Abstract
Cracking of wet-chemically precipitated nanocrystalline TiO2 films deposited on different platelet-like substrates is investigated. The thicknesses of the films are also in the nanometric range: 60, 140 or 300 nm. Scanning electron microscopy, X-ray diffraction and nitrogen adsorption are employed to determine layer thickness, grain size, and porosity. The synthesis of TiO2 films through an aqueous route affords very good reproducibility of these properties (layer thickness ±5 nm). Mica, SiO2 and Al2O3 platelets are used as substrates, providing different properties with regard to surface charge, structure and roughness. The drying step is found to be responsible for the cracking of some of the TiO2 layers and the evolution of the cracks during sintering is related to shrinkage of the substrate. Film thickness as well as the chemical nature of the substrate influences the cracking of nanocrystalline TiO2 films during the drying step.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Advanced ceramic materials synthesis · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Angle-dependent optical effects deriving from submicron structures of films and pigments10.1021/cr970075u ↗
2. Effect pigments-past, present and future10.1016/j.porgcoat.2005.07.003 ↗
3. Synthesis of glasses from gels: the problem of monolithic gels10.1007/BF01203507 ↗
4. Attempts to avoid cracks during drying10.1016/0022-3093(88)90024-5 ↗
5. Deposition and sintering of particle films on a rigid substrate10.1111/j.1151-2916.1987.tb05645.x ↗
6. Flaw generation during constrained sintering of metal-glass multilayer films10.1111/j.1151-2916.1989.tb06297.x ↗
7. Mechanics of sintering thin films-II cracking due to self-stress10.1016/0167-6636(90)90034-D ↗
8. Theory of drying10.1111/j.1151-2916.1990.tb05082.x ↗
9. Drying of granular ceramic films: I effect of processing variables on cracking behavior10.1111/j.1151-2916.1993.tb07762.x ↗
10. Drying of granular ceramic films: II drying stress and saturation uniformity10.1111/j.1151-2916.1993.tb04014.x ↗
11. Crack growth and damage in constrained sintering films10.1111/j.1151-2916.1993.tb03969.x ↗
12. Reed · 1995
13. Rahaman · 2003
14. Cracking and orientation of solution-deposited rutile TiO2 films10.1021/cm035107a ↗
15. The decohesion of thin films from brittle substrates10.1016/0001-6160(88)90282-9 ↗
16. Buckle delamination of textured TiO2 thin films on mica10.1016/j.tsf.2005.04.075 ↗
17. Bauer, G., Osterried, K., Schmidt, C., Vogt, R., Kniess, H. B., Uhlig, M. et al., Coloured and coated platelike pigments. WO Patent 93/08237, 1991.
18. Jolivet · 2000
19. Muscovite surface structure imaged by fluid contact mode AFM10.1007/s002690050177 ↗
20. New effect pigments using innovative substrates Silica and alumina platelets extend the product variety and performance range of pearlescent pigments
21. The isoelectric points of sapphire crystals and alpha-alumina powder10.1016/S0927-7757(02)00366-7 ↗
22. Shrinkage during drying of silica gel10.1016/0022-3093(95)00187-5 ↗
23. Shrinkage of silica gels aged in TEOS10.1016/0022-3093(96)00136-6 ↗
24. Drying gels II film and flat plate10.1016/S0022-3093(87)80334-4 ↗
25. Drying gels VIII revision and review10.1016/0022-3093(89)90029-X ↗
26. Constrained film sintering of nanocrystalline TiO210.1111/j.1151-2916.2000.tb01487.x ↗
27. Legrand · 1998
28. High-temperature healing of lithographically introduced cracks in sapphire10.1111/j.1151-2916.1990.tb06558.x ↗
29. Instability of polycrystalline bridges that span cracks in powder films densified on a substrate10.1111/j.1151-2916.1994.tb05366.x ↗
30. Chemical solution routes to single-crystal thin films10.1126/science.273.5277.903 ↗
31. Single-step dip coating of crack-free BaTiO3 films>1μm thick: effect of poly(vinylpyrrolidone) on critical thickness10.1111/j.1151-2916.2000.tb01330.x ↗
32. Freund · 2003
33. Crack formation in TiO2 films prepared by sol–gel processing: quantification and characterization10.1016/j.tsf.2006.11.193 ↗