Reactive consolidation of layered-ternary Ti2AlN ceramics by spark plasma sintering of a Ti/AlN powder mixture
Source abstract
Abstract
Abstract A reactive consolidation process for preparing ternary Ti2AlN ceramics was investigated by spark plasma sintering (SPS). A Ti/AlN powder mixture with a molar ratio of 2:1 was consolidated at temperatures ranging from 800 to 1450 °C. The phase composition and microstructure evolution during the process were characterized by X-ray diffraction (XRD) and scanning electron microscopy (SEM) equipped with an energy dispersive spectroscopy (EDS). A series of intermediate phases, namely TiN, Ti3Al, Ti3AlN and TiAl were indentified, which revealed a reaction pathway towards the formation of Ti2AlN.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Metal and Thin Film Mechanics · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. The MN+1 AXN phases: a new class of solids; thermodynamically stable nanolaminates10.1016/S0079-6786(00)00006-6 ↗
2. Processing and characterization of Ti2AlC, Ti2AlN, and Ti2AlC0.5N0.510.1007/s11661-006-0243-3 ↗
3. Layered machinable ceramics for high temperature applications10.1016/S1359-6462(96)00418-6 ↗
4. Electronic structure and bonding properties of layered machinable Ti2AlC and Ti2AlN ceramics10.1103/PhysRevB.61.12570 ↗
5. Ti2AlN, eine stickstoffhaltige H-phase10.1007/BF00905710 ↗
6. Effect of shock-activation on post-shock reaction synthesis of ternary ceramics10.1063/1.1483729 ↗
7. Synthesis and microstructure of layered-ternary Ti2AlN ceramic10.1016/j.scriptamat.2007.01.049 ↗
8. An approach to the synthesis of AlN–Ti2AlN composite10.2497/jjspm.56.541 ↗
9. Synthesis of high-purity bulk Ti2AlN by spark plasma sintering (SPS)10.1016/j.ceramint.2007.04.009 ↗
10. Formation of tough interlocking microstructures in silicon nitride ceramics by dynamic ripening10.1038/417266a ↗
11. Consolidation enhancement in spark-plasma sintering: impact of high heating rates10.1063/1.2822189 ↗
12. The effect of electric field and pressure on the synthesis and consolidation of materials: a review of the spark plasma sintering method10.1007/s10853-006-6555-2 ↗
13. Fundamental investigations on the spark plasma sintering/synthesis process. III. Current effect on reactivity10.1016/j.msea.2005.06.066 ↗
14. Application of pulse discharge sintering (PDS) technique to rapid synthesis of Ti3SiC2 from Ti/Si/C powders10.1016/S0955-2219(02)00044-4 ↗
15. Synthesis of high-purity polycrystalline Ti3AlC2 through pulse discharge sintering Ti/Al/TiC powders10.1016/j.jallcom.2007.02.105 ↗
16. Synthesis reactions for Ti3AlC2 through pulse discharge sintering Ti/Al4C3/TiC powder mixture10.1016/j.scriptamat.2006.07.018 ↗
17. Rapid synthesis of Ti2AlC by spark plasma sintering technique10.1016/j.matlet.2004.07.052 ↗
18. Synthesis and characterization of Cr2AlC ceramics prepared by spark plasma sintering10.1016/j.matlet.2007.02.023 ↗
19. Phase equilibria in the Ti–Al binary system10.1016/S1359-6454(00)00118-X ↗
20. Solid-state phase equilibria in the titanium–aluminum–nitrogen system10.1007/s11669-004-0134-5 ↗
21. Fast densification and deformation of titanium powder10.1179/174329005X71939 ↗
22. Fundamental investigations on the spark plasma sintering/synthesis process. II. Modeling of current and temperature distributions10.1016/j.msea.2004.11.019 ↗
23. Modelling of the temperature distribution during field assisted sintering10.1016/j.actamat.2005.05.042 ↗
24. Microstructural characterization and phase development at the interface between aluminum nitride and titanium after annealing at 1300–1500°C10.1111/j.1551-2916.2005.00880.x ↗