Abstract The self-crack-healing ability was systematically studied using flexural strength measurement of beams containing a semi-elliptical surface crack made by Vickers indenter. Beams of Al2O3/SiC ceramic nanocomposite with a good self-crack-healing ability predetermined for four-point and three-point bend test were prepared by ceramographic techniques. Flexural strength and fracture toughness were determined using three- and four-point bend method. Thermal aging in range from 1000 °C up to 1300 °C for 1 h was applied to find optimal conditions to heal the samples pre-cracked by the indentation technique. Fractographical analyses using an optical and/or scanning electron microscopy has been carried out to investigate the surface crack behaviour. Very good self-crack healing ability has been proved for surface micro-cracks having length up to 250 μm and depth no higher than 100 μm.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Concrete and Cement Materials Research · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Strength recovery behaviour of machined Al2O3/SiC nano-composite ceramics by crack-healing10.1016/j.jeurceramsoc.2006.11.080 ↗
2. Crack-healing ability of structural ceramics and a new methodology to guarantee the structural integrity using the ability and proof-test10.1016/j.jeurceramsoc.2004.01.027 ↗
3. Crack healing behaviour and high-temperature strength of mullite/SiC composite ceramics10.1016/S0955-2219(01)00431-9 ↗
4. Crack-healing and mechanical behaviour of Al2O3/SiC composites at elevated temperature10.1111/j.1460-2695.2004.00785.x ↗
5. Crack-healing behaviour of mullite/SiC/Y2O3 composites and its application to the structural integrity of machined components10.1016/j.jeurceramsoc.2004.08.024 ↗
6. Crack-healing and oxidation behaviour of silicon nitride ceramics10.1016/S0955-2219(03)00645-9 ↗
7. Crack-healing behaviour and static fatigue strength of Si3N4/SiC ceramics held under stress at temperature (800, 900 and 1000°C)10.1016/S0955-2219(02)00428-4 ↗
8. Improvement of static fatigue strength of Si3N4/SiC crack-healed under cyclic stress10.1016/j.jeurceramsoc.2004.06.010 ↗
9. Crack-healing behaviour and resultant strength properties of silicon carbide ceramic10.1016/j.jeurceramsoc.2004.01.021 ↗
10. Microstructure and fracture-mechanical properties of carbon derived Si3N4+SiC nanomaterials10.1016/j.msec.2005.09.032 ↗
11. EN 843-1 Advanced technical ceramics. Mechanical properties of monolithic ceramic at room temperature. Part 1. Determination of flexural strength; 1995.
12. EN 843-2 Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature. Part 2. Determination of Young's modulus, shear modulus and Poisson's ratio; 2006.
13. Measurement of elastic constants of orthotropic materials by resonant frequency method