Corrosion behaviour of R2O–CaO–SiO2 glasses submitted to accelerated weathering

N. Carmona, M.A. Villegas, J.M. Fernández Navarro

Publisher page

Abstract

Abstract Four glasses in the R2O–CaO–SiO2 (R = Na, K) system, following similar compositions to historical glasses used for production of stained glass windows, were prepared with different CaO/R2O ratio. The samples were submitted to accelerated weathering test under different temperature and relative humidity conditions, as well as under controlled SO2-polluted atmosphere. The experimental set up was selected to simulate the main conditions responsible for the deep deterioration submitted by the historical stained glass windows. Such damage has been very important during the last century, as a consequence of highly polluted industrial environments. As far as the results concern, it has been shown that 400 cycles of variable temperature and humidity are capable to develop pits on the glass surface, its shape and intensity depending on the glass composition. When weathering cycles were carried out with 10 ppm SO2 under high humidity conditions, calcium carbonate crystals appeared upon the glass surface, whereas calcium sulphate crystallisation occurred for higher SO2 concentration. The mechanism of chemical damage has been proposed and discussed in terms of the reaction between the Ca2+-ions leached from the glass sample and the environmental SO2. The former whole reaction occurred through an intermediate stage: the calcium carbonate crystallisation. That salt was displaced by sulphate only when the SO2 concentration was high enough.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Building materials and conservation · Conservation Techniques and Studies · Cultural Heritage Materials Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Fernández Navarro, J. M., Procesos de alteración de vidrieras medievales. Estudios y tratamientos de protección. Mater. Construcc., 1996, 46, 5–25, 242–243.10.3989/mc.1996.v46.i242-243.526 ↗
2. Fernández Navarro, J. M., Causas del deterioro fı́sico y quı́mico de los vidrios históricos. Jornadas Naciones sobre Restauración y Conservación de Vidrios, San Ildefonso, 2000, 17–37.
3. Les vitraux médiévaux: caractérisation phisico-chimie de l’alteration
4. Weathering effects on materials from historical stained glass windows
5. Decay of medieval stained glass at York, Canterbury and Carlise. Part 1. Composition of the glass and its weathering products
6. L’influence de la corrosion sur la vitese de décomposition des verres du Moyen Age
7. Deterioration of stained glass by atmospheric corrosion and micro-organims10.1007/BF00550580 ↗
8. The action of water and the sulphur dioxide on glass surfaces
9. Origin of sulphated grey crusts on glass in polluted urban atmosphere: stained glass windows of Tous Cathedral (France)
10. Surface analytical investigations on naturally weathered medieval stained glass
11. Deterioration of stained medieval glass by atmospheric attack. Pt. 1. Scanning electron microscopic investigations of the weathering phenomena
12. Fuchs, D. R., The effects of air pollutants on glass. In The Effects of Air Pollutants on Materials, ed. D. S. Lee and T. A. McMullen. AEA Workshop, London, 1994, pp. 29–32.
13. Lifanov, F. A., Ojovan, M. I., Stefanovsky, S. V. and Burcl, R., Cold crucible vitrification of NPP operational waste. Mater. Res. Soc. Symp. Proc., 2003, 757(II5.13), 1–6.10.1557/PROC-757-II5.13 ↗
14. Waste glass behaviour in a loamy soil of a wet repository site10.1016/S0022-3115(01)00593-1 ↗
15. Carmona, N., Study of Alteration Processes in Stained Glass Windows and Restoration and Protection Treatments. Ph.D. dissertation, Universidad de Valladolid, July 2002.
16. Composition et álteration des verres de vitraux anciens
17. Chemical composition of medieval stained glasses from the cathedral of León (Spain)
18. Ratio of CaO/K2O > 2 as evidence of a special Rhenish type of medieval stained glass
19. The morphology of weathering on historical glasses
20. Using triangular diagrams to understand the behaviour of medieval glasses
21. A new approach to predicting the durability of medieval window glass
22. A study of the weathering behaviour of medieval glass from York Minster
23. Fernández Navarro, J. M., El vidrio, ed. Spanish Council for Scientific Research, CSIC, Madrid, 1985.
24. Spanish Standard UNE 43-702-74, Ensayos de vidrios. Determinación del coeficiente de dilatación lineal.
25. Spanish Standard UNE 43-703-78, Ensayos de vidrio. Determinación dilatométrica de la temperatura de transformación.
26. Standard DIN 50017, Methods of Testing in Damp Heat Atmospheres. DIN, Berlin, 1967.
27. Standard DIN 50018, Testing in a Saturated Atmosphere in the Presence of Sulphur Dioxide. DIN, Berlin, 1982.
28. Carmona, N., Garcı́a-Heras, M., Gil, C. and Villegas, M. A., Deterioro de vidrios en medio submarino.ed. Ayuntamiento de Santoña. Monte Buciero, La conservación del material arqueológico Subacuático vol. 9, Santander, 2003, 327–349.
29. Thermal and chemical behaviour of different glasses containing steel fly ash and their transformation into glass-ceramics10.1016/S0955-2219(01)00492-7 ↗
30. ISO 719, Glass. Hydrolytic Resistance of Glass Grains at 98°C. Method of Test and Classification. 1985.