Corrosion of spinel clinker by CaO–Al2O3–SiO2 ladle slag
Source abstract
Abstract
Abstract Three different grades of sintered spinel clinker were used containing 47, 69 and 94 wt.% Al 2 O 3 , respectively, i.e. MgO-rich, stoichiometric and Al 2 O 3 -rich. Based on these clinkers, the corrosion mechanism of each spinel clinker by CaO–Al 2 O 3 –SiO 2 slag was investigated and the corrosion and penetration behavior of castables containing powdered spinel clinker examined. A layer of MgO·(Al, Fe) 2 O 3 complex spinel formed at the slag-refractory interface was proportional to the MgO content of the spinel clinkers, and it depressed the slag corrosion. The free MgO and spinel minerals in each spinel clinker mainly trapped Fe 2 O 3 from the slag. CaO–Al 2 O 3 compounds were formed at the slag-clinker interface by the reaction between free Al 2 O 3 in the Al 2 O 3 -spinel clinker and CaO from slag. Slag penetration into the spinel clinkers was retarded by these compounds. As a result of adding fine spinel powder to the matrix of Al 2 O 3 -based castables, it was observed that higher content of MgO in spinel clinker showed better resistance to slag corrosion but lower resistance to slag penetration.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Wear mechanism of castable for steel ladle by slag
2. Improvement of alumina-magnesia castable for steel ladle wall
3. Effect of spinel raw material on corrosion resistance for steel ladle catable
4. Refractory characteristics of spinels with various MgO contents
5. Melt corrosion of oxide and oxide-carbon refractories10.1179/095066099101528234 ↗
6. Effect of CaO content on the hot strength of alumina-spinel castables in the temperature range of 1000–1500 °C10.1111/j.1151-2916.1998.tb02719.x ↗
7. Microstructural analysis of corroded alumina-spinel castable refractories10.1016/S0955-2219(96)00073-8 ↗
8. Melting relations of magnesium oxide-iron oxide mixtures in air
9. Direct and indirect dissolution of sapphire in calcia–magnesia–alumina–silica melts10.1111/j.1151-2916.1990.tb04269.x ↗