journal article·2005-10

Crack-healing behaviour of mullite/SiC/Y2O3 composites and its application to the structural integrity of machined components

Sang-Kee Lee, Masato Ono, Wataru Nakao, Koji Takahashi, Kotoji Ando

Publisher page

Abstract

Abstract High-strength mullite/SiC/Y 2 O 3 composite ceramics with a great crack-healing ability were developed and subjected to three-point bending. A semicircular surface crack 100 μm in diameter was made in each specimen. Crack-healing behaviour was systematically studied as a function of crack-healing temperature and healing time, and the bending strength of the specimens crack-healed up to 1573 K was investigated. The effects of the crack-healing treatment on the structural integrity and reliability of machined components were studied systematically. Four main conclusions were drawn from the present study: (1) mullite/SiC/Y 2 O 3 composite ceramics have the ability to heal after cracking from 1423 K to 1673 K in air, (2) the heat-resistance limit temperature for strength of the crack-healed specimen is ≅1473 K, while at 68% of the specimens fractured from outside the crack-healed zone in the tested-temperature range of 300–1573 K, (3) due to the crack-healing treatment, the strength of the machined specimen increased by 40–200%. Local fracture strength was assumed to recover completely, and the cracks formed by machining were healed completely, and (4) a large self-crack-healing ability is desirable for obtaining a higher structural integrity in ceramic components.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Concrete and Cement Materials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Damage healing and strengthening behavior in intelligent mullite/SiC ceramics10.1111/j.1460-2695.1995.tb00924.x ↗
2. Effect of pre-crack size and testing temperature on fatigue strength properties of crack healed mullite10.2472/jsms.50.920 ↗
3. Crack healing behavior and high-temperature strength of mullite/SiC composite ceramics10.1016/S0955-2219(01)00431-9 ↗
4. Fatigue strength properties of crack healed mullite/SiC composite ceramics10.2472/jsms.48.1173 ↗
5. Crack-healing by heat treatment10.1111/j.1151-2916.1970.tb12002.x ↗
6. Healing of surface cracks in polycrystalline Al2O310.1111/j.1151-2916.1970.tb12148.x ↗
7. Crack-healing and strengthening of thermally shocked alumina10.1111/j.1151-2916.1976.tb10949.x ↗
8. Crack-healing behavior of monolithic alumina and strength of crack-healed member10.2472/jsms.52.667 ↗
9. Crack-healing behavior of Al2O3 toughened by SiC whiskers10.1111/j.1151-2916.2003.tb03622.x ↗
10. High temperature fatigue strength of crack-healed Al2O3 toughened by SiC whiskers10.1111/j.1151-2916.2004.tb07720.x ↗
11. Crack-healing behavior of hot-pressed silicon nitride due to oxidation10.1016/0956-716X(92)90574-X ↗
12. Threshold stress intensity for oxidative healing in silicon nitride10.1007/BF00278010 ↗
13. A preliminary study on crack healing behavior of Si3N4/SiC composite ceramics10.1046/j.1460-2695.1998.00052.x ↗
14. Crack-healing behavior, high-temperature and fatigue strength of SiC-reinforced silicon nitride composite10.1023/A:1006715825737 ↗
15. Effect of crack-healing and proof-testing procedures on fatigue strength and reliability of Si3N4/SiC composites10.1016/S0955-2219(02)00232-7 ↗
16. Crack-healing and oxidation behavior of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
17. Crack-healing behavior under stress of mullite/silicon carbide ceramics and the resultant fatigue strength10.1111/j.1151-2916.2001.tb00960.x ↗
18. Crack-healing behavior of structural ceramics under constant and cyclic stress at elevated temperature10.2109/jcersj.110.741 ↗
19. In situ crack-healing behavior of mullite/SiC composite ceramics10.2472/jsms.52.998 ↗
20. Strength recovery of ground ceramics by heat treatment in a shot time
21. Effects of rare earth oxide addition on the sintering of mullite10.2109/jcersj.99.351 ↗
22. Effects of Y2O3 addition on the sinterability and microstructure of mullite (part 1)—phase transformation and sinterability10.2109/jcersj.100.1159 ↗
23. Effects of Y2O3 addition on the sinterability and microstructure of mullite (part 2)—crystallization of liquid phase and grain growth10.2109/jcersj.101.331 ↗
24. Effects of Y2O3 on crack healing ability and high temperature strength of structural mullite10.2472/jsms.51.458 ↗
25. Reaction-bonding behavior of mullite ceramics with Y2O3 addition10.1016/S0955-2219(01)00288-6 ↗
26. Crack-healing behavior of Si3N4/SiC ceramics under stress and fatigue strength at the temperature of healing (1000°C)10.1016/S0955-2219(01)00435-6 ↗
27. Crack-healing behavior of Si3N4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature10.1111/j.1151-2916.2002.tb00446.x ↗
28. Crack-healing behavior and static fatigue strength of Si3N4/SiC ceramics held under stress at temperature (800, 900, 1000°C)10.1016/S0955-2219(02)00428-4 ↗
29. Nakao, W., Ono, M., Lee, S. K., Takahashi, K. and Ando K., Mechanical properties of SiC reinforced alumina composites attached crack-healing ability. In Proceedings of the 11th Materials and Processing Conference. The Japan Society of Mechanical Engineers, Tokyo, 2003, pp. 59–60.10.1299/jsmemp.2003.11.59 ↗
30. Nishida · 1973