Crystal growth of bismuth tungstate Bi2WO6 by slow cooling method using borate fluxes
Source abstract
Abstract
Abstract Ferroelectric Bi 2 WO 6 (BWO) single crystals have been grown by a flux method below the phase transition (ferro- to paraelectric) temperature. Sodium chloride, LiBO 2 , Li 2 B 4 O 7 (LBO), Na 2 B 4 O 7 (NBO) and Na 2 B 4 O 7 ·10H 2 O were selected as the flux. We found that LBO and NBO are suitable flux materials for crystal growth. The phase diagram of the BWO–LBO(NBO) system was investigated by the combination of the differential thermal analysis and the quench method. In the BWO–LBO(NBO) binary system, the mixtures of the end members without intermediate compounds were observed. On the basis of the phase diagram, we have obtained plate-like crystals with sizes up to 0.7 mm thickness from the solidified melts with the mole ratio BWO:LBO of 7:3. The crystals are single domain, yellow in color, and have well developed smooth {0 0 1} faces. The dielectric constant, ɛ 33 / ɛ 0 , of the crystals is 90 at room temperature and the ferroelectric behavior is available.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Solid-state spectroscopy and crystallography · Optical and Acousto-Optic Technologies · Acoustic Wave Resonator Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. Polymorphism and properties of Bi2WO6 and Bi2MoO610.1002/pssa.2210930106 ↗
2. Growth, crystallography and dielectric properties of Bi2WO610.1080/00150197208241519 ↗
3. The Bi2O3–WO3 system
4. Flux growth of Bi2WO6 single crystal below the transformation temperature10.1016/0022-0248(78)90327-5 ↗
5. Flux growth of bismuth tungstate, Bi2WO610.1016/0022-0248(81)90463-2 ↗
6. Crystal structure of Bi2WO610.1016/0038-1098(69)90288-9 ↗
7. Structure refinement of commensurately modulated bismuth tungstate, Bi2WO610.1107/S0108768191008030 ↗