire-EDM. The tribological potential of novel electrical discharge machinable SiC-ZrN composite disk against SiC ball at various conditions of reciprocating sliding contacts was investigated. Friction is less affected by reinforcement content at room temperature (25 ℃) but significant change is observed at high temperature (600 ℃). Minimum one order of lower wear rate is reported with an increase in temperature from 25 ℃ to 600 ℃. The major wear mechanism changed from abrasion to tribo oxidation with increase in temperature.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Mechanical properties of hot-forged silicon carbide ceramics10.1016/j.scriptamat.2004.09.012 ↗
2. Liquid phase sintered silicon carbide (LPS-SiC) ceramics having remarkably high oxidation resistance in wet air10.1016/j.jeurceramsoc.2005.05.015 ↗
3. F. Ghasripoor, R.K. Schmid, M.R. Dorfman, U.S. Patent No. 5,997,248. (1999) Washington, DC: U.S. Patent and Trademark Office.
4. Improving the anti-seizure ability of SiC seal in water with RIE texturing10.1023/A:1022650813314 ↗
5. Automotive and industrial applications of structural ceramics in Japan10.1016/j.jeurceramsoc.2007.09.016 ↗
6. G. Hilmas, W. Fahrenholtz, A.A. Buchheit, D.M. Deason, Silicon Carbide Ceramics for Aerospace Applications-Processing, Microstructure, and Property Assessments, Mater. Sci. Tech., Maney Publishing (2005).
7. Various methods of machining advanced ceramic materials10.1016/0924-0136(94)90144-9 ↗
8. Liquid phase sintering and microstructure-property relationships of silicon carbide ceramics with oxynitride additives10.1016/S0254-0584(00)00437-5 ↗
9. High-temperature effects in the fracture mechanical behaviour of silicon carbide liquid-phase sintered with AlN-Y2O3 additives10.1016/S0955-2219(00)00317-4 ↗
10. Development of spark plasma sintered conductive SiC–TiB2 composites for electrical discharge machining applications10.1111/ijac.13940 ↗
11. Past and current trends in electric discharge based machining of Silicon Carbide
12. Effective nitrogen doping for fabricating highly conductive β-SiC ceramics10.1111/j.1551-2916.2011.04799.x ↗
13. Effects of Y2O3-RE2O3 (RE = Sm, Gd, Lu) additives on electrical and mechanical properties of SiC ceramics containing Ti2CN10.1016/j.jeurceramsoc.2015.09.042 ↗
14. TiN modified SiC with enhanced strength and electrical properties10.1016/j.jeurceramsoc.2016.11.007 ↗
15. Electrical and thermal properties of SiC-Zr2CN composites sintered with Y2O3-Sc2O3 additives10.1016/j.jeurceramsoc.2016.09.001 ↗
16. Development of conductive SiC-ZrN-TiB2 ceramics: a pathway towards electrical discharge machinable SiC based ceramics10.1016/j.jeurceramsoc.2024.04.044 ↗
17. Room and high temperature reciprocated sliding wear behavior of SiC-WC composites10.1016/j.ceramint.2017.09.080 ↗
18. Effect of impingement angle and WC content on high temperature erosion behavior of SiC-WC composites10.1016/j.ijrmhm.2017.07.014 ↗
19. Role of hBN content, humidity, and temperature on the sliding wear behaviour of SiC ceramics10.1016/j.jeurceramsoc.2023.08.015 ↗
20. In situ preparation of a SiC–TiB2 composite and its wear fracture mechanism at high temperatures10.1007/s10853-022-07050-w ↗
21. Influence of TiB2 and wear conditions on friction and wear behaviour of SiC ceramics in reciprocating sliding10.1016/j.jeurceramsoc.2023.12.055 ↗
22. The group IV carbides and nitrides10.1002/9781118700853.ch14 ↗
23. Sliding wear behaviour of ZrN and (Zr, 12 wt% Hf) N coatings10.1016/j.triboint.2005.01.038 ↗
24. Friction and wear behaviors of the PVD ZrN coated carbide in sliding wear tests and in machining processes10.1016/j.wear.2007.03.014 ↗
25. B.R. Golla, T. Bhandari, A. Mukopadhyay, B. Basu, Titanium Boride, Ultra-High Temperature Ceramics: Materials for Extreme Environment Applications, First Edition. (2014) by John Wiley & Sons, Inc.10.1002/9781118700853.ch13 ↗
26. Ultra-high temperature ceramics: materials for extreme environments10.1016/j.scriptamat.2016.10.018 ↗
27. Thermal stability of zircon (ZrSiO4)10.1016/j.jeurceramsoc.2007.12.040 ↗
28. A critical evaluation of indentation techniques for measuring fracture toughness. I: direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗
29. Compositional identification of the intergranular phase in liquid phase sintered SiC10.1016/S0955-2219(02)00006-7 ↗
30. Electrical and mechanical properties of pressureless sintered SiC-Ti2CN composites10.1016/j.jeurceramsoc.2018.03.040 ↗
31. Influence of ZrO2 addition on melting kinetics of a YSiAlO glass-ceramic10.1016/0955-2219(96)00054-4 ↗
32. Improvements in Mechanical Properties in SiC by the addition of TiC Particles10.1111/j.1151-2916.1984.tb19174.x ↗
33. Electrical discharge machining of ZrO2/TiN particulate composite10.1179/bct.2000.99.2.77 ↗
34. Mechanism of transfer film formation during repeat pass sliding of ceramic materials10.1016/0043-1648(90)90083-M ↗
35. Running-in: art or engineering?10.1007/BF02834123 ↗
36. Sliding wear of silicon carbide-titanium boride ceramic-matrix composite10.1111/j.1151-2916.1993.tb03815.x ↗
37. Tailoring friction and wear properties of titanium boride reinforced silicon carbide composites
38. Wear map of ceramics10.1016/S0043-1648(96)07363-2 ↗
39. High-temperature oxidation of the nitrides of the group IV transition metals: II. Oxidation of zirconium and hafnium nitrides10.1007/BF00800246 ↗
40. High temperature tribology of ceramics10.1016/0301-679X(89)90168-0 ↗
41. Wear and wear transition in silicon carbide ceramics during sliding10.1111/j.1151-2916.1996.tb08579.x ↗
42. Genesis and role of wear debris in sliding wear of ceramics10.1016/S0043-1648(00)00465-8 ↗
43. Tribological and interfacial phenomena in Al2O3/ SiC and SiC/SiC couples at high temperature10.1016/S0955-2219(89)80004-4 ↗
44. Effect of doping elements on the friction and wear properties of SiC in unlubricated sliding condition10.1016/j.wear.2003.10.016 ↗
45. C.D. Wagner, W.M. Riggs, L.E. Davis, J.F. Moulder, G.E. Muilenberg. Handbook of X-Ray photoelectron Spectroscopy, Perkin-Elmer Corp., (1979).
46. XPS studies on the oxidation behavior of SiC particles10.1016/S0025-5408(97)00222-5 ↗
47. Microstructure, mechanical properties and friction/wear behavior of hot-pressed Si3N4/BN ceramic composites
48. Oxidation behavior of ZrB2/SiC laminates: effect of composition on microstructure and mechanical strength10.1016/j.jeurceramsoc.2014.12.029 ↗
49. Bonding and XPS chemical shifts in ZrSiO4 versus SiO2 and ZrO2: charge transfer and electrostatic effects10.1103/PhysRevB.63.125117 ↗