Injection molding of surface modified powders with high solid loadings: A case for fabrication of translucent alumina ceramics

Wei Liu, Zhipeng Xie, Tiezhu Bo, Xianfeng Yang

Publisher page

Abstract

Abstract Solid loading is a critical key to the fabrication of ceramic compacts with high densities via ceramic injection molding. As reported in most previous work, solid loading of ultra-fine alumina feedstock system could be achieved only up to ∼58 vol% with stearic acid (SA) as the surface modification agent. In present work, different from the traditional work in which SA has been introduced just in the powder blending process, we have successfully prepared the feedstock with a much higher solid loading up to ∼64 vol% by a prior ball milling treatment of ceramic powders with a small amount of SA before the traditional blending process. It can be attributed to that SA can be coated homogeneously around the powder surfaces by a chemical reaction induced by ball milling treatment. Highly translucent Al2O3 ceramics have been fabricated, which suggests an alternative route for fabrication of translucent ceramics with high quality.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Injection Molding Process and Properties · Advanced materials and composites · Epoxy Resin Curing Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Production of micro-porous austenitic stainless steel by powder injection molding10.1016/j.scriptamat.2007.10.004 ↗
2. The rheologyical effect of carbon nanotubes on the iron based metal powder injection molding feedstock
3. Production of alumina parts by powder injection molding with a binder system based on high density polyethylene10.1016/j.jeurceramsoc.2007.08.004 ↗
4. Influence of solid loading and particle size distribution on the porosity development of green alumina ceramic mouldings10.1016/S0272-8842(96)00063-6 ↗
5. Effects of stearic-acid on the injection-molding of alumina10.1111/j.1151-2916.1995.tb08050.x ↗
6. Influence of stearic acid on suspension structure and green microstructure of injection-molded zirconia ceramics10.1016/S0272-8842(98)00024-8 ↗
7. Mechanism of thermal debinding and water debinding for ceramic injection molding
8. Particle packing in ceramic injection-molding10.1111/j.1151-2916.1990.tb06742.x ↗
9. Preparation of hard metal (WC-10Co) components by powder injection moulding10.4028/www.scientific.net/KEM.189-191.579 ↗
10. Interaction between binder and powder in injection-molding of alumina10.1007/BF01151118 ↗
11. Sacks · 1987 · 11
12. The use of silane coupling agents in ceramic injection moulding10.1007/BF01115777 ↗
13. Surface modification of powders with carboxylic-acids10.1007/BF01730436 ↗
14. Torque evolution and effects on alumina feedstocks prepared by various kneading sequences10.1016/S0955-2219(99)00061-8 ↗
15. Dispersion of nano-sized γ-alumina powder in non-polar solvents10.1111/j.1551-2916.2005.00858.x ↗
16. Development of niobium powder injection molding. Part I. Feedstock and injection molding10.1016/j.ijrmhm.2005.06.003 ↗
17. Properties of ceramic injection moulding formulations10.1007/BF01160583 ↗
18. Rheology of injection-molded zirconia-wax mixtures10.1023/A:1004727214419 ↗
19. Ivensen · 1973
20. The influence of powder loading and binder additive on the properties of alumina injection-moulding blends10.1007/BF01171549 ↗