Synthesis, microstructure, and mechanical properties of WC–TiC–Co ceramic composites
Source abstract
Abstract
Abstract A ceramic composite constituting the formula 78 wt% WC–16 wt% TiC–6 wt% Co denoted as the 78WC–16TiC–6Co ceramic composite was fabricated using a powder metallurgy process, by utilising commercially available WC and Co powders, and laboratory produced TiC powders. TiC powders were produced from machining chips of Grade 4 Titanium. Five different procedures were followed for the manufacturing process by altering the amount of the binding agent (stearic acid) and/or compacting pressure and/or sintering regime (temperature and time) and/or mixing process (dry mixing and mechanical alloying). Characterisation investigations conducted on the sintered samples revealed that stearic acid as the binding agent resulted in the decrease of the relative density while mechanical alloying (MA) induced finer microstructures. The 78WC–16TiC–6Co composites manufactured from commercially available and laboratory produced TiC powders using similar process procedures (including MA) exhibited similar characteristics in terms of relative density, hardness, and wear performance.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Orthopaedic implants and arthroplasty · Tunneling and Rock Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Kriz R. Sintering of a Powder Compact. Virginia Tech; 2004. http://www.sv.vt.edu/classes/MSE2034_NoteBook/MSE2034_kriz_NoteBook/diffusion/apps/sinter.html. [last accessed 27.05.10].
2. Brookes · 1998
3. Schwartzkopf · 1953
4. Toth · 1971
5. Physical and chemical nature of cemented carbides10.1179/095066079790136363 ↗
6. Brooks · 1983
7. Report on carcinogens background document for cobalt–tungsten carbide: powders and hard metals. U.S. Department of Health and Human Services; 2009.
8. Effect of WC/TiC grain size ratio on microstructure and mechanical properties of WC–TiC–Co cemented carbides10.1016/j.ijrmhm.2005.04.018 ↗
9. Consolidation of binderless WC–TiC by high frequency induction heating sintering10.1016/j.ijrmhm.2007.01.006 ↗
10. Microstructure and wear behavior of laser-textured and micro-alloyed Co-based WC and TiC composite sintered-carbide coating10.1016/j.jmatprotec.2008.02.045 ↗
11. Grain and phase boundary segregation in WC–Co with TiC, ZrC, NbC or TaC additions10.1016/j.ijrmhm.2010.06.010 ↗
12. Properties of ultra-fine grain binderless cemented carbide ‘RCCFN’10.1016/0263-4368(95)92676-B ↗
13. Rapid sintering of ultra-fine WC–10 wt% Co by high-frequency induction heating10.1007/s10853-005-2422-9 ↗
14. Rapid sintering process and mechanical properties of binderless ultra fine tungsten carbide10.1016/j.msea.2006.07.127 ↗
15. Application of a wax-based binder in PIM of WC–TiC–Co cemented carbides, Int10.1016/j.ijrmhm.2005.04.006 ↗
16. Microstructural characterization of WC–TiC–Co cutting tools during high-speed machining of P20 mold steel10.1016/j.matchar.2003.10.005 ↗
17. Trent · 2000
18. Peştreli D. Effect of Mechanical Alloying on The Sintering Behaviour of WC–Co Hardmetal System. MSc. Thesis, Istanbul Technical University, Istanbul; 2009.
19. Wirmark · 1983
20. Strength and reinforcement of interfaces in cemented carbides10.1016/j.ijrmhm.2005.05.010 ↗
21. Analysis of interfaces in WC–Co with cubic carbide additions
22. Effects of cobalt intergranular segregation on interface energetics in WC–Co10.1016/j.actamat.2004.01.013 ↗
23. Cermets: I, fundamental concepts related to microstructure and physical properties of cermet systems10.1111/j.1151-2916.1956.tb15624.x ↗
24. Duman D. Production of Titanium Carbide Powder From Titanium Scrap and Its Utilization in Hard Metal Production, MSc. Thesis, Istanbul Technical University, Istanbul; 2010.
25. Characterization of WC–Co with cubic carbide additions10.1016/j.ijrmhm.2008.11.007 ↗
26. Microstructure of (W,Ti)C–Co system containing platelet WC10.1016/j.msea.2010.06.056 ↗
27. Wachtman · 2009
28. Influence of porosiy on hardness and Young's modulus of nanoporous EB-PVD TBC's by nanoindentation10.1016/j.matlet.2005.06.014 ↗
29. Porosity-dependence of elastic moduli and hardness of 3Y-TZP ceramics10.1016/S0272-8842(98)00037-6 ↗
30. Bhurshan · 1999