journal article·2005-08

Low-temperature ageing degradation of 2.5Y-TZP heat-treated at 1650°C

A. Feder, M. Anglada

Publisher page

Abstract

Abstract Low temperature ageing degradation at 250 °C in air of 2.5 mol% Y-TZP with various grain sizes has been investigated by using specimens in the form of discs of 8 mm diameter and 1 mm in thickness. The increase in tetragonal grain size, as well as some cubic phase, were attained by heat-treating 0.3 μm fine grain size Y-TZP at 1650 °C for different times. XRD and Raman spectroscopy analysis were used to evaluate the amount of tetragonal to monoclinic (t–m) phase transformation after different ageing times at 250 °C in air up to 900 h and its effect on strength was measured by using the biaxial ball-on-three-balls test. It is shown that transformability under ageing conditions at 250 °C increases with tetragonal grain size. Raman analysis was done punctually at various distances form the edge of the aged samples and it is shown that the nucleation of monoclinic sites begins at the edge of the samples and that the depth of the transformation zone varies with the distance from the edge to the centre of the samples. Biaxial strength always decreases with ageing time and is influenced by the presence of micro and macrocracks formed at the surface centre of the aged samples. This depends strongly on the tetragonal grain size and on the depth of the transformed layer at the central part of the discs.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Green · 1989
2. Mechanics of transformation toughening in brittle materials10.1111/j.1151-2916.1982.tb10426.x ↗
3. Thermal and mechanical properties of Y2O3-stabilized tetragonal zirconia polycrystals
4. Aging behaviour of Y-TZP
5. Changes in crystalline phase and microstructure on the surface of yttria-doped tetragonal zirconia polycrystals (Y-TZP) by annealing in humid conditions
6. Mechanical properties of Y-PSZ after aging at low-temperature10.1016/0267-3762(86)90011-1 ↗
7. Phase transformation in Y2O3-partially-stabilized ZrO2 polycrystals of various grain sizes during low-temperature aging in water10.1111/j.1151-2916.1998.tb02677.x ↗
8. Degradation during aging of transformation-toughened ZrO2–Y2O3 materials at 250°C10.1111/j.1151-2916.1986.tb07415.x ↗
9. X-ray photoelectron spectroscopy investigation on the low-temperature degradation of 2mol% Y2O3–ZrO2 ceramics10.1111/j.1151-2916.1996.tb08084.x ↗
10. Hydrothermal degradation of cubic zirconia10.1016/S1359-6454(03)00362-8 ↗
11. Transformation toughening10.1007/BF00809057 ↗
12. Effect of heat treatment on grain size, phase assemblage, and mechanical properties of 3mol% Y-TZP10.1111/j.1151-2916.1996.tb08980.x ↗
13. Fracture toughness and mechanical strength of Y-TZP/PSZ ceramics10.1016/S1359-6462(01)01020-X ↗
14. On the transformation toughening of Y-ZrO2 ceramics with mixed Y-TZP/PSZ microstructures10.1016/S0955-2219(00)00273-9 ↗
15. Phase analysis in zirconia systems10.1111/j.1151-2916.1972.tb11290.x ↗
16. The ball on three balls test for strength testing of brittle discs: stress distribution in the disc10.1016/S0955-2219(01)00458-7 ↗
17. Fracture variability and R-curve behavior in yttria-stabilized zirconia ceramics10.1023/A:1017923008382 ↗
18. Phase relationships in the zirconia-yttria system10.1007/BF01031853 ↗
19. Critical effect of cubic phase on aging in 3mol% yttria-stabilized zirconia ceramics for hip replacement prosthesis10.1016/j.biomaterials.2004.01.002 ↗