Effect of AlN-content on the microstructure and fracture toughness of hot-pressed and heat-treated LPS–SiC ceramics

K. Strecker, M.-J. Hoffmann

Publisher page

Abstract

Abstract The influence of additive content on the microstructural development of hot-pressed and heat-treated LPS–SiC has been investigated using AlN–Y2O3 mixtures at a molar ratio of 80:20, varying the total amount from 5, 10, 15 to 20 wt.%. Specimen were hot-pressed at 1900 °C for 1 h in nitrogen atmosphere under an applied pressure of 25 MPa and subsequently heat-treated at 2000 °C for 1, 2, 4 and 8 h. It has been found that the transformation rate of β- into α-SiC is retarded by higher AlN-contents and the formation of the 6H α-SiC polytype is favored. Furthermore, grain growth during annealing is also effectively inhibited. While hardness remained almost unchanged, fracture toughness varied with additive content and/or duration of the heat-treatment. Fracture toughness increased during the first 1 or 2 h of annealing,depending on the AlN-content, and diminishing for more prolonged treatments. The maximum fracture toughness has been determined for samples containing 10 wt.% of additives, hot-pressed and annealed during 1 h.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (18)

Show source-provided references
1. Prochazka, S., The role of boron and carbon in the sintering of silicon carbide. In Special Ceramics, Vol. 6, ed. P. Popper. The British Ceramic Resaerch Association, Stoke-on-Trent, 1975, p. 171.10.1007/978-1-4684-3150-6_28 ↗
2. Sintering of covalent solids10.1111/j.1151-2916.1976.tb10979.x ↗
3. Tanaka, H., Sintering of silicon carbide. In Silicon Carbide—I, Fundamental and Solid Reaction, ed. S. Somiya and Y. Inomata. Elsevier Applied Science, London, New York, 1991, p. 213.10.1007/978-94-011-3842-0_10 ↗
4. Pressureless sintering of SiC10.1111/j.1151-2916.1982.tb10460.x ↗
5. In situ-toughened silicon carbide10.1111/j.1151-2916.1994.tb07024.x ↗
6. Grain growth and fracture toughness of fine-grained Silicon Carbide ceramics10.1111/j.1151-2916.1995.tb09100.x ↗
7. Effect of initial α-phase content on microstructure and mechanical properties of sintered silicon carbide10.1111/j.1151-2916.1998.tb02748.x ↗
8. Microstructure and mechanical properties of α-silicon carbide sintered with yttrium–aluminium garnet and silica10.1111/j.1551-2916.1999.tb20082.x ↗
9. Influence of the α/β-SiC phase transformation on microstructural development and mechanical properties of liquid phase sintered silicon carbide10.1023/A:1004552704872 ↗
10. Effect of β-to-α-phase transformation on the microstructural development and mechanical properties of fine-grained silicon carbide ceramics10.1111/j.1151-2916.2001.tb00773.x ↗
11. Flssigphasensintern von Siliziumcarbid mit oxinitridischen Zustzen
12. High-temperature effects in the fracture mechanical behaviour of silicon carbide liquid-phase sintered with AlN–Y2O3 additives10.1016/S0955-2219(00)00317-4 ↗
13. Liquid phase sintering and microstructure-property relationships of silicon carbide ceramics with oxynitride additives10.1016/S0254-0584(00)00437-5 ↗
14. Liquid phase sintered SiC processing and transformation controlled microstructure tailoring10.1590/S1516-14392000000400007 ↗
15. Izhevskyi, V. A., Genova, L. A., Bressiani, A. H. A. and Bressiani, J. C., Liquid-phase sintered silicon carbide based ceramics with AlN–Y2O3 and AlN–La2O3 additives. In Seventh International Symposium: Ceramic Materials and Components for Engines, ed. J. G. Heinrich and F. Aldinger. Wiley, VCH, Verlag, GmbH, Weinheim, 2001, p. 593.10.1002/9783527612765.c101 ↗
16. Liquid-phase sintering of SiC-based ceramics10.4028/www.scientific.net/KEM.189-191.173 ↗
17. The quantitative calculation of SiC-polytypes from measurements of X-ray-diffraction peak intensities10.1007/BF00551044 ↗
18. Evaluation of KIc of brittle solids by the indentation method with low crack-to-indent ratios10.1007/BF00724706 ↗