Degradation mechanisms of a SiC fiber reinforced self-sealing matrix composite in simulated combustor environments
Source abstract
Abstract
Abstract Non-oxide ceramic matrix composites are potential candidates to replace the current nickel-based alloys for a variety of high temperature applications in the aerospace field. The durability of a SiC(f)/PyC(i)/[Si, C, B](m) composite with a multi-layered self-sealing matrix and Hi-Nicalon fibers was investigated at 1200 °C for exposure durations up to 600 h. The specimens are aged in a variety of slow-flowing air/steam gas mixtures and total pressures, ranging from atmospheric pressure with a 10–50% water content to 1 MPa with 10–20% water content. The degradation of the composite was determined from the measurement of residual strength and strain to failure on post-exposure specimens and correlated with microstructural observation of the damaged tows. The most severe degradation of the composite occurred at 1 MPa in an air/steam (80/20) gas mixture. Correlation between this degradation and the dissolving of the SiC fibers in the generated boria-containing glass, is discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Lamouroux, F., Pailler, R., Naslain, R. and Cataldi, M., French Patent No. 95 14843, 1995.
2. Multilayer systems based on B, B4C, SiC and SiBC for environmental composite protection
3. Bouillon, E., Spriet, P., Habarou, G., Louchet, C., Arnold, T., Ojard, G. C. et al., Engine test and post engine test characterization of self sealing ceramic matrix composites for nozzle applications in gas turbine engines, ASME TURBO EXPO 2004. Power for Land, Sea and Air. Vienna, Austria, 2004. ID GT-2004-53976.10.1115/GT2004-53976 ↗
4. Martin, X., Rebillat, F. and Guette, A., Oxidation behavior of a multilayered (Si–B–C) ceramic in a complex atmosphere N2/O2/H2O. High Temp. Corros. Mater. Chem., in press.
5. Kinetic oxidation laws of boron carbide in dry and wet environments
6. Thermodynamic study of B2O3 reactivity in H2O(g)N2(g)/O2(g) atmospheres at high pressure and high temperature
7. Farizy, G., Mécanisme de fluage sous air de composites SiCf/SiBCm à matrice auto-cicatrisante. Ph.D. thesis, University of Caen, 2002.
8. Oxidation behaviour of a multi-layered ceramic matrix composite (SiC)f/C/(SiBC)m10.1016/S0266-3538(00)00243-8 ↗
9. Quemard, L., Rebillat, F., Guette, A., Tawil, H. and Louchet-Pouillerie, C., Corrosion behavior of a SiC fiber reinforced self sealing matrix composite at intermediate temperature and in a high pressure steam environment, in press.
10. Mechanical and thermal properties of a self sealing matrix composite and determination of the lifetime duration10.1002/9780470294628.ch54 ↗
11. Bouillon, E., Lamouroux, F., Baroumes, L., Cavalier, J. C., Spriet, P. and Habarou, G., An improved long life duration CMC for jet aircraft engine applications, ASME TURBO EXPO 2002. Amsterdam, The Netherlands, 2002. ASME ID GT-2002-30625.10.1115/GT2002-30625 ↗
12. High temperature oxidation of boron nitride. I. Monolithic boron nitride10.1111/j.1551-2916.1999.tb20075.x ↗
13. High temperature oxidation of boron nitride. II. Boron nitride layers in composites10.1111/j.1151-2916.1999.tb01944.x ↗
14. Paralinear oxidation of CVD SiC in water vapor10.1111/j.1151-2916.1997.tb02810.x ↗
15. Oxidation and volatilisation of silica formers in water vapor10.1111/j.1151-2916.2003.tb03459.x ↗
16. Oxidation kinetics of chemically vapor-deposited silicon carbide in wet oxygen10.1111/j.1151-2916.1994.tb05357.x ↗
17. Mass spectrometric identifictaion of Si–O–H(g) species from the reaction of silica with water vapor at atmospheric pressure10.1111/j.1151-2916.1997.tb02935.x ↗
18. SiC recession caused by SiO2 scale volatility under combustion conditions. I. Experimental results and empirical model10.1111/j.1151-2916.1999.tb02004.x ↗
19. SiC recession caused by SiO2 scale volatility under combustion conditions. II. Thermodynamics and gaseous diffusion model10.1111/j.1151-2916.1999.tb02005.x ↗
20. Degradation of silicon carbide in combustion gas flow at high temperature and speed
21. Development of an original design of high temperature–high pressure furnace
22. Approche des propriétés de l’interface fibre-matrice dans les composites à matrice céramiques: résistance à la décohesion
23. Assessment of a microcomposite test procedure for evaluating constituent properties of ceramic matrix composite10.1111/j.1151-2916.1995.tb08814.x ↗
24. A pervasive mode of oxidative degradation in a SiC–SiC composite10.1111/j.1151-2916.1998.tb02696.x ↗
25. Oxidative pest degradation of Hi-Nicalon/BN/SiC composite as a function of temperature and time in the burner rig
26. Tensile behavior of as-fabricated and burner rig exposed SiC/SiC composites with Hi-Nicalon Type S Fibers