journal article·2007-01

Chemical durability of glazed surfaces

Linda Fröberg, Thomas Kronberg, Stina Törnblom, Leena Hupa

Publisher page

Abstract

Chemical durability of glazes is previously mostly studied as corrosion of the glassy phase. In this work the focus is on corrosion tendency of the typical crystalline phases in raw glazes. Fifteen experimental glazes were ball-milled of commercial raw materials. After fast-firing in industrial kiln and traditional firing in laboratory furnace the glazes were immersed in aqueous solutions of different pH. Changes in the phase composition of the surfaces were analysed with visual examination, XRD and SEM/EDX applying a procedure allowing to study the same crystal both before and after immersion. The results indicate that wollastonite type crystals were attacked in all but the most alkaline solutions. Diopside, quartz and corundum crystals did not show any marked attack. The interfacial layer around feldspar crystals as well as the glassy phase in the glazes corroded in the most acidic and alkaline environments.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Recycling and utilization of industrial and municipal waste in materials production · Pigment Synthesis and Properties · Recycling and Waste Management Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (14)

Show source-provided references
1. Corrosion of glazes and enamels
2. Kingery · 1976
3. Qualicer
4. Durability of mat glazes in hydrochloric acid solution10.4028/www.scientific.net/KEM.264-268.1565 ↗
5. Vane-Tempest · 2004 · Vol. I
6. Plasma-sprayed glass-ceramic coatings on ceramic tiles: microstructure, chemical resistance and mechanical properties10.1016/j.jeurceramsoc.2004.06.018 ↗
7. Thermal and chemical properties of diopside-wollastonite glass–ceramics in the SiO2–CaO–MgO system from raw materials10.1016/S0272-8842(02)00114-1 ↗
8. White · 1992
9. Dissolution of wollastonite and its flotation and surface interactions with tallow-1, 3-diaminopropane (duomeen T)10.1016/j.mineng.2004.11.001 ↗
10. Atomistic simulation of the surface structure of wollastonite and adsorption phenomena relevant to flotation10.1016/S0301-7516(03)00092-9 ↗
11. Experimental determination of the effect of dissolved CO2 on the dissolution kinetics of Mg and Ca silicates at 25°C10.1016/j.chemgeo.2004.12.011 ↗
12. McCracken · 1992
13. Chemical resistance and cleanability of glazed surfaces10.1016/j.susc.2004.11.048 ↗
14. Fröberg, L., Kronberg, T. and Hupa, L., Influence of firing parameters on phase composition of raw glazes, J. Eur. Ceram. Soc., accepted for publication.