Degradation mechanisms of magnesia-chromite refractories by high-alumina stainless steel slags under vacuum conditions
Source abstract
Abstract
Abstract The corrosion behaviour of magnesia-chromite refractory by an alumina-rich (15–20 wt.%) stainless steelmaking slag is investigated by rotating finger tests in a vacuum induction furnace. The influence on the refractory wear, of the process temperature, corrosion time and, in particular, the high Al 2 O 3 content in the slag, is discussed. Two distinct mechanisms cause primary chromite degradation: FeO x and Cr 2 O 3 decomposition because of low oxygen potentials and dissolution by infiltrated slag due to the high Al 2 O 3 slag content. Upon decomposition, small metallic particles and pores are homogeneously generated inside the primary chromite. At the refractory/slag interface, a relatively continuous solid (Mg,Mn)[Al,Cr] 2 O 4 spinel layer is formed. Its density and stability decreases with higher temperatures and more turbulent conditions. The spinel formation arises through heterogeneous in situ precipitation from a slag rich in spinel forming compounds. Higher Al 2 O 3 levels in the slag promote the spinel layer formation, which may limit slag infiltration. Finally, it is shown that the present experimental procedure is an excellent tool to simulate refractory wear in industrial processes, diminishing the risks associated with plant trials.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Materials Engineering and Processing · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Extending the lining life of ALZ nv's ladle lining
2. Degradation mechanisms of magnesia-chromite refractories in vacuum-oxygen decarburisation ladles during the production of stainless steel10.1179/030192300677525 ↗
3. A study of slag-infiltrated magnesia-chromite refractories using hybrid microwave heating10.1016/S0955-2219(00)00343-5 ↗
4. New high-quality MgO-Cr2O3-bricks and Cr-free alternatives for the lining of RH/DH-vessels
5. Refractory wear in the argon–oxygen decarburization process
6. Slag testing of refactories for ladle refining by ESR method
7. Fused basic refractories in the argon–oxygen decarburization process
8. Application of high Cr2O3 magnesia chrome refractories to secondary refining systems
9. Texture and slag resistance of commercial fused magnesia-chrome clinker
10. Refractory/slag systems for ladle and secondary refining processes
11. Volume expansion and structural damage in periclase-chrome refractories
12. Dissolution of chromite in liquid slag: Empirical relationship
13. Use of phase diagrams in studies of refractory corrosion10.1179/095066000101528304 ↗
14. On the formation of protective spinel layers on refractories
15. Laboratory set-up to study refractories in VOD process conditions
16. Laboratory study of the interaction mechanisms between magnesia-chromite refractories and Al2O3-rich VOD slags
17. Optimisation of an accurate and precise and analysis procedure for metallurgical VOD slags with ICP-OES
18. Local corrosion of magnesia-chromite refractory at slag-metal interface
19. Jones, P. T., Degradation mechanisms of basic refractory materials during the secondary refining of stainless steel in VOD ladles. PhD Thesis, Leuven, 2000, Chapter VIII, 23.
20. Melt corrosion of oxide and oxide-carbon refractories10.1179/095066099101528234 ↗
21. Engh · 1992
22. Jones, P. T., Degradation mechanisms of basic refractory materials during the secondary refining of stainless steel in VOD ladles. PhD Thesis, Leuven, 2000, Chapter VII, 6.