journal article·2011-01

Microstructure homogeneity control in spark plasma sintering of Al2O3 ceramics

Cao Wang, Xin Wang, Zhe Zhao

Publisher page

Abstract

Homogeneous microstructure control in the SPS (spark plasma sintering) sintered big size Al2O3 ceramic was realized by the synergy effect of grain boundary tailoring and proper pressure profile design. Two-step pressure profile itself did not show any efficient densification enhancement if no grain boundary modifier MgO added. The two-step pressure profile can effectively reduce average grain size and grain size difference over the sintered specimen, while MgO doping can reduce the average grain size in the whole sintered samples. Finally, a general strategy to overcome the intrinsic temperature gradient in SPS is suggested.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
2. Spark plasma sintering of nano-crystalline ceramics10.4028/www.scientific.net/KEM.264-268.2297 ↗
3. Grain-size effects on the ferroelectric behavior of dense nanocrystalline BaTiO3 ceramics10.1103/PhysRevB.70.024107 ↗
4. Spark plasma sintering of alumina10.1111/j.1151-2916.2002.tb00381.x ↗
5. Transparent polycrystalline alumina using spark plasma sintering: effect of Mg, Y and La doping10.1016/j.jeurceramsoc.2009.12.001 ↗
6. Spark plasma sintering of transparent alumina10.1016/j.scriptamat.2007.06.009 ↗
7. Optically transparent polycrystalline Al2O3 produced by spark plasma sintering10.1111/j.1551-2916.2007.02086.x ↗
8. Transparent nanometric cubic and tetragonal zirconia obtained by high-pressure pulsed electric current sintering10.1002/adfm.200600959 ↗
9. Transparent MgAl2O4 ceramic produced by spark plasma sintering10.1016/j.scriptamat.2009.03.039 ↗
10. Formation of Al2O3 grains with different sizes and morphologies during the pulse electric current sintering process10.1557/JMR.2001.0482 ↗
11. Direct evidence of temperature variation within ceramic powder compact during pulse electric current sintering10.1111/j.1551-2916.2005.00722.x ↗
12. Differential sintering by improper selection of sintering parameters during pulse electric current sintering10.1111/j.1551-2916.2004.00159.x ↗
13. Pressure effect on the homogeneity of spark plasma-sintered tungsten carbide powder10.1111/j.1551-2916.2009.03211.x ↗
14. Study of temperature field in spark plasma sintering10.1016/S0921-5107(01)00780-2 ↗
15. Finite element modeling of electric current-activated sintering: the effect of coupled electrical potential, temperature and stress10.1016/j.actamat.2007.02.022 ↗
16. FEM analysis of the temperature and stress distribution in spark plasma sintering: modelling and experimental validation10.1016/j.commatsci.2010.05.021 ↗
17. Average grain size in polycrystalline ceramics10.1111/j.1151-2916.1969.tb11975.x ↗
18. Grain boundary migration in ceramics10.1023/A:1008656302007 ↗
19. Grain boundary electronic structure related to the high-temperature creep resistance in polycrystalline Al2O310.1016/S1359-6454(02)00122-2 ↗