Microwave dielectric properties of Mg4Nb2O9–3.0wt.% LiF ceramics prepared with CaTiO3 additions
Source abstract
Abstract
Abstract A family of low-temperature co-fired ceramics (LTCC) based on mixtures of Mg4Nb2O9–3.0 wt.% LiF (MNLF) and CaTiO3 ceramics has been investigated for microwave applications. In this study, it was found that, when increasing amounts of CaTiO3 additions from 0 to 10 wt.%, the temperature coefficient of resonant frequency (τf) extremely varied from −71.5 to 39.9 ppm/°C. The dielectric constants (ɛr) increased from 12.3 to 18.3 and the quality factor (Q·f) drastically decreased from 118,989 to 11,119 GHz. From these results, the MNLF–6 wt.% CaTiO3 ceramic sintered at 950 °C for 10 h was shown to be the appropriate dielectric properties: ɛr = 15.7, Q·f = 22,098 GHz, and τf = −3.3 ppm/°C. As for the chemical compatibility of MNLF–6 wt.% CaTiO3 ceramic with Ag, any secondary phase was not recognized from the XRPD profile of the samples heat-treated at 920 °C for 10 h. Thus, it was considered that the MNLF–x wt.% CaTiO3 ceramics are applicable to the multilayer devices with silver.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microwave Dielectric Ceramics Synthesis · Ferroelectric and Piezoelectric Materials · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. Low-fire bismuth-based dielectric ceramics for microwave use10.1143/JJAP.31.3152 ↗
2. Low-firing and microwave dielectric properties of Ba[(Ni0.6Zn0.4)0.33Nb0.67]O3 ceramics doped with Sb2O5 and B2O310.1023/A:1004523502454 ↗
3. Effect of B2O3 additives on sintering and microwave dielectric behaviors of CuO-doped ZnNb2O6 ceramics10.1143/JJAP.41.758 ↗
4. Improvements in the sintering and microwave properties of BiNbO4 microwave ceramics by V2O5 addition10.1016/S0955-2219(99)00228-9 ↗
5. Use of titanates to achieve a temperature-stable low-temperature co-fired ceramic dielectric for wireless applications10.1111/j.1151-2916.2002.tb00179.x ↗
6. Crystal structure of corundum type Mg4(Nb2−xTax)O9 microwave dielectric ceramics with low dielectric loss10.1016/S0955-2219(03)00167-5 ↗
7. Single crystal structure refinement of a magunesium niobium oxide: Mg4Nb2O910.1016/S0025-5408(00)00300-7 ↗
8. Use of LiF to achieve a low-temperature co-fired ceramics (LTCC) with low dielectric loss
9. A dielectric resonator method of measuring inductive capacities in the millimeter range10.1109/TMTT.1960.1124749 ↗
10. Ba(Zn1/3Ta2/3)O3 ceramics with low dielectric loss at microwave frequencies10.1111/j.1151-2916.1983.tb10074.x ↗
11. Barium rare-earth zirconates: synthesis, characterization and their possible application as substrates for YBa2Cu3O7−δ superconductors10.1016/0025-5408(95)00162-X ↗
12. Interaction of Ag/Pb metallization with lead and Bismuth oxide-based fluxes in multilayer ceramic capacitors10.1111/j.1151-2916.1992.tb05584.x ↗