Seamless joining of silicon carbide ceramics through an sacrificial interlayer of Dy3Si2C2
Source abstract
Abstract
Abstract A ternary carbide Dy3Si2C2 coating was fabricated on the surface of SiC through a molten salt technique. Using the Dy3Si2C2 coating as the joining interlayer, seamless joining of SiC ceramic was achieved at temperature as low as 1500 °C. Phase diagram calculation indicates that seamless joining was achieved by the formation of liquid phase at the interface between Dy3Si2C2 and SiC, which was squeezed out under pressure and continuously consumed by the joining interlayer. This work implies the great potential of the family of ternary rare-earth metal carbide Re3Si2C2 (Re = Y, La-Nd) as the sacrificial interlayer for high-quality SiC joining.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · MXene and MAX Phase Materials · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Handbook of SiC properties for fuel performance modeling
2. Material properties of a sintered α-SiC10.1063/1.556000 ↗
3. The critical issues of SiC materials for future nuclear systems10.1016/j.scriptamat.2017.03.001 ↗
4. Joining of SiC by Al infiltrated TiC tape: effect of joining parameters on the microstructure and mechanical properties10.1016/j.jeurceramsoc.2011.08.001 ↗
5. Joining of β-SiC by spark plasma sintering10.1016/j.jeurceramsoc.2013.12.023 ↗
6. Recent advances in joining of SiC-based materials (monolithic SiC and SiCf/SiC composites): joining processes, joint strength, and interfacial behavior10.1007/s40145-018-0297-x ↗
7. Thickness-dependent phase evolution and bonding strength of SiC ceramics joints with active Ti interlayer10.1016/j.jeurceramsoc.2016.12.009 ↗
8. Flexural strength and shear strength of silicon carbide to silicon carbide joints fabricated by a molybdenum diffusion bonding technique10.1111/j.1551-2916.2005.00381.x ↗
9. Liquid infiltration joining of 2D C/SiC composite10.1515/SECM.2006.13.1.31 ↗
10. Wetting of SiC by Al-Ti alloys and joining by in-situ formation of interfacial Ti3Si(Al)C210.1016/j.jeurceramsoc.2018.04.025 ↗
11. Pressureless brazing of zirconia to stainless steel with Ag–Cu filler metal and TiH2 powder10.1016/j.jeurceramsoc.2008.04.008 ↗
12. Reaction joining of SiC ceramics using TiB2-based composites10.1016/j.jeurceramsoc.2010.07.017 ↗
13. High-temperature stability of laser-joined silicon carbide components
14. A glass in the CaO/MgO/Al2O3/SiO2 System for the rapid laser sealing of alumina10.1016/j.ceramint.2016.12.073 ↗
15. Fast joining SiC ceramics with Ti3SiC2 tape film by electric field-assisted sintering technology
16. Copper–SiC whiskers composites with interface optimized by Ti3SiC210.1007/s10853-018-2255-y ↗
17. Fabrication and characterization of SPS sintered SiC-based ceramic from Y3Si2C2-coated SiC powders10.1016/j.jeurceramsoc.2018.07.054 ↗
18. Magnetic and electrical properties of a new series of rare earth silicide carbides with the composition R3Si2C2 (R=Y, La-Nd, Gd-Tm)10.1006/jssc.1998.7772 ↗
19. The Thermo-Calc databank system10.1016/0364-5916(85)90021-5 ↗
20. Preparation of TiC/Ti2AlC coating on carbon fiber and investigation of the oxidation resistance properties10.1111/jace.15784 ↗
21. Y2O3–Al2O3–SiO2-based glass-ceramic fillers for the laser-supported joining of SiC10.1016/j.jeurceramsoc.2014.01.019 ↗