High temperature oxidation of multilayered SiC processed by tape casting and sintering
Source abstract
Abstract
The oxidation behaviour of a multilayer SiC ceramic was investigated at high temperatures. The ceramic samples were processed by tape casting of a slurry containing α-SiC powders, forming of green tubular components and sintering without pressure. The oxidation resistance of this ceramic material was investigated by temperature programmed oxidation (TPO); the gaseous oxidation products were analysed by mass spectrometry. Thermal gravimetric analyses (TGA) were also performed. Buckles, machined from the multilayer ceramic tubes, were submitted to long-term oxidation treatments carried out at 1200, 1400 and 1600 °C in air. The microstructure and the radial compressive strength of these specimens were compared before and after oxidation. Microstructure was investigated by SEM–EDS and X-ray diffraction. The multilayered SiC showed increased toughness with respect to conventional ceramics, owing to delamination phenomena occurring before failure. Oxidation mainly affected the material surface, where a thin layer of silica grew. Oxidation treatments did not suppress the energy adsorbing mechanism occurring during the fracture process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. 1995
2. Interface characterization by TEM, AES and SIMS in tough SiC (ex-PCS) fibre-SiC (CVI) matrix composites with a BN interphase10.1007/BF01159815 ↗
3. Identification of carbon sublayer in a Hi-Nicalon/BN/SiC composite10.1023/A:1006695105463 ↗
4. Oxidation mechanism and kinetics of a 1D-SiC/C/SiC composite material: I, an experimental approach10.1111/j.1151-2916.1994.tb07015.x ↗
5. Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D-Nicalon/C/SiC composites: 1 ageing under vacuum or argon10.1016/S0955-2219(96)00067-2 ↗
6. Effect of ageing treatments at high temperatures on the microstructure and mechanical behaviour of 2D-Nicalon/C/SiC composites: 2 ageing under CO and influence of a SiC seal-coating10.1016/S0955-2219(96)00204-X ↗
7. Degradation at 1200 °C of a SiC coated 2D-Nicalon/C/SiC composite processed by Sicfill method10.1016/S0955-2219(00)00029-7 ↗
8. Mechanical properties of oxidation-resistant SiC/C compositionally graded graphite materials10.1111/j.1151-2916.1997.tb03209.x ↗
9. Multi-layer CVD-SiC coating for oxidation protection of carbon/carbon composite
10. Fibre and interfacial properties measured in situ for a 3D woven SiC/SiC-based composite with glass sealant10.1016/S1359-835X(98)00154-7 ↗
11. Davies, I. J., Ishikawa, T., Suzuki, N., Shibuya, M., Hirokawa, T. and Gotoh, J., Tensile and in situ fibre properties of 3-D SiC/SiC-based composite tested at elevated temperature in vacuum and air with and without an oxidation protection system. In Ceramic Engineering and Science Proceedings, Proc. of the 1998 22nd Annual Conference on Composites, Advanced Ceramics, Materials and Structures: A. Part 1. Cocoa Beach, Fl, USA, 1998, pp. 275–282.10.1002/9780470294482.ch31 ↗
12. Thick sol-gel coatings based on the B2O3–SiO2 system10.1016/S0022-3093(97)00073-2 ↗
13. Lipetzky, P. and Hilig, W.B., Limitations and benefits to the use of structural silicides under combustion conditions. In Processing and design issues in high temperature materials, Proceedings of the Engineering Foundation Conference, Davos (Switz.), 1996; Minerals, Metals and Materials Soc. (TMS), Warrendale, PA, USA 1997 pp. 359–367.
14. Surface oxidation by microwave-induced plasma of candidate composite materials for space shuttle protection10.1007/BF00582490 ↗
15. Tape casting of high dielectric ceramic composite substrates for microelectronic application10.1016/S0924-0136(99)00131-4 ↗
16. Tape casting of aqueous Al2O3 slurries10.1016/S0955-2219(00)00043-1 ↗
17. Al2O3/TiC/(MoSi2+Mo2B5) multilater composite prepared by tape casting10.1016/S0955-2219(99)00031-X ↗
18. The fabrication and failure of laminar ceramic composites10.1016/0956-7151(92)90471-P ↗
19. Alumina and alumina/zirconuia multilayer composites obtained by slip casting10.1111/j.1151-2916.1989.tb07692.x ↗
20. Tape casting of Al2O3/ZrO2 laminated composites10.1111/j.1151-2916.1986.tb04836.x ↗
21. Microstructure and high-temperature mechanical behavior of alumina/alumina–yttria-stabilized tetragonal zirconia multilayer composites10.1111/j.1151-2916.1997.tb03097.x ↗
22. Multilayer Al2O3/SiC ceramic with improved mechanical behavior10.1016/S0955-2219(00)00048-0 ↗
23. Fracture behavior of multilayer silicon nitride/boron nitride ceramics10.1111/j.1151-2916.1996.tb08996.x ↗
24. Processing of a novel multilayered silicon nitride10.1111/j.1151-2916.1996.tb08959.x ↗
25. Fracture behavior of chemically-vapor-deposited SiC-coated graphite: I, experimental results10.1111/j.1151-2916.1993.tb06610.x ↗
26. Multilayer composites in Al2O3 /MoSi2 system10.1016/S0254-0584(00)00448-X ↗
27. Mullite/zirconia laminate composites for high temperature application10.1016/S0955-2219(00)00157-6 ↗
28. Flexural properties of brittle multilayer materials: I, modelling10.1111/j.1151-2916.1994.tb05350.x ↗
29. Crack deflection in ceramic/ceramic laminates with strong interfaces10.1111/j.1151-2916.1995.tb08455.x ↗
30. Toughening of layered ceramic composites with residual surface compression10.1111/j.1151-2916.1996.tb07883.x ↗
31. Residual stresses in alumina-zirconia laminates10.1016/S0955-2219(99)00103-X ↗