High-Jc YBa2Cu3O7−x-Ag superconducting thin films synthesized through a fluorine-free MOD method

X. Tang, Y. Zhao, W. Wu, N.H. Andersen, J.-C. Grivel

Publisher page

Abstract

Abstract Obtaining a high critical current density (Jc) remains the main challenge in developing fluorine-free metal organic deposition (MOD) methods to fabricate YBCO superconducting thin films. Silver addition was used to raise the Jc values in this research work. By reacting with propionic acid and ammonia, AgNO3 was initially mixed with YBCO carboxylate precursors dissolved in methanol. High-temperature in situ XRD measurements on the YBCO-Ag powders revealed that silver addition lowers the incongruent melting temperature of YBCO to 760 °C and resulted in a smooth surface morphology of the YBCO films at a temperature as low as 760 °C. Grain growth and intergranular conductivity were also found to be improved by silver doping. After annealing under optimized conditions, a high Jc of 4.6 MA/cm2 was obtained in a YBCO-Ag thin film with 10 wt% Ag.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Physics of Superconductivity and Magnetism · Copper Interconnects and Reliability · Magnetic properties of thin films

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Superconducting oxide films with high transition temperature prepared from metal trifluoroacetate precursors10.1063/1.99752 ↗
2. High critical current density thick MOD-derived YBCO films10.1109/77.784685 ↗
3. Large-area uniform ultrahigh-Jc YBa2Cu3O7−x film fabricated by the metalorganic deposition method using trifluoroacetates10.1088/0953-2048/14/7/101 ↗
4. Texture development and superconducting properties of YBa2Cu3Ox thin films prepared by a solution process in low oxygen partial pressure10.1088/0953-2048/14/5/308 ↗
5. High critical current density scheme of YBa2Cu3O7−x films by metalorganic deposition using trifluoroacetates10.1088/0953-2048/15/6/313 ↗
6. Preparation of YBCO films on CeO2-buffered (001) YSZ substrates by a non-fluorine MOD method10.1111/j.1551-2916.2004.01669.x ↗
7. Textured YBCO-film formation by sol–gel process and post annealing10.1016/S0955-2219(98)00182-4 ↗
8. Formation of epitaxial YBCO Thin films by ex-situ processing of a polymerized complex10.1109/TASC.2003.811983 ↗
9. Observation of carboxylic groups in the lattice of sintered Ba2YCu3O7−y high-Tc superconductors10.1103/PhysRevB.36.7148 ↗
10. Water-vapor-controlled reaction for fabrication of YBCO films by fluorine-free sol–gel process10.1109/TASC.2010.2050589 ↗
11. Preparation of YBCO films by an excimer-laser-assisted MOD by scanning irradiation10.1016/j.physc.2007.02.038 ↗
12. Large critical currents and improved epitaxy of laser ablated Ag doped YBa2Cu3O7−δ thin films10.1063/1.109014 ↗
13. Enhanced Jc and improved grain-boundary properties in Ag-doped YBa2Cu3O7−δ films10.1063/1.119452 ↗
14. Doping effect of Ag nanoparticles on critical current of YBa2Cu3O7−δ10.1016/j.physc.2010.11.005 ↗
15. Anisotropic critical currents in Ba2YCu3O7 analyzed using an extended Bean model10.1063/1.102387 ↗
16. Nucleation and mesostrain influence on percolating critical currents of solution derived YBa2Cu3O7 superconducting thin films10.1016/j.physc.2012.04.020 ↗
17. Mechanisms for hetero-epitaxial nucleation of YBa2Cu3O∼6.1 at the buried precursor/SrTiO3 interface in the post deposition reaction process10.1063/1.1436285 ↗
18. Conversion behavior comparison of TFA-MOD and non-fluorine solution-deposited YBCO films10.1016/j.physc.2009.04.008 ↗
19. Elucidation of mechanism in fluorine-free prepared YBa2Cu3O7−δ coatings10.1021/ic9021799 ↗
20. Nature of textured growth of laser-deposited YBaCuO thin films on (100) MgO10.1016/0921-5107(91)90006-H ↗
21. Isothermal sections and primary crystallization in the quasiternary YO1.5-BaO-CuOx system at p(O2)=0.21×105Pa10.1006/jssc.1993.1118 ↗
22. Influence of partial melting temperature on structure and superconducting properties of YBCO film by non-fluorine MOD10.1007/s10948-009-0635-x ↗
23. Grain-growth enhancement in the YBa2Cu3O7−x superconductor by silver-oxide doping10.1016/0167-577X(89)90071-2 ↗
24. Reactive liquid phase sintering of solution-derived YBa2Cu3O7−x superconducting thin films: Part 1. Ambient and precursor effects on BaO-CuO liquid phase formation10.1557/JMR.1993.2134 ↗
25. Reactive liquid phase sintering of YBa2Cu3O7−x superconducting thin films: Part 2. Sintering mechanism and film properties10.1557/JMR.1994.0844 ↗
26. Processing effect on microstructure and superconducting properties of sintered ReBa2Cu3Oy ceramics – the role of ionic radius10.1016/S0955-2219(00)00074-1 ↗
27. Textured YBCO films grown on wires: application to superconducting cables10.1088/0953-2048/25/12/125008 ↗
28. Improvement current transport properties of post annealed YBa2Cu3O7−x thin films using Ag doping10.1063/1.361473 ↗
29. Sublimation induced shape evolution of silver tubes10.1002/smll.200901189 ↗
30. Shi · 1995 · 360
31. The role of Ag in the pulsed laser growth of YBCO thin films
32. Correlation of the electric field effect with the weak link behaviour in granular YBCO superconductors10.1088/0953-2048/12/6/305 ↗
33. On the role of Ag in improved YBa2Cu3O7−δ10.1016/S0921-4534(97)00474-7 ↗
34. Chemical solution techniques for epitaxial growth of oxide buffer and YBa2Cu3O7 films10.1016/S0955-2219(03)00448-5 ↗
35. YBCO superconducting film coated on LaAlO3 substrate by TFA-MOD process10.1007/s10948-005-3384-5 ↗
36. Chemical solution deposition of YBa2Cu3O7−x films by dip coating
37. High-rate fabrication of YBCO coated conductors using TFA-MOD method10.1016/j.phpro.2012.03.444 ↗
38. Fabrication of high-Jc YBCO films by the TFA-MOD process using YBCO powder as precursor10.1109/TASC.2005.847758 ↗