journal article·2003-01

Thermal shock resistance of yttria-stabilized zirconia with Palmqvist indentation cracks

G. Fargas, D. Casellas, L. Llanes, M. Anglada

Publisher page

Abstract

Thermal shock behaviour of two tetragonal zirconia polycrystals stabilised with 2.5% molar yttria and with different fracture toughness have been investigated by analysing stable crack extension of indentation Palmqvist cracks in the quench indentation test. It is shown that the ratio between the thermal stress intensity factor and the fracture toughness can be easily obtained by measuring the stable crack extension. It is shown that deviations from the expected maximum stable crack extension during thermal shock can be accounted for by subcritical crack growth and by a reduction in the level of residual stresses. For small indentation loads, R-curve effects become important and must be considered to explain the experimental results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Perspective on the development of high-toughness ceramics10.1111/j.1151-2916.1990.tb06493.x ↗
2. Transformation toughening in zirconia-containing ceramics10.1111/j.1151-2916.2000.tb01221.x ↗
3. Transformation toughening Part 1–410.1007/BF00809057 ↗
4. Quantitatives studies of thermal shock in ceramics based on a novel test technique10.1111/j.1151-2916.1981.tb09606.x ↗
5. Elastic energy as design criteria for thermal shock10.1111/j.1151-2916.1963.tb14605.x ↗
6. Thermal stress resistance parameters for brittle refractory ceramics: A. compendium
7. The Vickers indentation technique used to evaluate thermal shock resistance of brittle materials10.1016/S1359-6462(97)00106-1 ↗
8. Toughness and thermal shock resistance of YBa2Cu3O7-x composite superconductors containing Y2BaCuO5 or Ag particles10.1016/S0921-5093(00)01316-2 ↗
9. Analysis and prediction of thermal shock in brittle materials10.1016/S1359-6454(00)00011-2 ↗
10. Lawn · 1995
11. Nihihara · J. Mater. Sci. Lett. · 1982 · 1310.1007/BF00724706 ↗
12. Failure due to semielliptical surface cracks under arbitrary stress distributions10.1046/j.1460-2695.2000.00277.x ↗
13. An analysis of the residual intensity factor of Vickers indentation cracks10.1016/0013-7944(95)00054-Y ↗
14. On the transformation toughening of Y-ZrO2 ceramics with mixed TZP/PSZ microstructures10.1016/S0955-2219(00)00273-9 ↗
15. Quinn, G. D., Kübler, J. and Getting, R., Fracture Toughness of Advanced Ceramics by the Surface Crack in Flexure (SCF) Method: A VAMAS Round Robin. VAMAS Technical Working Area 3, Report No. 17, 1993.
16. Indentation pre-cracking of Y-TZP: implications to R-curves and strength10.1016/S0921-5093(97)00726-0 ↗
17. A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements10.1111/j.1151-2916.1981.tb10320.x ↗