Injection molding, debinding and sintering of ZrO2 ceramic modified by silane couping agent
Source abstract
Abstract
Abstract In this paper, Injection molding, debinding and sintering of ZrO2 ceramic modified by silane coupling agent (A151) were studied by measuring the melt index of feedstocks, the soluble removal ratio of green parts, the bending strength of green and sintered parts, the surface and fractural morphologies of sintered parts. The results showed that the melt index of ZrO2 feedstocks, the weight removal ratio of soluble binders, and the bending strength of green parts increased after adding A151. When the density of sintered parts was between 5.97–6.03 g/cm3, it was not the main factor influencing the bending strength. However, the bending strengths of sintered parts decreased due to microcrack formation when thermal debinding process was too fast or slow. The interesting phenomenon of the abnormal grain growth with transgranular fracture in the sintered parts obviously occurred above 1550 ℃, which made the effect of sintering temperature on the strength become complex.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Dental materials and restorations · Injection Molding Process and Properties · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. From porcelain-fused-to-metal to zirconia: clinical and experimental considerations10.1016/j.dental.2010.10.024 ↗
2. State of the art of zirconia for dental applications10.1016/j.dental.2007.05.007 ↗
3. The zirconia ceramic: strengths and weaknesses10.2174/1874210601408010033 ↗
4. Binder removal via a two-stage debinding process for ceramic injection molding parts10.1016/j.ceramint.2013.10.032 ↗
5. Effect of microcrystalline wax on the solvent debinding of the Sr-ferrite ceramics prepared by powder injection molding10.1016/j.jeurceramsoc.2016.12.026 ↗
6. Binder system for micropowder injection molding10.1016/S0167-577X(00)00276-7 ↗
7. Thermal removal of multicomponent binder from ceramic injection mouldings10.1016/S0955-2219(02)00015-8 ↗
8. Effects of different backbone binders on the characteristics of zirconia parts using wax-based binder system via ceramic injection molding10.1007/s40145-016-0205-1 ↗
9. Micro PIM moves into the zone of industrial possibility10.1016/S0026-0657(09)70219-X ↗
10. Surface adhesion between ceramic injection molding feedstocks and processing tools10.1016/j.ceramint.2015.08.132 ↗
11. Influence of stearic acid concentration on the processing of ZrO2-containing feedstocks suitable for micropowder injection molding10.1111/j.1744-7402.2010.02519.x ↗
12. Debinding behaviors and mechanism of injection molded ZrO2 ceramics using kerosene as solvents10.4028/www.scientific.net/KEM.512-515.431 ↗
13. Investigation of the solvent debinding in the injection molding of ZrO2 ceramics using LDEP, HDPE and wax binders10.1016/j.ceramint.2018.11.062 ↗
14. Characterization of silane-modified ZrO2 powder surfaces10.1002/(SICI)1096-9918(199711)25:12<917::AID-SIA314>3.0.CO;2-3 ↗
15. The use of silane coupling agents in ceramic injection moulding10.1007/BF01115777 ↗
16. The use of silane coupling agents in ceramic injection moulding: effect on polymer removal10.1007/BF00727870 ↗
17. Surface modification of BMN particles with silane coupling agent for composites with PTFE10.1016/j.apsusc.2017.04.072 ↗
18. Surface modification of ceramic powders by titanate coupling agent for injection molding using partially water soluble binder system10.1016/j.jeurceramsoc.2011.11.017 ↗
19. Improvement of the rheological properties of the zirconia/polypropylene system for ceramic injection moulding using coupling agents10.1007/BF02403833 ↗