journal article·2012-09

A dense and fine-grained SiC/Ti3Si(Al)C2 composite and its high-temperature oxidation behavior

Shibo Li, Gui-Ming Song, Yang Zhou

Publisher page

Abstract

A dense SiC/Ti3Si(Al)C2 composite was synthesized by in situ hot pressing powders of Si, TiC and Al as a sintering additive at 1500 ◦ C for 2 h under 30 MPa in Ar atmosphere. This composite has a fine-grained and homogeneous microstructure with grain sizes of 5m for Ti3Si(Al)C2 and of 1m for SiC. The SiC/Ti3Si(Al)C2 composite possesses an improved oxidation resistance, with parabolic rate constants of 4.57 × 10 −8 kg 2 /m 4 /s at 1200 ◦ C and 1.31 × 10 −7 kg 2 /m 4 /s at 1300 ◦ C. This study provides an experimental evidence to confirm the formation of amorphous phases in the oxide scale of the SiC/Ti3Si(Al)C2 composite. Microstructure and phase composition of the SiC/Ti3Si(Al)C2 composite and oxide scales were identified by X-ray diffractometry and scanning electron microscopy. The mechanism for the enhanced oxidation resistance has been discussed. © 2012 Elsevier Ltd. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Synthesis and characterization of a remarkable ceramic:Ti3SiC210.1111/j.1151-2916.1996.tb08018.x ↗
2. Titanium silicon carbide: a metal or a ceramic?
3. The Mn+1AXn phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
4. Progress in research and development on MAX phases: a family of layered ternary compounds10.1179/1743280410Y.0000000001 ↗
5. Oxidation behavior of Ti3SiC2 at high temperature in air10.1016/S0921-5093(02)00210-1 ↗
6. Oxidation behavior of silicide coating on Ti3SiC2-based ceramic10.1007/s10019-002-0201-7 ↗
7. Influence of Al–La co-cementation on the oxidation of Ti3SiC2-based ceramic10.1023/A:1024677632382 ↗
8. Mechanism for the enhanced oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution10.1016/j.actamat.2004.04.015 ↗
9. High-temperature oxidation of Ti3Al0.5Si0.5C2 compounds between 900 and 1200°C in air10.1016/j.jallcom.2008.01.111 ↗
10. Synthesis and high temperature mechanical properties of Ti3SiC2/SiC composite10.1007/BF01209221 ↗
11. Synthesis of Ti3SiC2/SiC and TiSi2/SiC composites using displacement reactions in the Ti–Si–C system10.1016/1359-6462(95)00663-X ↗
12. Mechanical properties and oxidation resistance of Ti3SiC2/SiC Composite by In Situ displacement reaction of Si and TiC10.1016/S0167-577X(02)01429-5 ↗
13. In situ synthesis of Ti3SiC2/SiC composite by displacement reaction of Si and TiC10.1016/j.msea.2004.03.046 ↗
14. Long time oxidation study of Ti3SiC2, Ti3SiC2/SiC and Ti3SiC2/TiC composites in air10.1149/1.1556035 ↗
15. Synthesis and characterization of 0.3 Vf TiC–Ti3SiC2 and 0.3 Vf SiC–Ti3SiC2 composites10.1016/S0925-8388(02)00985-4 ↗
16. In situ reaction synthesis and characterization of Ti3Si(Al)C2/SiC composites10.1016/j.ceramint.2005.07.004 ↗
17. Improved strength-impairing contact damages resistance of Ti3Si(Al)C2/SiC composites10.1016/j.jeurceramsoc.2006.07.018 ↗
18. Microstructure and properties of Ti3SiC2/SiC nanocomposites fabricated by spark plasma sintering10.1016/j.compscitech.2007.06.006 ↗
19. High temperature oxidation behavior and mechanism of Ti3SiC2–SiC nanocomposites in air10.1016/j.compscitech.2007.10.029 ↗
20. Rapid fabrication of Ti3SiC2–SiC nanocomposite using the spark plasma sintering–reactive synthesis (SPS–RS) method10.1016/j.scriptamat.2006.09.029 ↗
21. In situ processing and high-temperature properties of Ti3Si(Al)C2/SiC composites10.1111/j.1744-7402.2006.02057.x ↗
22. Ternary carbide of titanium and silicon
23. Reaction layers around SiC particles in Ti: an electron microscopy study10.1016/S1359-6454(99)00151-2 ↗
24. Experimental investigation and thermodynamic calculation of the titanium–silicon–carbon system10.1111/j.1151-2916.2000.tb01170.x ↗
25. High temperature oxidation behavior of Ti3SiC2-based material in air10.1016/S1359-6454(01)00247-6 ↗
26. Field-activated pressure-assisted combustion synthesis of polycrystalline Ti3SiC210.1557/JMR.1999.0124 ↗
27. Tribophysical properties of polycrystalline bulk Ti3AlC210.1111/j.1551-2916.2005.00588.x ↗
28. Synthesis and characterization of Ti3AlC210.1111/j.1151-2916.2000.tb01281.x ↗
29. Synthesis and deformation microstructure of solid solution Ti3SiAl0.2C1.810.1016/j.msea.2006.08.005 ↗
30. Effect of Al addition on pressure less reactive sintering of Ti3SiC210.1016/j.scriptamat.2006.08.019 ↗
31. Solid–liquid reaction synthesis of layered machinable Ti3AlC2 ceramic10.1039/b108685e ↗
32. Effect of aluminum on the reaction synthesis of ternary carbide Ti3SiC210.1016/S1359-6462(03)00391-9 ↗
33. Oxidation of Ti3SiC2 in air10.1149/1.1837846 ↗
34. Effect of Si content on the oxidation resistance of Ti3Al1−xSixC2 (x=0.25) solid solutions at 1000–1400°C in air10.1007/s11085-006-9007-0 ↗
35. The morphology of oxides and oxidation behavior of Ti3SiC2-based composite at high-temperature10.1016/S0266-3538(02)00285-3 ↗
36. Improving the high-temperature oxidation resistance of Zr2Al3C4 by silicon pack cementation10.1557/JMR.2008.0285 ↗
37. Oxidation behavior of Al4SiC4 ceramic up to 1700°C10.1016/j.corsci.2006.10.028 ↗
38. Formation of TiC hexagonal platelets and their growth mechanism10.1016/j.powtec.2007.09.018 ↗
39. Defect structures in single crystal TiC10.1080/01418619308221208 ↗
40. Reaction layers around SiC particles in Ti: an electron microscopy study10.1016/S1359-6454(99)00151-2 ↗
41. Si-induced twinning of TiC and formation of Ti3SiC2 platelets10.1016/S1359-6454(02)00248-3 ↗
42. Effects of Si and Al on twin boundary energy of TiC10.1016/S1359-6454(03)00032-6 ↗
43. Synthesis of Ti3AlC2 powders using Sn as an additive10.1111/j.1551-2916.2005.00818.x ↗
44. High temperature mass spectrometric study of the vaporization behaviour of SiC–SiO2 system10.1016/j.jallcom.2007.01.174 ↗
45. High-temperature passive oxidation of chemically vapor deposited silicon carbide10.1111/j.1151-2916.1989.tb07658.x ↗