The improvement in oxidation resistance of carbon by a graded SiC/SiO2 coating
Source abstract
Abstract
Abstract A dense functionally gradient SiC/SiO2 coating has been developed to improve the oxidation resistance of carbon at elevated temperatures. SiC was coated on the surface of a graphite substrate by a reaction between thermally evaporated silicon and carbon at 1400 °C. The SiO2 layer was deposited by exposing the SiC coated specimens next to a bed of Si powder in a flowing H2–H2O gas (PH2O=2.6×10−2 atm) at 1400 °C. The formed SiC/SiO2 layers were dense and had gradient compositions with good adhesion to the carbon substrate. However, as the coating thickness increased, the coating layer became cracked and delaminated from the substrate due to thermal stress. The specimens with the continuous SiC/SiO2 layer showed a remarkably improved oxidation resistance up to 1200 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Diamond and Carbon-based Materials Research · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Ceramic coatings for carbon–carbon composites
2. Evolution of in-situ refarctories in the 20th century10.1111/j.1151-2916.1998.tb02497.x ↗
3. Behavior of SiC and Al added to carbon-contaning refractories
4. Effect of refractory oxides on the oxidation of graphite and amorphous carbon10.1111/j.1151-2916.1996.tb09009.x ↗
5. High-temperature properties of unburned MgO-C bricks containing Al and Si powders10.1111/j.1151-2916.1998.tb02713.x ↗
6. Glass sealants for carbon–carbon composites10.1007/BF01151661 ↗
7. Booth, R. E., Shuford, D. M. and Linck, J. S., Conversion Coating on Carbon/Carbon Composites with Controlled Microstructure. US Patent 5330789, 19 July 1994.
8. Functionally gradient SiC coatings produced by chemical vapor reaction10.1557/PROC-363-251 ↗
9. CVD and CVR silicon-based functionally gradient coatings on C–C composites10.1016/0008-6223(94)00166-W ↗
10. Oxidation-resistant carbon–carbon composites up to 1700 °C10.1016/0008-6223(94)00173-W ↗
11. The improvement in oxidation resistance of CVD–SiC coated C/C composites by silicon infiltration pre-treatment10.1016/S0008-6223(97)00207-8 ↗
12. Protective glass coating for carbon–carbon composites10.1016/S0008-6223(98)00100-6 ↗
13. Oxidation protection of carbon–carbon composites by sol-gel ceramic coatings10.1023/A:1004739823438 ↗
14. Oxidation behavior of carbon–carbon composites with a three layer coating from room temperature to 1700 °C10.1016/S0008-6223(98)00293-0 ↗
15. Oxidation resistant SiC coating for graphite materials10.1016/S0008-6223(99)00010-X ↗
16. Improvement in oxidation resistance of carbon by formation of a protective SiO2 layer on the surface10.1016/S0955-2219(01)00213-8 ↗
17. Corrosion of silicon-based ceramics in combustion environments10.1111/j.1151-2916.1993.tb03684.x ↗
18. Volatility diagrams for silica, silicon nitride, and silicon carbide and their application to high-temperature decomposition and oxidation10.1111/j.1151-2916.1990.tb06677.x ↗