journal article·2000-09

Pressureless sintering of Al2O3 containing up to 20 vol% zirconium diboride (ZrB2)

Stefan Postrach, Jürgen Pötschke

Publisher page

Abstract

Abstract The production of particle composites by means of pressureless sintering provides a cost-effective alternative to production variants such as hot-pressing. However, minimal quantities of additives are sufficient to impede the densification of oxidic matrix components. This paper examines the sintering behaviour of alumina powder as a function of the volume fraction of ZrB 2 (up to 20 vol%). A distinction can be made between two sintering ranges according to the temperature: at T⩽1700° a solid-state process applies. This process is decisively influenced by the boron oxide (B 2 O 3 ) contained in the raw material ZrB 2 . The validity of the Lange model, which describes the influence of increasing volumes of inclusions on the densification behaviour of a crystalline matrix phase, is confirmed in this temperature range. At T >1700°C, an aluminium borate melt occurs, accelerating the sintering process substantially. As a result, the composites quickly attain matrix densities greater than 95% of the theoretical density. At higher firing temperatures the ZrB 2 particles coalesce, resulting in the formation of an electrically conductive penetration structure at a content level of 20 vol%.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Boron and Carbon Nanomaterials Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Effect of inclusions on densification10.1111/j.1151-2916.1992.tb07836.x ↗
2. Powell, C. F., Borides. In High Temperature Materials and Technology, ed. I. E. Campbell and E. M. Sherwood. John Wiley & Sons, Inc., New York, 1967.
3. Rahaman, M. N. and De Jonghe, L. C., Effect of rigid inclusions on the sintering of glass powder compacts. Journal of the American Ceramic Society, 1987, 70, C-348–C-351.10.1111/j.1151-2916.1987.tb04877.x ↗
4. Factors controlling the sintering of ceramic particulate composites10.1111/j.1151-2916.1992.tb04465.x ↗
5. X-ray photoelectron spectroscopy studies of metallic diborides10.1111/j.1151-2916.1992.tb05515.x ↗
6. Herstellung von mehrphasigen Hartstoffen im System B4C–Si–Ti durch reaktive Schmelzinfiltration, Sprechsaal
7. Effect of B2O3 addition on the sintering of α-Al2O310.1016/0272-8842(95)00050-X ↗
8. Preparation and characterization of aluminium borate10.1111/j.1151-2916.1992.tb05622.x ↗
9. Constrained network model for predicting densification behavior of composite powders10.1557/JMR.1987.0059 ↗
10. Schatt · 1992
11. Stranski, I. N., Eine Plauderei über Gleichgewichtsformen von Kristallen. Journal of Crystal Growth, 1972, 3–8.10.1016/0022-0248(72)90053-X ↗
12. Petzold, A., Ulbricht, J., Aluminiumoxid, Rohstoff-Werkstoff-Werkstoffkomponente. Deutscher Verlag für Grundstoffindustrie, Leipzig, 1991.
13. Telle, R., Boride and carbide ceramics. In Materials Science and Technology, A Comprehensive Treatment, Vol. 11, ed. R. W. Cahn, P. Haasen, E. J. Kramer, Structure and Properties of Ceramics, Ed. M. V. Swain. VCH Verlagsgesellschaft Weinheim, 1994.