journal article·2013-09

Microstructure, mechanical and thermal properties of in situ toughened boron carbide-based ceramic composites co-doped with tungsten carbide and pyrolytic carbon

Jie Yin, Zhengren Huang, Xuejian Liu, Zhaoquan Zhang, Dongliang Jiang

Publisher page

Abstract

Abstract Boron carbide (B 4 C)-based ceramics were pressureless sintered to a relative density of 96.1% at 2150 °C, with the co-incorporation of tungsten carbide and pyrolytic carbon. The as-batched boron carbide power was 7.89 m 2 g −1 in surface area. A level of fracture toughness as high as 5.80 ± 0.12 MPa m 1/2 was achieved in the BW-6C composite. Sintering aids of carbon and tungsten boride were formed by an in situ reaction. The toughness improvement was attributed to the presence of thermal residual stress as well as the W 2 B 5 platelets. The thermal conductivity and thermal expansivity of the BW-6C composite as a function of temperature are also reported in this work. Our current study demonstrated that the B 4 C–W 2 B 5 composites could be potential candidate materials for structural applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Boron and Carbon Nanomaterials Research · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Pressureless sintering of boron carbide10.1111/j.1151-2916.2003.tb03498.x ↗
2. Synthesis and consolidation of boron carbide: a review10.1179/095066009X12506721665211 ↗
3. High-hardness B4C textured by a strong magnetic field technique10.1016/j.scriptamat.2010.10.010 ↗
4. Flexural strength, fracture toughness, and hardness of silicon carbide and boron carbide armor ceramics10.1111/j.1744-7402.2010.02501.x ↗
5. In situ boron carbide–titanium diboride composites prepared by mechanical milling and subsequent spark plasma sintering10.1007/s10853-008-2563-8 ↗
6. Improvements of the microstructure and erosion resistance of boron carbide with additives10.1023/A:1004888522607 ↗
7. U.S. Patent. 4320204. Sintered high density boron carbide; 1982.
8. The influence of carbon on the microstructure and mechanical properties of sintered boron carbide10.1016/0022-5088(81)90195-8 ↗
9. Properties of polycrystalline boron carbide sintered in the presence of tungsten boride (W2B5) without pressing10.1007/BF00722070 ↗
10. Hardness and fracture toughness of pressureless-sintered boron carbide (B4C)10.1111/j.1151-2916.2002.tb00260.x ↗
11. Thevenot · J Eur Ceram Soc · 1990 · 6 · 20510.1016/0955-2219(90)90048-K ↗
12. Processing of in situ toughened B–W–C composites by reaction hot pressing of B4C and WC10.1016/S1359-6462(00)00502-9 ↗
13. Microstructural coarsening during sintering of boron carbide10.1111/j.1151-2916.1989.tb06252.x ↗
14. Processing and mechanical properties of boron carbide sintered with TiC10.1016/S0955-2219(98)00071-5 ↗
15. Barsoum · 2003
16. Rahaman · 2003
17. Microcracking in B4C–TiB2 composites10.1111/j.1151-2916.1995.tb08671.x ↗
18. The effects of residual stress distributions on indentation-induced microcracking in B4C–TiB2 eutectic ceramic composites10.1111/j.1551-2916.2011.04664.x ↗
19. Rudy E, Windisch S. Ternary phase equilibria in transition metal–boron–carbon–silicon systems, Report No. AFML-TR-65-2, Contract No. USAF 33(615)-1249. Air Force Materials Laboratory, Wright-Patterson Air Force: Base, Ohio, 1965, p. 1–72.10.21236/ADA470307 ↗
20. Pressureless sintering of boron carbide10.1016/j.ceramint.2005.02.008 ↗
21. High toughness in pressureless densified ZrB2-based composites co-doped with boron–titanium carbides10.1016/j.scriptamat.2011.12.036 ↗
22. Microstructure and mechanical properties of hot-pressed B4C/(W,Ti)C ceramic composites10.1016/S0272-8842(01)00113-4 ↗
23. Toughening of a particulate-reinforced ceramic-matrix composite by thermal residual stress10.1111/j.1151-2916.1990.tb05209.x ↗
24. Mechanical properties of WC–WB–W2B composites prepared by reaction sintering of B4C–W–WC powders10.1016/S0955-2219(03)00253-X ↗
25. Boride-based hard materials
26. Pressureless sintered in situ toughened ZrB2–SiC platelets ceramics10.1016/j.jeurceramsoc.2011.04.040 ↗
27. Boron-rich solids: a chance for high-efficiency high-temperature thermoelectric energy conversion10.1016/0921-5107(94)04023-W ↗
28. The influence of W2B5 addition on microstructure and thermoelectric properties of B4C ceramic10.1016/S0272-8842(99)00089-9 ↗
29. Mechanical and thermal properties of 99% and 92% alumina at cryogenic temperatures10.1016/j.ceramint.2011.03.066 ↗
30. Preparation and thermoelectric characterization of SiC–B4C composites10.1007/s11664-010-1129-0 ↗